Ni-Fe-C Alloy Effect on η-phases Formed during TIG Welding of YG30 with S45C AITranslate

Department of Materials Science and Engineering, Dalian Railway Academy;Department of Materials Science and Engineering, Dalian Railway Academy;Department of Materials Science and Engineering, Dalian Railway Academy;Department of Materials Science and Engineering, Dalian Railway Academy;Department of Materials Science and Engineering, Dalian Railway Academy
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The welding joints between YG30 and S45C by using Ni-Fe-C alloys as weld metal were obtained by TIG welding.The welding joints were studied by means of optical microscope, SEM, EPMA, X-rays, micro hardness etc. The results showed that the welding joints between YG30 and S45C by TIG welding, can be obtained by using Ni-Fe-C alloys as weld metal,The harmful η phase can be restricted by the addition of C element into Ni-Fe alloys.So the inadequate carbide of the W-Co-C system induced by the C diffusion and the high ingredient Fe are the two vital factors to η phase formation, and η phase was M6C, M12C type carbides

KeyWords AITranslate

YG30 Ni-Fe-C alloys TIG Welding η phases

1吴冲浒.我国硬质合金产业近期发展思考[J].稀有金属与硬质合金,2000,28(1):26-30. 被引量:13

2陈飞雄,李世魁.硬质合金与球墨铸铁热等静压扩散连接的研究[J].粉末冶金技术,1995,13(1):8-13. 被引量:6

3[苏]卡扎何夫H.φ.材料的扩散焊接[M].北京:国防工业出版社,1980..

4赵秀娟 等.WC-30Co/S45C钢TIG焊焊接接头复合碳化物形成分析[J].材料科学与工艺,2001,:682-682.

5.YB 882—76.硬质合金金相检验方法[S].,1976..

1王立跃,徐道荣.硬质合金的焊接特点、焊接方法与研发进展[J].现代焊接,2010(12):17-20. 被引量:6

2徐培全,姚舜,杨德新,赵秀娟,芦凤桂,陈春焕,王庆章.Study on the Formation of η Phase During TIG Welding[J].上海交通大学学报:英文版,2004,9(3):6-10.

3翟秋亚,徐锦锋,蔡再生.细直径YG5FA硬质合金/45Cr钢储能焊工艺分析[J].焊接学报,2007,28(8):13-16. 被引量:9

4朱警雷,黄继华,张华,赵兴科.硬质合金与钢异种金属焊接的研究进展[J].焊接,2008(2):15-19. 被引量:27

5刘晓平,杨程,章建军.医用一次性牙钻电容储能焊工艺[J].焊接技术,2009,38(12):39-42.

6吴相省.硬质合金/钢活性液相扩散焊接技术研究[J].硬质合金,2011,28(2):103-110. 被引量:5

7徐培全,芦凤桂,张培磊,杨尚磊,于治水.硬质合金/因瓦合金激光-氩弧复合焊缝界面的显微组织与元素扩散[J].机械工程材料,2011,35(4):4-6. 被引量:2

8罗蒙丽.硬质合金钎焊技术的现状与发展[J].硬质合金,2015,0(2):108-118. 被引量:16

9张一鸣,潘金芝,夏爽,赵秀娟,陈春焕.梯度硬质合金与45钢的TIG焊研究[J].机械制造文摘:焊接分册,2018(5):17-21. 被引量:1

1张军锋,罗维,李晓军,张健阁.旋转导向工具导向头系统机械结构分析[J].中国石油和化工标准与质量,2020(8):179-180.

