daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Controlling Cellulose Membrane Performance via Solvent Choice during Precursor Membrane Formation AITranslate

Middle East Technical University; Middle East Technical University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Fabrication of cellulose membranes by alkaline hydrolysis of cellulose acetate (CA) membranes is a simple alternative method to preparing cellulose membranes via phase inversion from their ionic liquid solutions. In this study, three different solvent systems were used to fabricate cellulose acetate membranes by phase inversion, which are dimethyl sulfoxide and its mixtures with acetone and acetic acid. Acetone as cosolvent led to an asymmetric morphology with the densest selective layer, whereas acetic acid led to a loose, almost isotropic structure with high porosity and pore connectivity, also reflected in the pure water permeance and molecular weight cutoff (MWCO) of the CA membranes. Comparing the effects of these cosolvents on the phase inversion process, acetic acid decreased the solvent quality, increased nonsolvent–solvent interactions, and in total decreased the polymer solutions’ stability against phase separation. The phase inversion rate when acetic acid was used as cosolvent was also markedly lower, which was attributed primarily to the solvent’s much higher viscosity. After alkaline hydrolysis of the CA membranes, which converted them into cellulose membranes, the permeance and MWCO of large-pore, small-pore, and dense membranes changed in different directions. This was attributed to a changing membrane structure due to partial degradation of cellulose chains in an alkaline medium, which in turn can affect transport through both the pores and the membrane matrix.

KeyWords AITranslate

phase inversion cellulose acetate membrane cosolvent alkaline hydrolysis cellulose membrane
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02185

Chinese Library Classification Number:

Citation Information:

Fabrication of cellulose membranes by alkaline hydrolysis of cellulose acetate (CA) membranes is a simple alternative method to preparing cellulose membranes via phase inversion from their ionic liquid solutions. In this study, three different solvent systems were used to fabricate cellulose acetate membranes by phase inversion, which are dimethyl sulfoxide and its mixtures with acetone and acetic acid. Acetone as cosolvent led to an asymmetric morphology with the densest selective layer, whereas acetic acid led to a loose, almost isotropic structure with high porosity and pore connectivity, also reflected in the pure water permeance and molecular weight cutoff (MWCO) of the CA membranes. Comparing the effects of these cosolvents on the phase inversion process, acetic acid decreased the solvent quality, increased nonsolvent–solvent interactions, and in total decreased the polymer solutions’ stability against phase separation. The phase inversion rate when acetic acid was used as cosolvent was also markedly lower, which was attributed primarily to the solvent’s much higher viscosity. After alkaline hydrolysis of the CA membranes, which converted them into cellulose membranes, the permeance and MWCO of large-pore, small-pore, and dense membranes changed in different directions. This was attributed to a changing membrane structure due to partial degradation of cellulose chains in an alkaline medium, which in turn can affect transport through both the pores and the membrane matrix.

quote

GB/T 7714-2015 [1] Fatma Seden Tekin, P. Zeynep ÇulfazEmecen. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02185.
MLA [1] Fatma Seden Tekin, and P. Zeynep ÇulfazEmecen. ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02185.
APA [1] Fatma Seden Tekin, & P. Zeynep ÇulfazEmecen. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02185
IEEE [1] Fatma Seden Tekin and P. Zeynep ÇulfazEmecen, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02185. keywords: {phase inversion;cellulose acetate membrane;cosolvent;alkaline hydrolysis;cellulose membrane}