The Study on the Density of MoSi_2 Dispersion-strengthened Copper AITranslate
Abstract AITranslate
The MoSi2 dispersion-strengthened copper alloy (DSC)has been preparaed by high-performance ball milling and cold pressing and sintering.The paper analyzed the effect of sintering temperature,ball milling method and compact density on the density of MoSi2 disperslion-strengthened copper alloy.The results show that the largest effect is sintering temperature,the optimal sintering temperature of Mosi2 DSC was 950 ℃;the effect of ball milling metlhod comes the second,but wet-way ball milling is better than dry-way ball milling.There is no distinct effect of compact density on the sintering density.
KeyWords AITranslate
1冯瑞 等.金属物理学(第一卷)[M].北京:科学出版社,2000.570.
2Hirschhom J S. Introduction to powder metallurgy[M], APMI, 1969.
1刘学龙,陈秀娟,袁子洲.机械合金化Mg-Ni二元系储氢合金的研究[J].粉末冶金工业,2004,14(4):34-39. 被引量:1
2冯薇薇,张修庆,宋羽,丁煜寰.球磨制备Cu-Ti-LaB_6复合粉末的研究[J].热加工工艺,2014,43(22):87-89. 被引量:2
3王谦,张寿柏,胡赓祥,孙卫权,吴菊清.富Al的Al-Ti系的机械合金化[J].上海有色金属,1998,19(1):1-7.
4李挺,李益民,陈良建,何浩,胡幼华.注射成形制备多孔钛及其性能[J].稀有金属材料与工程,2011,40(2):335-338. 被引量:5
5宁爱林.MoSi2弥散强化铜的研制[J].邵阳高等专科学校学报,2002,15(3):219-220.
6杨霆,郑军妹,刘晓刚,程永超,罗丰华.烧结温度对420不锈钢组织和性能的影响[J].粉末冶金技术,2016,34(5):373-379. 被引量:12
7贾昌申,肖克民,刘海侠,周好斌.直流TIG电弧的电流密度研究[J].西安交通大学学报,1994,28(4):33-38. 被引量:11
8李松林,刘燚,R. A. Varin,刘怀菲,崔建民,陈仕奇.球磨方式对纳米晶Mg2FeH6储氢材料合成与放氢性能的影响[J].中国有色金属学报,2008,18(1):42-47. 被引量:9
9陈枭,王洪涛,富伟,王芳,白小波.燃气流量对TiB_2-50Co涂层组织及耐磨损腐蚀性能的影响[J].稀有金属,2015,39(3):227-234. 被引量:1
10张元晶,周明,王阳俊.高速铣削SiC_p/Al复合材料表面形貌功率谱密度研究[J].工具技术,2010,44(9):17-20.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.11[金属学及工艺—金属材料]
Citation Information:
The MoSi2 dispersion-strengthened copper alloy (DSC)has been preparaed by high-performance ball milling and cold pressing and sintering.The paper analyzed the effect of sintering temperature,ball milling method and compact density on the density of MoSi2 disperslion-strengthened copper alloy.The results show that the largest effect is sintering temperature,the optimal sintering temperature of Mosi2 DSC was 950 ℃;the effect of ball milling metlhod comes the second,but wet-way ball milling is better than dry-way ball milling.There is no distinct effect of compact density on the sintering density.
quote
| GB/T 7714-2015 | [1] NING Ai-lin, SHEN Qi-zhi, LUO Yu-mei, et al. The Study on the Density of MoSi_2 Dispersion-strengthened Copper[J]. Rare Metals and Cemented Carbides, 2003(2): 24-25. |
| MLA | [1] NING Ai-lin, et al., "The Study on the Density of MoSi_2 Dispersion-strengthened Copper." Rare Metals and Cemented Carbides, no. 2, 2003, pp. 24-25. |
| APA | [1] NING Ai-lin, SHEN Qi-zhi, LUO Yu-mei, & CHEN Guo-xin. (2003). The Study on the Density of MoSi_2 Dispersion-strengthened Copper. Rare Metals and Cemented Carbides(2), 24-25. |
| IEEE | [1] NING Ai-lin, SHEN Qi-zhi, LUO Yu-mei, and CHEN Guo-xin, "The Study on the Density of MoSi_2 Dispersion-strengthened Copper," Rare Metals and Cemented Carbides, no. 2, pp. 24-25, 2003. keywords: {MoSi_2/Cu;sintering density;sintering temperature;ball milling method;compact density} |