Extraction of Vanadium from the Carbonaceous and Siliceous Vanadium Shale AITranslate
Abstract AITranslate
Description is made of the property of carbonaceous and sdiceous vanadmm staale and test resmts on processes of direct acid leaching and blank oxidization and roasting acid leaching for vanadium extraction from the ROM ore. Comparison of technical and economic index shows that the use o{ ROM ore direct acid leaching resulted in 20.1~ less investment,1.85 ~ higher FIRR on investment (pre-income tax) and 0.28 year shorter investment return period, yet 4.8% more specific processing cost for per ton of ROM ore. This process is characterized by short process flowsheet, simple and sophisticated process,energy-saving and en- vironmentally friendly and easy for commercial production,It can he used for reference and popularized for similar vanadium mineral processing.
KeyWords AITranslate
1鲁兆伶.用酸法从石煤中提取五氧化二钒的试验研究与工业实践[J].湿法冶金,2002,21(4):175-183. 被引量:139
2刘利军,李继壁,宾智勇,卫亚儒.陕西某碳硅质钒矿提钒工艺研究[J].有色金属:选矿部分,2006(3):28-30. 被引量:15
1孙伟,辜小川,刘润清,马岩,郑博明.某炭质石煤钒矿中钒的赋存状态及其浮选研究[J].矿冶工程,2013,33(6):28-31. 被引量:9
2辜小川,孙伟,刘润清,宋韶博,陈秀珍.湖南某脱碳石煤的选矿试验研究[J].有色金属:选矿部分,2014(5):67-71. 被引量:8
3庄树新,刘翼民,曾盛伟,陈晓彬,张晶晶.从硅质岩钒矿酸浸液中萃取钒的工艺优化[J].厦门理工学院学报,2015,23(3):25-30. 被引量:1
4蒋京航,叶国华,张世民,张爽.石煤直接酸浸提钒工艺研究进展[J].矿冶,2016,25(6):35-39. 被引量:12
5刘立平,沙占魁,张随成,王群英.某钒矿石提钒工艺试验的比较研究[J].贵州地质,2017,34(1):45-49. 被引量:1
1胡洋,何东升,谢志豪,吴玉元,李克尧.石煤型钒矿预富集技术研究现状[J].金属矿山,2018,47(12):73-79. 被引量:14
2辜小川,孙伟,刘润清,宋韶博,陈秀珍.湖南某脱碳石煤的选矿试验研究[J].有色金属:选矿部分,2014(5):67-71. 被引量:8
3宋裕华,李正要,冯金敏.方山口石煤钒矿选碳的试验研究[J].矿冶工程,2014,34(5):66-69. 被引量:2
4刘佳鹏,孙伟,王丽,刘新运,张明明.陕西某石煤钒矿的新型选矿工艺研究[J].有色金属:选矿部分,2015(2):58-63. 被引量:11
5张丽敏,韦华祖,叶从新,魏党生,蒋素芳.某高钙银钒石煤矿综合回收银钒选矿工艺试验研究[J].湖南有色金属,2015,31(5):6-9. 被引量:2
6张丽敏,叶从新,魏党生.某石煤钒矿磨矿以及预先抛尾工艺试验[J].现代矿业,2015,0(11):63-66. 被引量:3
7储焰平,高龙,肖赛君,章俊.矿热电炉处理粘土钒矿生产钒铁合金新工艺[J].铁合金,2016,0(2):9-12. 被引量:1
8张丽敏.某高钙镁石煤钒矿选矿工艺研究[J].有色金属:选矿部分,2016(4):33-38. 被引量:2
9刘春,张一敏,包申旭,汤家焰.选择性磨矿对含钒石煤单体解离的影响研究[J].有色金属:选矿部分,2016(5):39-44. 被引量:6
10杨大锦.2016年云南冶金年评[J].云南冶金,2017,46(2):58-78.
1林经萍,刘耀驰,庄树新,刘后芝,孔秀.从高硅质钒矿浸出液中萃取钒的工艺研究[J].广州化工,2015,43(3):70-71. 被引量:3
2邢兆文.提高转炉煤气回收量途径的分析[J].冶金动力,1994(3):38-41. 被引量:1
3汪志家.转底炉生产直接还原铁用于炼钢的设想[J].鞍钢技术,1994(3):7-11. 被引量:1
4吴卫煌.氯酸钠分金试验研究及工业应用[J].黄金,2017,38(3):68-70. 被引量:2
5G.J.Desroches,李瑞兴.哈得逊湾采矿与熔炼有限公司锌厂的最新发展[J].中国有色冶金,1989(4):25-30.
6周静.唐钢360m^2烧结机低成本生产实践[J].甘肃冶金,2016,38(2):13-17.
7周静.唐钢360m^2烧结机低成本生产实践[J].四川冶金,2016,38(3):6-11.
8硬质合金价格7月开始上调[J].中国钨业,1993,0(10):33-33.
9李祖芳.画眉坳钨矿用浮选法生产低钙钨产品效益显著[J].中国钨业,1991,0(3):36-36.
10刘祖波.浅析锰硅合金中矿石综合锰含量的最佳控制[J].铁合金,2007,38(3):13-15.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
Description is made of the property of carbonaceous and sdiceous vanadmm staale and test resmts on processes of direct acid leaching and blank oxidization and roasting acid leaching for vanadium extraction from the ROM ore. Comparison of technical and economic index shows that the use o{ ROM ore direct acid leaching resulted in 20.1~ less investment,1.85 ~ higher FIRR on investment (pre-income tax) and 0.28 year shorter investment return period, yet 4.8% more specific processing cost for per ton of ROM ore. This process is characterized by short process flowsheet, simple and sophisticated process,energy-saving and en- vironmentally friendly and easy for commercial production,It can he used for reference and popularized for similar vanadium mineral processing.
quote
| GB/T 7714-2015 | [1] LI Xiao-jian. Extraction of Vanadium from the Carbonaceous and Siliceous Vanadium Shale[J]. Rare Metals and Cemented Carbides, 2011(4): 1-3. |
| MLA | [1] LI Xiao-jian. "Extraction of Vanadium from the Carbonaceous and Siliceous Vanadium Shale." Rare Metals and Cemented Carbides, no. 4, 2011, pp. 1-3. |
| APA | [1] LI Xiao-jian. (2011). Extraction of Vanadium from the Carbonaceous and Siliceous Vanadium Shale. Rare Metals and Cemented Carbides(4), 1-3. |
| IEEE | [1] LI Xiao-jian, "Extraction of Vanadium from the Carbonaceous and Siliceous Vanadium Shale," Rare Metals and Cemented Carbides, no. 4, pp. 1-3, 2011. keywords: {vanadium ore;carbonaceous and siliceous vanadium shale;acid leaching;roasting;vanadium extraction} |