Preparation of Refractory Metal Compounds by Mechanical Alloying AITranslate
Abstract AITranslate
The characteristic of mechanical alloying (MA) is described in this paper: emphasis is given to the study of the process and mechanism of refractory compounds made by MA. We consider that it is an effective method to make the refractory compounds by MA.
KeyWords AITranslate
1章桥新,张东明.机械合金化制备金属铌的难熔化合物[J].无机材料学报,1995,10(2):253-256. 被引量:1
2柳林,李兵,丁星兆,马学鸣,戚震中,董远达.机械合金化法制备超高熔点金属碳化物纳米材料[J].科学通报,1994,39(5):471-474. 被引量:17
3李运姣,李洪桂,刘茂盛,孙培梅.浅谈机械活化在湿法冶金中的应用[J].稀有金属与硬质合金,1993,21(3):38-42. 被引量:18
1张厚安,王德志,刘心宇,王碧玉.球料比对机械合金化合成MoSi_2过程的影响[J].湘潭矿业学院学报,1997,12(1):68-71. 被引量:1
2李岩,刘心宇.MoSi_2球磨工艺的探讨[J].稀有金属与硬质合金,2000,28(3):11-13. 被引量:4
3陈枭,王洪涛,白小波,王玉伟,都学飞.TiB_2增强50Ni基金属陶瓷复合粉末与涂层的研究[J].兵器材料科学与工程,2013,36(3):32-35. 被引量:3
4陈枭,王洪涛,纪岗昌,白小波,富伟.TiB_2增强Co基金属陶瓷粉末与涂层组织结构研究[J].兵器材料科学与工程,2014,37(5):1-4. 被引量:1
1卢希龙,卢迪芬,陈森凤,王英连.机械力化学在纳米无机材料制备中的应用[J].硅酸盐通报,2004,23(6):66-70. 被引量:11
2周琦,马勤,郭铁明,季根顺,贾建刚.MoSi_2机械球磨过程中的物相转变[J].有色金属,2005,57(3):28-30. 被引量:2
3左可胜,席生岐,周敬恩.Mo-Si二元粉末机械合金化及其热力学分析[J].西安交通大学学报,2006,40(9):1062-1065.
4袁慎坡,陈萌莉.高能球磨法细化合金钢粉末工艺的研究[J].新技术新工艺,2007(6):84-86.
5张厚安,刘心宇,陈平.二硅化钼自配副在干摩擦条件下的摩擦学性能研究[J].摩擦学学报,2001,21(6):456-459. 被引量:12
6王芬玲,杨卿,邹军涛,梁淑华.机械合金化制备Ni-B-Si合金粉末[J].稀有金属材料与工程,2015,44(8):1985-1989. 被引量:1
7赵明娟,谢池,赵龙志,唐延川,张坚.机械合金化转速对CNTs-SiC/Ni激光熔覆微观结构的影响[J].兵器材料科学与工程,2017,40(5):68-71. 被引量:1
8黄小晓,涂赣峰,王术新,宋建勋,刘莹,王正宗.TiB_(2)涂层的制备及其应用研究进展[J].稀有金属材料与工程,2022,51(3):1087-1099. 被引量:1
9陈枭,张晓敏,陈珑,关晓晓,黄硕文,范亚乔,段小华.超音速火焰喷涂TiB_2-40Ni涂层的组织和耐磨性[J].金属热处理,2014,39(12):107-109. 被引量:3
1章桥新,张东明.机械合金化制备金属铌的难熔化合物[J].无机材料学报,1995,10(2):253-256. 被引量:1
2李沐山.高温自蔓合成法制取难熔化合物[J].硬质合金,1991,8(1):6-13. 被引量:1
3粉末热压[J].粉末冶金技术,2016,34(2):118-118.
Basic Information:
DOI:
Chinese Library Classification Number:TF123.3[冶金工程—粉末冶金]
Citation Information:
The characteristic of mechanical alloying (MA) is described in this paper: emphasis is given to the study of the process and mechanism of refractory compounds made by MA. We consider that it is an effective method to make the refractory compounds by MA.
quote
| GB/T 7714-2015 | [1] ZHANG Qiao-xin, WANG Sheng-rui, MAO Tian-er. Preparation of Refractory Metal Compounds by Mechanical Alloying[J]. Rare Metals and Cemented Carbides, 1995(3): 26-28. |
| MLA | [1] ZHANG Qiao-xin, et al., "Preparation of Refractory Metal Compounds by Mechanical Alloying." Rare Metals and Cemented Carbides, no. 3, 1995, pp. 26-28. |
| APA | [1] ZHANG Qiao-xin, WANG Sheng-rui, & MAO Tian-er. (1995). Preparation of Refractory Metal Compounds by Mechanical Alloying. Rare Metals and Cemented Carbides(3), 26-28. |
| IEEE | [1] ZHANG Qiao-xin, WANG Sheng-rui, and MAO Tian-er, "Preparation of Refractory Metal Compounds by Mechanical Alloying," Rare Metals and Cemented Carbides, no. 3, pp. 26-28, 1995. keywords: {mechanical alloying, refractory metal compounds,composition mechanism} |