Thermodynamic Analysis on Phosphate Decomposition of Scheelite AITranslate

School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Equilibrium diagrams of Ca-W-P-H_2O system are established on the basis of thermodynamic data.The diagrams,which are constructed under conditions of 25 ℃and 0.01 mol/L and 0.5 mol/L of total phosphorus-containing ions concentrations[P], show the effect of system pH value and total phosphorus-containing ions on system equilibrium.The results showed that phosphate solution is an efficient reagent for scheelite decomposition.High [P] is beneficial for the decomposition,but extras phosphate will cause difficulty in purification.In view of stringent requirement of ammonium paratunngstate as the intermediate product for impurity P,the author believe better decomposition can be obtained by proper improvement of pH value with low-concentration free P.

KeyWords AITranslate

scheelite phosphate decomposition thermodynamic analysis concentration logarithm diagram

1李洪桂.稀有高熔点金属(上)[M].北京:冶金工业出版社,1999.36.

2吴建国.白钨矿添加磷酸盐苛性碱浸取的热力学分析[J].化工冶金,1987,8(3):1-1.

3迪安JA 魏俊发译.兰氏化学手册[M].北京:科学出版社,1991..

1马飞,赵中伟,曹才放,张刚,霍广生,陈爱良,李洪桂.硫化钠分解彩钼铅矿热力学研究[J].中国钼业,2008,32(1):44-47. 被引量:9

2赵中伟,曹才放,李洪桂.碳酸钠分解白钨矿的热力学分析[J].中国有色金属学报,2008,18(2):356-360. 被引量:16

3张刚,赵中伟,李江涛,陈爱良,霍广生,李洪桂.氢氧化钠分解钼酸铅矿的热力学分析[J].中南大学学报:自然科学版,2008,39(5):902-906. 被引量:13

4张刚,赵中伟,曹才放,黄少波.磷酸盐分解钼酸钙的热力学[J].北京科技大学学报,2009,31(11):1394-1399. 被引量:5

5曹才放,赵中伟,刘旭恒,王小波.硅酸钠分解白钨矿的热力学研究[J].中国有色金属学报,2012,22(9):2636-2641. 被引量:6

6何贵香,何利华,曹才放,赵中伟,陈星宇,陈爱良,刘旭恒,贺跃辉.氢氧化钠分解白钨矿的热力学分析[J].粉末冶金材料科学与工程,2013,18(3):368-372. 被引量:9

7谭敦强,李亚蕾,杨欣,陆磊,陆德平.杂质元素对钨产品结构及性能的影响[J].材料导报,2013,27(17):98-100. 被引量:5

8曾之琪,肖连生,张贵清.碱性钨萃余液返回高压浸出的试验研究[J].稀有金属与硬质合金,2013,41(6):1-6. 被引量:1

9李江涛,赵中伟,丁文涛.超声波场作用下Na_3PO_4分解白钨矿的动力学[J].中国有色金属学报,2014,24(6):1607-1615. 被引量:6

10何文,谭敦强,朱红波,邝海,欧阳国霞.铈与YG6硬质合金制备过程中富钙相的交互作用[J].粉末冶金材料科学与工程,2016,21(4):515-521. 被引量:2

1张刚,赵中伟,曹才放,黄少波.磷酸盐分解钼酸钙的热力学[J].北京科技大学学报,2009,31(11):1394-1399. 被引量:5

2石玉臣,赵中伟,陈爱良,霍广生,李洪桂.金川镍阳极液硫化除铜的研究[J].有色金属:冶炼部分,2010(2):9-12. 被引量:6

3张文朴.加强钼资源综合利用与再生研发 促进我国生态钼业建设[J].中国钼业,2010,34(2):13-18. 被引量:3

4刘建华,彭瑛,张淑英,沈志农.白钨矿物相组成对浸出率的影响[J].湖南工业大学学报,2010,24(3):1-4.

