China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences; East China University of Science and Technology; East China University of Science and Technology; East China University of Science and Technology; Jiangnan University; China|University of Chinese Academy of Sciences; East China University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The synthesis of heteroatom-doped porous carbons for efficient electrochemical production of hydrogen peroxide (H2O2) through two-electron (2e–) oxygen reduction reaction (ORR) has attracted increasing research attention since it offers a promising renewable substitute for the traditional complex energy-intensive anthraquinone process. Herein, a novel pyrolysis-free mechanochemical approach was developed for straightforward conversion of small organic molecules into metal-free heteroatom-doped mesoporous carbons (HMCs), where the uniqueness of this one-pot ball-milling technique not only exceeds the limit of volatilities of traditional carbonaceous precursors but also eliminates the need for any additional mesoporous templates. The abundance of molecular precursors (up to 23 different molecules) provides a facile means to introduce a wide variety of heteroatoms (B, N, O, P, S, F, Cl, etc.) into the resultant carbon materials, accompanied by in situ formation of rich mesopores. As a result, the resulting N/O co-doped mesoporous carbon with the highest Brunauer–Emmett–Teller (BET) surface area of 1238 m2 g–1 exhibits exceptional H2O2 selectivity of 95.2% in 0.1 M KOH solution at 0.70 V (vs. reversible hydrogen electrode, RHE) and a large H2O2 production rate of ca. 265 mmol gcat.–1 h–1, ranking at the top among all metal-free carbonaceous electrocatalysts. We anticipate our findings will facilitate new possibilities for the development of mesoporous carbons for electrocatalytic applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c01005

Chinese Library Classification Number:

Citation Information:

The synthesis of heteroatom-doped porous carbons for efficient electrochemical production of hydrogen peroxide (H2O2) through two-electron (2e–) oxygen reduction reaction (ORR) has attracted increasing research attention since it offers a promising renewable substitute for the traditional complex energy-intensive anthraquinone process. Herein, a novel pyrolysis-free mechanochemical approach was developed for straightforward conversion of small organic molecules into metal-free heteroatom-doped mesoporous carbons (HMCs), where the uniqueness of this one-pot ball-milling technique not only exceeds the limit of volatilities of traditional carbonaceous precursors but also eliminates the need for any additional mesoporous templates. The abundance of molecular precursors (up to 23 different molecules) provides a facile means to introduce a wide variety of heteroatoms (B, N, O, P, S, F, Cl, etc.) into the resultant carbon materials, accompanied by in situ formation of rich mesopores. As a result, the resulting N/O co-doped mesoporous carbon with the highest Brunauer–Emmett–Teller (BET) surface area of 1238 m2 g–1 exhibits exceptional H2O2 selectivity of 95.2% in 0.1 M KOH solution at 0.70 V (vs. reversible hydrogen electrode, RHE) and a large H2O2 production rate of ca. 265 mmol gcat.–1 h–1, ranking at the top among all metal-free carbonaceous electrocatalysts. We anticipate our findings will facilitate new possibilities for the development of mesoporous carbons for electrocatalytic applications.

quote

GB/T 7714-2015 [1] Na Yang, Xiang Zhu, Guofeng Wang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01005.
MLA [1] Na Yang, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01005.
APA [1] Na Yang, Xiang Zhu, Guofeng Wang, Lulu Zhou, Xiaoxiao Zhu, Jiaqi Pan, Wei Yu, Chungu Xia, & Chengcheng Tian. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01005
IEEE [1] Na Yang, Xiang Zhu, Guofeng Wang, Lulu Zhou, Xiaoxiao Zhu, Jiaqi Pan, Wei Yu, Chungu Xia, and Chengcheng Tian, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01005.