Nanoscale Heterostructured Materials Based on Metal Oxides for a Chemiresistive Gas Sensor AITranslate

Tezpur University; Tezpur University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nanomaterials with exceptional physical and chemical properties are the key to the success of the next generation of gas sensor technology, which is expected to have special features like being lightweight and flexible for wearability, mechanical robustness, reliable operation with wide environmental changes, and self-powered, in addition to the general sensor characteristics. The design of the chemiresistor with nanostructured hybrid material has indicated a great potential to meet these current demands, drawing significant attention to the technological developments in the past decades. The nanotechnology driven strategic design of the hybrid nanostructures is predicted to be pivotal for the development of nanomaterials bearing distinct physical and chemical properties and catalytic power, enabling them to produce overall improvements in sensor efficiency. In this review, a comprehensive review on the recent progress of hybrid gas sensors fabricated by coupling various metal oxides and 2D materials like transition metal dichalcogenides, graphene, and its derivatives are presented. The limitations of the current materials, key challenges, as well as the futuristic strategy for material design delivering fascinating properties and modern growth techniques are highlighted. A special emphasis has been given to hybrid sensors made with transition metal dichalcogenides, which are considered to be an emerging material and very few works have reported on its hybrid with metal oxides. The relevance of reliable detection of hydrogen is felt due to the dramatic rise in the use of hydrogen in industrial, commercial, and household purposes. As the whole world is moving toward a hydrogen economy, reliable, accurate, and robust hydrogen sensors will be a crucial component of the technological systems. In view of this, the current status and recent progress on hydrogen sensors based on heterostructured nanomaterials are also presented to the reader.

KeyWords AITranslate

chemiresistor heterojunction metal oxide transitional metal dichalcogenides graphene
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c00841

Chinese Library Classification Number:

Citation Information:

Nanomaterials with exceptional physical and chemical properties are the key to the success of the next generation of gas sensor technology, which is expected to have special features like being lightweight and flexible for wearability, mechanical robustness, reliable operation with wide environmental changes, and self-powered, in addition to the general sensor characteristics. The design of the chemiresistor with nanostructured hybrid material has indicated a great potential to meet these current demands, drawing significant attention to the technological developments in the past decades. The nanotechnology driven strategic design of the hybrid nanostructures is predicted to be pivotal for the development of nanomaterials bearing distinct physical and chemical properties and catalytic power, enabling them to produce overall improvements in sensor efficiency. In this review, a comprehensive review on the recent progress of hybrid gas sensors fabricated by coupling various metal oxides and 2D materials like transition metal dichalcogenides, graphene, and its derivatives are presented. The limitations of the current materials, key challenges, as well as the futuristic strategy for material design delivering fascinating properties and modern growth techniques are highlighted. A special emphasis has been given to hybrid sensors made with transition metal dichalcogenides, which are considered to be an emerging material and very few works have reported on its hybrid with metal oxides. The relevance of reliable detection of hydrogen is felt due to the dramatic rise in the use of hydrogen in industrial, commercial, and household purposes. As the whole world is moving toward a hydrogen economy, reliable, accurate, and robust hydrogen sensors will be a crucial component of the technological systems. In view of this, the current status and recent progress on hydrogen sensors based on heterostructured nanomaterials are also presented to the reader.

quote

GB/T 7714-2015 [1] Biplob Mondal, Pranjal Kumar Gogoi. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c00841.
MLA [1] Biplob Mondal, and Pranjal Kumar Gogoi. ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c00841.
APA [1] Biplob Mondal, & Pranjal Kumar Gogoi. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c00841
IEEE [1] Biplob Mondal and Pranjal Kumar Gogoi, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c00841. keywords: {chemiresistor heterojunction metal oxide transitional metal dichalcogenides graphene}