Emergence of Structural Phosphorescence in Free-Standing, Laterally Organized Polymer Nanofiber Membranes AITranslate

Karlsruhe Institute of Technology (KIT); Karlsruhe Institute of Technology (KIT); University of Michigan; University of Michigan; University of Michigan; Karlsruhe Institute of Technology (KIT); Karlsruhe Institute of Technology (KIT); Karlsruhe Institute of Technology (KIT); Karlsruhe Institute of Technology (KIT); University of Michigan; Cornell University; University of Michigan
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In the past decade, the phosphorescence of metal-free confined polymer structures has generated interest in optoelectronics due to their sustainability, low toxicity, and deployment in sensing applications. Herein, a free-standing array of laterally organized nanofibers was prepared via templated chemical vapor deposition polymerization into a liquid crystalline (LC) phase, and their optical properties were compared to compositionally identical films. The fibers converge into laterally aligned membranes that maintain a high internal order despite the surfaces of the membranes remaining uniform and closed. The membranes consisted of hourglass-shaped nanofibers with features in the micro- and nanometer regime. Free-standing nanofiber membranes differ from polymer films of equivalent chemical composition in several key features: (1) Anisotropic growth of polymer nanofibers with constraint and compliance to an LC template, (2) a high surface-to-volume ratio, and (3) the occurrence of a long-lived emission in the blue region, which persists for multiple seconds after excitation. This study constitutes the first report of long-lived emission from solid-state poly(p-xylylenes) nanofibers. Prospective applications of morphologically controlled polymer arrays with structural luminescence include organic sensors and optoelectronic devices.

KeyWords AITranslate

liquid crystal (LC) templated chemical vapor deposition (CVD) 3D laterally organized freestanding nanofiber membranes surface Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01477

Chinese Library Classification Number:

Citation Information:

In the past decade, the phosphorescence of metal-free confined polymer structures has generated interest in optoelectronics due to their sustainability, low toxicity, and deployment in sensing applications. Herein, a free-standing array of laterally organized nanofibers was prepared via templated chemical vapor deposition polymerization into a liquid crystalline (LC) phase, and their optical properties were compared to compositionally identical films. The fibers converge into laterally aligned membranes that maintain a high internal order despite the surfaces of the membranes remaining uniform and closed. The membranes consisted of hourglass-shaped nanofibers with features in the micro- and nanometer regime. Free-standing nanofiber membranes differ from polymer films of equivalent chemical composition in several key features: (1) Anisotropic growth of polymer nanofibers with constraint and compliance to an LC template, (2) a high surface-to-volume ratio, and (3) the occurrence of a long-lived emission in the blue region, which persists for multiple seconds after excitation. This study constitutes the first report of long-lived emission from solid-state poly(p-xylylenes) nanofibers. Prospective applications of morphologically controlled polymer arrays with structural luminescence include organic sensors and optoelectronic devices.

quote

GB/T 7714-2015 [1] Mirella Wawryszyn, Robin Wilhelm, John Kim, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01477.
MLA [1] Mirella Wawryszyn, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01477.
APA [1] Mirella Wawryszyn, Robin Wilhelm, John Kim, Xiaoyang Zhong, Jeffery E. Raymond, Richard Thelen, Vanessa Trouillet, Matthias Schwotzer, Stefan Bräse, Do Hoon Kim, Nicholas L. Abbott, & Joerg Lahann. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01477
IEEE [1] Mirella Wawryszyn, Robin Wilhelm, John Kim, Xiaoyang Zhong, Jeffery E. Raymond, Richard Thelen, Vanessa Trouillet, Matthias Schwotzer, Stefan Bräse, Do Hoon Kim, Nicholas L. Abbott, and Joerg Lahann, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01477. keywords: {liquid crystal (LC) templated chemical vapor deposition (CVD);3D laterally organized freestanding nanofiber membranes;surface;Show More}