Electrolyte-Gated Perovskite Transistors Functionalized with Conjugated Polymers AITranslate

Dongguk University; Dongguk University; Dongguk University; Dongguk University; Dongguk University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In emerging perovskite transistors, interfacial engineering is pivotal for modulating the effective charge carrier transport; however, the gate dielectric layer and its interface remain unexplored owing to the limited chemical stability of perovskites. Here, we propose an interfacial functionalization with a conjugated polymer to allow the use of a high capacitance electrolyte dielectric in top-gate perovskite transistors. This multifunctional approach, exploiting orthogonal solution-processed polymers, enables blocking of chemical diffusion during the deposition of the dielectric, allows passivation of defects on the perovskite surface, results in air stability enhancement, and boosts mobility via the formation perovskite–polymer hybrid channels. The optimized conjugated polymer-capped lead iodide perovskite transistors showed a remarkable hole mobility of over 30 cm2 V–1 s–1 at ≤2 V. This result demonstrated the possibility of realizing high mobility through interfacial functionalization of perovskites in transistor applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c01039

Chinese Library Classification Number:

Citation Information:

In emerging perovskite transistors, interfacial engineering is pivotal for modulating the effective charge carrier transport; however, the gate dielectric layer and its interface remain unexplored owing to the limited chemical stability of perovskites. Here, we propose an interfacial functionalization with a conjugated polymer to allow the use of a high capacitance electrolyte dielectric in top-gate perovskite transistors. This multifunctional approach, exploiting orthogonal solution-processed polymers, enables blocking of chemical diffusion during the deposition of the dielectric, allows passivation of defects on the perovskite surface, results in air stability enhancement, and boosts mobility via the formation perovskite–polymer hybrid channels. The optimized conjugated polymer-capped lead iodide perovskite transistors showed a remarkable hole mobility of over 30 cm2 V–1 s–1 at ≤2 V. This result demonstrated the possibility of realizing high mobility through interfacial functionalization of perovskites in transistor applications.

quote

GB/T 7714-2015 [1] Vivian NketiaYawson, Benjamin NketiaYawson, Henry Opoku, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01039.
MLA [1] Vivian NketiaYawson, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01039.
APA [1] Vivian NketiaYawson, Benjamin NketiaYawson, Henry Opoku, Ji Hyeon Lee, & Jea Woong Jo. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01039
IEEE [1] Vivian NketiaYawson, Benjamin NketiaYawson, Henry Opoku, Ji Hyeon Lee, and Jea Woong Jo, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01039.