daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on the Removal of Ammonia from APT Crystal Mother Liquor AITranslate

School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology;School of Metallurgy and Chemistry Engineering, Jiangxi University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ammonia in APT crystal mother liquor was removed by adding sodium tungstate with sodium hydroxide and magnesium salts. The results show that the content of ammonia in the treated solution can be removed down to 0. 042 g/L up to 98.88% removal rate. The resultant sodium tungstate solution was diluted 10 times before prepared as ion exchange feed solution, the content of ammonia in the raffinate is less than 0. 000 5 % ,which can meet China national discharge standard.

KeyWords AITranslate

APT crystal mother liquor ammonia removal by converting Mg salt precipitation

1徐迎春,姜萍.仲钨酸铵结晶母液的回收与利用[J].稀有金属与硬质合金,2004,32(3):29-31. 被引量:4

2张贵清,尚广浩,肖连生.纳滤法处理仲钨酸铵结晶母液的研究[J].稀有金属,2007,31(3):346-350. 被引量:7

3刘久清,周康根,张启修,龚柏凡.处理仲钨酸铵结晶母液的研究[J].无机盐工业,2002,34(4):1-3. 被引量:2

4钟理,谭春伟,胡孙林,刘军,徐光明,陈微明,廖平.氨氮废水降解技术进展[J].化工科技,2002,10(2):59-62. 被引量:34

1万林生,邓登飞,赵立夫,李红超,徐国钻,梁勇.钨绿色冶炼工艺研究方向和技术进展[J].有色金属科学与工程,2013,4(5):15-18. 被引量:18

1万林生,舒柳飞,赵立夫,谌勇明,李红超.黑钨矿与碳酸钙人工合成白钨的反应过程和机理[J].稀有金属与硬质合金,2014,42(2):1-4. 被引量:3

2万林生,黄小晶,杨亮,邓登飞,李红超,谌勇明.钨酸钠溶液氢氧化钙苛化-沉淀白钨的研究[J].有色金属科学与工程,2014,5(4):23-27. 被引量:3

3黄泽辉,韩宝军,邓登飞,龚丹丹,邓声华,李红超.煤渣过滤调酸钨冶炼废水的研究[J].赣南师范学院学报,2014,35(6):46-48. 被引量:1

4万林生,潘明然,谌勇明,赵立夫,李红超.黑钨矿与碳酸钙人工合成白钨工艺研究[J].稀有金属与硬质合金,2014,42(6):1-3.

5刘飞飞,罗贤平,辛鹏武,龚亚忠.基于机器视觉的钨浓度在线检测系统[J].中国钨业,2015,30(6):73-76. 被引量:1

6刘飞飞,罗贤平,古帅奇,辛鹏武.碱煮过程浸出率预测与优化研究[J].有色金属:冶炼部分,2016(5):29-32. 被引量:1

7万林生,张龙辉,赖星任,杨亮,梁勇,刘鹏.(NH_4)_2HPO_4-H_2O系仲钨酸铵溶解性能及磷钨杂多酸形成的影响[J].稀有金属与硬质合金,2016,44(3):1-4. 被引量:1

8万林生,金先文,赖星任,杨亮,刘鹏,梁勇.(NH_4)_2HPO_4-NH_3·H_2O-H_2O系APT溶解度研究[J].稀有金属与硬质合金,2016,44(5):6-10. 被引量:1

9杨金洪,李江涛,刘文婷,赵中伟.硝酸-磷酸混合溶液中钨的萃取[J].中国有色金属学报,2018,28(5):1024-1032. 被引量:2

10曹才放,章行,李小文,邱晓辰,李昱芃,钟镇宇,王艺瞾,王建松.氯型季铵树脂对钨酸根吸附的热力学研究[J].有色金属科学与工程,2018,9(3):1-4. 被引量:2

1路辉,谢刚,俞小花,李荣兴.仲钨酸铵结晶母液处理技术研究进展[J].稀有金属与硬质合金,2009,37(4):44-47. 被引量:5

2徐迎春,姜萍.仲钨酸铵结晶母液的回收与利用[J].稀有金属与硬质合金,2004,32(3):29-31. 被引量:4

3梅东海.由仲钨酸铵结晶母液提钨的工艺方法[J].中国钨业,1990(10):18-20. 被引量:1

4一种从仲钨酸铵结晶母液中回收钨和氯化铵的方法[J].化学试剂,2008,30(1):76-76.

5邓解德.离子交换法回收仲钨酸铵结晶母液中的钨[J].中国钨业,1999,14(1):29-32. 被引量:7

6卢勇甘.仲钨酸铵结晶母液处理技术的发展与工艺评价[J].中国钨业,2012,27(5):29-31. 被引量:1

7张贵清,尚广浩,肖连生.纳滤法处理仲钨酸铵结晶母液的研究[J].稀有金属,2007,31(3):346-350. 被引量:7

8朱同浩.余碱分解法回收仲钨酸铵结晶母液中钨的工业实践[J].中国钨业,1991,0(7):14-16. 被引量:4

9陈树茂,郭永忠.离子交换法处理仲钨酸铵结晶母液试验与实践[J].中国钨业,2001,16(3):22-24. 被引量:14

10韩曙祥.用离子交换处理仲钨酸铵结晶母液工艺探讨[J].中国钨业,1993,0(5):10-13.

Basic Information:

DOI:

Chinese Library Classification Number:TF803.25[冶金工程—有色金属冶金]

Citation Information:

Ammonia in APT crystal mother liquor was removed by adding sodium tungstate with sodium hydroxide and magnesium salts. The results show that the content of ammonia in the treated solution can be removed down to 0. 042 g/L up to 98.88% removal rate. The resultant sodium tungstate solution was diluted 10 times before prepared as ion exchange feed solution, the content of ammonia in the raffinate is less than 0. 000 5 % ,which can meet China national discharge standard.

quote

GB/T 7714-2015 [1] WAN Lin-sheng, GONG Dan-dan, FU Zan-hui, et al. Study on the Removal of Ammonia from APT Crystal Mother Liquor[J]. Rare Metals and Cemented Carbides, 2011(4): 4-7.
MLA [1] WAN Lin-sheng, et al., "Study on the Removal of Ammonia from APT Crystal Mother Liquor." Rare Metals and Cemented Carbides, no. 4, 2011, pp. 4-7.
APA [1] WAN Lin-sheng, GONG Dan-dan, FU Zan-hui, LI Hong-chao, & SUN Li. (2011). Study on the Removal of Ammonia from APT Crystal Mother Liquor. Rare Metals and Cemented Carbides(4), 4-7.
IEEE [1] WAN Lin-sheng, GONG Dan-dan, FU Zan-hui, LI Hong-chao, and SUN Li, "Study on the Removal of Ammonia from APT Crystal Mother Liquor," Rare Metals and Cemented Carbides, no. 4, pp. 4-7, 2011. keywords: {APT;crystal mother liquor;ammonia removal by converting;Mg salt precipitation}