2翟秋亚,梁存琨,成军,徐锦锋.Cu基微晶钎料高频钎焊0Cr18Ni9Nb/YG6分析[J].焊接学报,2008,29(9):23-26. 被引量:2

3赵一生,高志国,魏世忠,杨涤心.碳钢/钢结硬质合金覆层材料制备及界面分析[J].深圳职业技术学院学报,2009,8(3):67-70. 被引量:1

4郦剑,罗娟,罗来马,俞佳,朱流.硬质合金与钢基体钎焊技术的研究进展[J].材料科学与工程学报,2009,27(6):955-958. 被引量:17

5周承商,易健宏,罗述东,彭元东.硬质合金与Cr12冷作钢的微波焊接工艺[J].焊接学报,2010,31(4):41-44. 被引量:2

6康晶,赵麦群,吕娟,赵雪琴,铃木实平.异种金属铁丝-铜板的电容储能冲击焊接[J].焊接学报,2010,31(4):93-96. 被引量:2

7李卓然,刘兵,樊建新,冯吉才.YG8硬质合金和低碳钢的高频感应钎焊[J].焊接学报,2010,31(10):97-100. 被引量:20

8朱蕾蕾,王海龙.基于CuMnCo钎料的YG6C硬质合金与16Mn钢的真空钎焊工艺研究[J].热加工工艺,2012,41(13):185-187. 被引量:3

9徐峰,翟秋亚,陈凯.细直径TA2/0Cr18Ni9Ti棒材储能焊接试验分析[J].焊接学报,2012,33(6):77-80. 被引量:5

10吕鹏,刘庆梅,徐楠.刃具硬质合金与结构钢钎焊工艺研究[J].中国新技术新产品,2012(19):106-106. 被引量:2

1王浩,杨德新,赵秀娟,陈春焕,王庆章.YG30硬质合金与45^#钢TIG焊接头组织及抗弯强度的研究[J].焊接技术,2005,34(1):9-11. 被引量:2

2王浩,杨德新,赵秀娟,陈春焕,王庆章,赵晓辉.YG30硬质合金与45钢TIG焊接头组织及抗弯强度的研究[J].焊接,2004(8):10-13. 被引量:10

3赵秀娟,王浩,杨德新,王庆章.焊丝成份对YG30/钢焊缝组织和硬度的影响[J].硬质合金,2004,21(2):94-98. 被引量:7

4王莎莎,赵秀娟,陈春焕,宋以国,王庆章.填充材料成分对YG30/焊缝界面区组织及硬度的影响[J].稀有金属与硬质合金,2007,35(1):18-21. 被引量:7

5李莉娜,赵秀娟,徐培全,闫祖翔.YG30硬质合金与因瓦合金TIG焊接头的组织与硬度的分析研究[J].硬质合金,2008,25(4):208-213. 被引量:4

6宋以国,赵秀娟,王莎莎,杨德新,赵晓辉,王庆章.焊后退火对YG30与45钢TIG焊界面组织的影响[J].热加工工艺,2007,36(3):20-22. 被引量:2

7宋以国,赵秀娟,杨德新,赵晓辉,王庆章.YG30硬质合金与45钢TIG焊界面组织的分析[J].硬质合金,2005,22(2):69-73. 被引量:10

8赵秀娟,杨德新,田头孝介,高泽幸治,山森英明,鸭田秀一.YG30硬质合金与45钢TIG焊接头组织中η相[J].焊接学报,2003,24(3):35-38. 被引量:24

9赵秀娟,杨德新,王浩,高泽幸治,山森英明,田头孝介.硬质合金与碳钢电子束对接焊接头的显微组织[J].机械工程材料,2005,29(5):21-23. 被引量:10

10赵秀娟,杨德新.硬质合金YG30/45钢TIG焊连接的研究[J].新技术新工艺,2004(3):34-35. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG14[金属学及工艺—金属材料]

Citation Information:

The welding joints between YG30 and S45C by using Ni-Fe-C alloys as weld metal were obtained by TIG welding.The welding joints were studied by means of optical microscope, SEM, EPMA, X-rays, micro hardness etc. The results showed that the welding joints between YG30 and S45C by TIG welding, can be obtained by using Ni-Fe-C alloys as weld metal,The harmful η phase can be restricted by the addition of C element into Ni-Fe alloys.So the inadequate carbide of the W-Co-C system induced by the C diffusion and the high ingredient Fe are the two vital factors to η phase formation, and η phase was M6C, M12C type carbides

quote

GB/T 7714-2015 [1] XU Pei-quan, YANG De-xin, ZHAO Xiu-juan, et al. Ni-Fe-C Alloy Effect on η-phases Formed during TIG Welding of YG30 with S45C[J]. Rare Metals and Cemented Carbides, 2003(2): 18-23.
MLA [1] XU Pei-quan, et al., "Ni-Fe-C Alloy Effect on η-phases Formed during TIG Welding of YG30 with S45C." Rare Metals and Cemented Carbides, no. 2, 2003, pp. 18-23.
APA [1] XU Pei-quan, YANG De-xin, ZHAO Xiu-juan, CHEN Chun-huan, & WANG Qing-zhang. (2003). Ni-Fe-C Alloy Effect on η-phases Formed during TIG Welding of YG30 with S45C. Rare Metals and Cemented Carbides(2), 18-23.
IEEE [1] XU Pei-quan, YANG De-xin, ZHAO Xiu-juan, CHEN Chun-huan, and WANG Qing-zhang, "Ni-Fe-C Alloy Effect on η-phases Formed during TIG Welding of YG30 with S45C," Rare Metals and Cemented Carbides, no. 2, pp. 18-23, 2003. keywords: {YG30;Ni-Fe-C alloys;TIG Welding;η phases}