Free-Standing Porous and Nonporous Polyethylene Thin Films Using Spin Coating: An Alternate to the Extrusion–Stretching Process AITranslate
Abstract AITranslate
Spin coating is widely used in the preparation of thin films as it yields reproducible results with uniform surface and controlled thickness. However, free-standing thin films of polyolefins have never been produced using spin coating as the coated films do not have sufficient strength to maintain their integrity without a supporting layer or substrate. Herein, we report free-standing thin films of polyolefins such as polyethylene with varying thickness ranging from 5 to 20 μm. In one such combination, 30% porosity, 5 MPa tensile strength, and 7 μm thickness were achieved. These films can be used as hydrophobic coating, filtration membranes, and oil-sorbents.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c02183
Chinese Library Classification Number:
Citation Information:
Spin coating is widely used in the preparation of thin films as it yields reproducible results with uniform surface and controlled thickness. However, free-standing thin films of polyolefins have never been produced using spin coating as the coated films do not have sufficient strength to maintain their integrity without a supporting layer or substrate. Herein, we report free-standing thin films of polyolefins such as polyethylene with varying thickness ranging from 5 to 20 μm. In one such combination, 30% porosity, 5 MPa tensile strength, and 7 μm thickness were achieved. These films can be used as hydrophobic coating, filtration membranes, and oil-sorbents.
quote
| GB/T 7714-2015 | [1] Junaid Saleem, Zubair Khalid Baig Moghal, Adriaan S. Luyt, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02183. |
| MLA | [1] Junaid Saleem, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02183. |
| APA | [1] Junaid Saleem, Zubair Khalid Baig Moghal, Adriaan S. Luyt, R. A. Shakoor, & Gordon McKay. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02183 |
| IEEE | [1] Junaid Saleem, Zubair Khalid Baig Moghal, Adriaan S. Luyt, R. A. Shakoor, and Gordon McKay, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02183. keywords: {freestanding thin film;polyolefins;spin coating;annealing;porous} |