Abstract AITranslate

The effects of cobalt on the reduction of molybdenum powder and mechanical properties of annealed Mo wire were investigated. The results show that the adding of cobalt benefits the reduction of MoO3and increases the density of sintered molybdenum bar. It also shows that cobalt can decrease the recrystallization temperature of molybdenum wireand distinctly improve the ductility of annealed molybdenum wire.

KeyWords AITranslate

molybdenum. cobalt wire mechanical property

1夏伟军,刘心宇,宁爱林.钴对钼丝加工及组织性能的影响[J].稀有金属与硬质合金,2001,29(2):36-40.

2李静,高家诚,王勇.掺杂提高钼丝再结晶温度的研究进展[J].稀有金属与硬质合金,2003,31(1):22-24. 被引量:15

1杨晓青,罗振中,郭荣辉,关鑫.稀土掺杂钼制品研究进展[J].中国钼业,2006,30(4):33-35. 被引量:12

2刘仁智,李大成,卜春阳,李晶.AKS掺杂粒子演变及其丝材性能研究[J].中国钼业,2007,31(6):42-47. 被引量:2

3刘仁智,李大成,卜春阳,李晶.AKS合金丝中第二相粒子形貌演变机理研究[J].热加工工艺,2008,37(8):22-25. 被引量:2

4张宏斌,祝要民,赵胜利,凌雄辉.Si-Al-K掺杂钼的高温力学性能和组织研究[J].热加工工艺,2008,37(22):32-33. 被引量:5

5刘仁智,李大成,卜春阳,李晶,刘东新.AKS掺杂钼板显微组织与力学性能研究[J].稀有金属,2009,33(1):12-16. 被引量:3

6卜春阳,孟庆乐,王快社,武洲.Mo-Al掺杂钼丝电解清洗质量分析[J].中国钼业,2012,36(4):44-47.

7魏世忠,周玉成,段素红,张国赏.氧化镧含量对钼板组织与性能的影响[J].河南科技大学学报:自然科学版,2013,34(2):1-4. 被引量:6

8王跃明,唐求豪,闫志巧,王芬,熊翔.等离子喷涂成型Mo/ZrC复合喷管的烧蚀性能研究[J].固体火箭技术,2018,41(6):778-786.

9朱向炜,张国赏,崔超鹏,魏世忠,郭松亮.Zr元素添加量对钼合金组织和性能的影响研究[J].稀有金属与硬质合金,2014,42(4):31-34. 被引量:2

10宗立君,周海涛,丁洪波,高风雷,刘克明.热机械处理对TZM合金组织和性能的影响[J].热处理技术与装备,2016,37(4):34-39. 被引量:1

1夏伟军,刘心宇,宁爱林.钴对钼丝加工及组织性能的影响[J].稀有金属与硬质合金,2001,29(2):36-40.

2特种细丝材的制备技术项目简介[J].新材料产业,2009(10).

3高瑞,班立志,江轩,吕保国.BJ-C型键合金丝的研制[J].稀有金属,1995,19(3):161-164. 被引量:1

4张传军,邬云骅,曹鸿,赵守仁,王善力,褚君浩.不同退火条件对磁控溅射CdS薄膜性能的影响[J].红外与毫米波学报,2013(4):298-303. 被引量:3

5吴永德.TD-LTE CSFB技术探讨[J].移动信息,2015,0(8):35-35. 被引量:1

6聂祚仁,黄惠忠,张久兴,王金淑,周美玲,左铁镛.碳化Mo-La_2O_3阴极丝高温光电子能谱分析[J].金属功能材料,1998,5(1):32-35. 被引量:3

7陈建军,谢显中.TD-SCDMA系统切换实现方式及时延性能分析[J].重庆邮电学院学报:自然科学版,2006,18(1):65-67.

8李安涛,郭梯云.应答业务对随机多址系统吞吐量及时延性能的影响[J].通信学报,1992,13(6):58-66. 被引量:3

9Yi-ning He,Xiao Liu,Qi Liao,周建军,Hong Huo,Lin Li.Thickness-dependent Orientation Structure in Poly(ethylene oxide) Multi-layer Crystals[J].高分子科学:英文版,2014,0(9):1253-1259. 被引量:1

10张书明,孙长印,朱李安,赛小峰,程昭,何益民,高鸿楷,侯洵.NEA GaAs光电阴极激活工艺研究[J].光子学报,1996,25(8):745-748.

Basic Information:

DOI:

Chinese Library Classification Number:TN110.41[电子电信—物理电子学]

Citation Information:

The effects of cobalt on the reduction of molybdenum powder and mechanical properties of annealed Mo wire were investigated. The results show that the adding of cobalt benefits the reduction of MoO3and increases the density of sintered molybdenum bar. It also shows that cobalt can decrease the recrystallization temperature of molybdenum wireand distinctly improve the ductility of annealed molybdenum wire.

quote

GB/T 7714-2015 [1] CHENG Jun, LIU Xin-yu, ZHANG Hou-an. A Study on Mo-Co Alloy Wire[J]. Rare Metals and Cemented Carbides, 1995(3): 22-25.
MLA [1] CHENG Jun, et al., "A Study on Mo-Co Alloy Wire." Rare Metals and Cemented Carbides, no. 3, 1995, pp. 22-25.
APA [1] CHENG Jun, LIU Xin-yu, & ZHANG Hou-an. (1995). A Study on Mo-Co Alloy Wire. Rare Metals and Cemented Carbides(3), 22-25.
IEEE [1] CHENG Jun, LIU Xin-yu, and ZHANG Hou-an, "A Study on Mo-Co Alloy Wire," Rare Metals and Cemented Carbides, no. 3, pp. 22-25, 1995. keywords: {molybdenum. cobalt wire, mechanical property}