5赵中伟,石玉臣,陈爱良,霍广生,李洪桂.Cu-Ni-Pb-Zn-Cl-H_2O体系的热力学分析[J].中南大学学报:自然科学版,2010,41(5):1680-1685. 被引量:2

6杨绍文,曹耀华,刘红召,高照国.低品位铅钼粗精矿浸出氧化钼的研究[J].有色金属:冶炼部分,2011(5):31-33. 被引量:3

7涂松柏,曹才放,赵中伟.EDTA浸出白钨矿的热力学分析[J].中国钨业,2011,26(3):27-30. 被引量:1

8郭万根,石玉臣,王含渊,张吉贵,黄蕴成,许新启.Co-Cu-Zn-Pb-Ni-Cl-H_2O体系的热力学分析[J].有色金属:冶炼部分,2011(9):5-8. 被引量:1

9梁勇,林如丹,张刚.化学共沉淀法制备纳米级NiFeCo合金前驱体的热力学分析[J].湿法冶金,2011,30(4):304-308. 被引量:2

10张好强,王莉娜,贾晓鸣,宋月星.硬质合金刀具中WC的浸出机理研究[J].稀有金属与硬质合金,2012,40(4):59-62.

1张刚,赵中伟,曹才放,黄少波.磷酸盐分解钼酸钙的热力学[J].北京科技大学学报,2009,31(11):1394-1399. 被引量:5

2丁治英,赵中伟.氟盐溶液浸出白钨矿的热力学分析[J].稀有金属与硬质合金,2004,32(1):8-10. 被引量:10

3杨幼明,万林生,张子岩.碱性条件下磷酸盐分解白钨试验研究[J].中国钨业,2006,21(5):32-36. 被引量:10

4何贵香,何利华,曹才放,赵中伟,陈星宇,陈爱良,刘旭恒,贺跃辉.氢氧化钠分解白钨矿的热力学分析[J].粉末冶金材料科学与工程,2013,18(3):368-372. 被引量:9

5吴金玲,李江涛,刘旭恒,陈星宇,何利华.碳酸钠选择性浸出钨钼混合矿的热力学[J].有色金属科学与工程,2013,4(5):33-38. 被引量:2

6马飞,赵中伟,曹才放,张刚,霍广生,陈爱良,李洪桂.硫化钠分解彩钼铅矿热力学研究[J].中国钼业,2008,32(1):44-47. 被引量:9

7史海燕,赵中伟.苛性钠分解黑钨矿的热力学分析[J].中国钨业,2006,21(5):24-27. 被引量:7

8赵中伟,曹才放,李洪桂.碳酸钠分解白钨矿的热力学分析[J].中国有色金属学报,2008,18(2):356-360. 被引量:16

9邱以清,刘振宇,周国平,王国栋.双辊连铸磷铜钢薄带异常偏析的研究[J].材料与冶金学报,2013,12(2):132-135. 被引量:1

10肖超,曾理,肖连生.钼酸钙酸分解热力学分析及其应用[J].有色金属科学与工程,2017,8(2):14-18. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF111.31[冶金工程—冶金物理化学]

Citation Information:

Equilibrium diagrams of Ca-W-P-H_2O system are established on the basis of thermodynamic data.The diagrams,which are constructed under conditions of 25 ℃and 0.01 mol/L and 0.5 mol/L of total phosphorus-containing ions concentrations[P], show the effect of system pH value and total phosphorus-containing ions on system equilibrium.The results showed that phosphate solution is an efficient reagent for scheelite decomposition.High [P] is beneficial for the decomposition,but extras phosphate will cause difficulty in purification.In view of stringent requirement of ammonium paratunngstate as the intermediate product for impurity P,the author believe better decomposition can be obtained by proper improvement of pH value with low-concentration free P.

quote

GB/T 7714-2015 [1] WANG Shi-bo, ZHAO Zhong-wei, LI Hong-gui. Thermodynamic Analysis on Phosphate Decomposition of Scheelite[J]. Rare Metals and Cemented Carbides, 2005(1): 1-4.
MLA [1] WANG Shi-bo, et al., "Thermodynamic Analysis on Phosphate Decomposition of Scheelite." Rare Metals and Cemented Carbides, no. 1, 2005, pp. 1-4.
APA [1] WANG Shi-bo, ZHAO Zhong-wei, & LI Hong-gui. (2005). Thermodynamic Analysis on Phosphate Decomposition of Scheelite. Rare Metals and Cemented Carbides(1), 1-4.
IEEE [1] WANG Shi-bo, ZHAO Zhong-wei, and LI Hong-gui, "Thermodynamic Analysis on Phosphate Decomposition of Scheelite," Rare Metals and Cemented Carbides, no. 1, pp. 1-4, 2005. keywords: {scheelite;phosphate decomposition;thermodynamic analysis;concentration logarithm diagram}