daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Carbon-Based Quantum Dots for Photovoltaic Devices: A Review Carbon-Based Quantum Dots for Photovoltaic Devices: A Review AITranslate

Department of Chemical Engineering, The Cooper Union for the Advancement of Science and Art; SRM University-AP;Institut National de la Recherche Scientifique-Centre Énergie Materiaux Télecommunications (INRS-EMT); Yonsei University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Interest in carbon quantum dots (CQDs) has recently boomed due to their potential to enhance the performance of various solar technologies as nontoxic, naturally abundant, and cleanly produced nanomaterials. CQDs and their other variations, such as nitrogen-doped carbon quantum dots (NCQDs) and graphene quantum dots (GQDs), have improved the performance of luminescent solar concentrators (LSCs) and photovoltaic (PV) cells due to their excellent optical properties. As fluorophores in LSCs, CQDs are mostly transparent to visible light and have absorption/re-emission spectra that can be easily controlled. The outstanding optical properties of CQDs make them promising materials to replace expensive, heavy-metal-based fluorophores. Various CQDs have also been used as or doped into the photoanode, counter electrode, hole transport layer (HTL), and electron transport layer (ETL) of dye-sensitized solar cells (DSSCs), organic solar cells (OSC), perovskite solar cells (PSCs), and other PV cell configurations. The addition of CQDs into the various solar cell components has reduced electron recombination, increased charge density, and boosted electron mobility, improving the performance of the PV cells. Enhancing the power conversion efficiency (PCE) of photovoltaic devices is essential in propagating green energy technology. Thus, CQDs offer an affordable, safe, and environmentally friendly method to advance photovoltaic performance.

KeyWords AITranslate

carbon quantum dots solar concentrator photoanode counter electrode hole transport layer and electron transport layer
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c00783

Chinese Library Classification Number:

Citation Information:

Interest in carbon quantum dots (CQDs) has recently boomed due to their potential to enhance the performance of various solar technologies as nontoxic, naturally abundant, and cleanly produced nanomaterials. CQDs and their other variations, such as nitrogen-doped carbon quantum dots (NCQDs) and graphene quantum dots (GQDs), have improved the performance of luminescent solar concentrators (LSCs) and photovoltaic (PV) cells due to their excellent optical properties. As fluorophores in LSCs, CQDs are mostly transparent to visible light and have absorption/re-emission spectra that can be easily controlled. The outstanding optical properties of CQDs make them promising materials to replace expensive, heavy-metal-based fluorophores. Various CQDs have also been used as or doped into the photoanode, counter electrode, hole transport layer (HTL), and electron transport layer (ETL) of dye-sensitized solar cells (DSSCs), organic solar cells (OSC), perovskite solar cells (PSCs), and other PV cell configurations. The addition of CQDs into the various solar cell components has reduced electron recombination, increased charge density, and boosted electron mobility, improving the performance of the PV cells. Enhancing the power conversion efficiency (PCE) of photovoltaic devices is essential in propagating green energy technology. Thus, CQDs offer an affordable, safe, and environmentally friendly method to advance photovoltaic performance.

quote

GB/T 7714-2015 [1] Andrew Kim, Jatis Kumar Dash, Pawan Kumar, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c00783.
MLA [1] Andrew Kim, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c00783.
APA [1] Andrew Kim, Jatis Kumar Dash, Pawan Kumar, & Rajkumar Patel. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c00783
IEEE [1] Andrew Kim, Jatis Kumar Dash, Pawan Kumar, and Rajkumar Patel, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c00783. keywords: {carbon quantum dots solar concentrator photoanode counter electrode hole transport layer and electron transport layer}