Eco-Friendly Hierarchical Nanoporous Microfiber Respirator Filters Fabricated Using Rotary Jet Spinning Technology (RJS) AITranslate
Abstract AITranslate
The current global health crisis caused by the SARS-CoV-2 virus (COVID-19) has increased the use of personal protective equipment, especially face masks, leading to the disposal of a large amount of plastic waste causing an environmental crisis due to the use of non-biodegradable and non-recyclable polymers, such as polypropylene and polyester. In this work, an eco-friendly biopolymer, polylactic acid (PLA), was used to manufacture hierarchical nanoporous microfiber biofilters via a single-step rotary jet spinning (RJS) technique. The process parameters that aid the formation of nanoporosity within the microfibers were discussed. The microstructure of the fibers was analyzed by scanning electron microscopy (SEM) and a noninvasive X-ray microtomography (XRM) technique was employed to study the three-dimensional (3D) morphology and the porous architecture. Particulate matter (PM) and aerosol filtration efficiency were tested by OSHA standards with a broad range (10–1000 nm) of aerosolized saline droplets. The viral penetration efficiency was tested using the ΦX174 bacteriophage (∼25 nm) with an envelope, mimicking the spike protein structure of SARS-CoV-2. Although these fibers have a similar size used in N95 filters, the developed biofilters present superior filtration efficiency (∼99%) while retaining better breathability (<4% pressure drop) than N95 respirator filters.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01387
Chinese Library Classification Number:
Citation Information:
The current global health crisis caused by the SARS-CoV-2 virus (COVID-19) has increased the use of personal protective equipment, especially face masks, leading to the disposal of a large amount of plastic waste causing an environmental crisis due to the use of non-biodegradable and non-recyclable polymers, such as polypropylene and polyester. In this work, an eco-friendly biopolymer, polylactic acid (PLA), was used to manufacture hierarchical nanoporous microfiber biofilters via a single-step rotary jet spinning (RJS) technique. The process parameters that aid the formation of nanoporosity within the microfibers were discussed. The microstructure of the fibers was analyzed by scanning electron microscopy (SEM) and a noninvasive X-ray microtomography (XRM) technique was employed to study the three-dimensional (3D) morphology and the porous architecture. Particulate matter (PM) and aerosol filtration efficiency were tested by OSHA standards with a broad range (10–1000 nm) of aerosolized saline droplets. The viral penetration efficiency was tested using the ΦX174 bacteriophage (∼25 nm) with an envelope, mimicking the spike protein structure of SARS-CoV-2. Although these fibers have a similar size used in N95 filters, the developed biofilters present superior filtration efficiency (∼99%) while retaining better breathability (<4% pressure drop) than N95 respirator filters.
quote
| GB/T 7714-2015 | [1] Kavin Sivaneri Varadharajan Idhaiam, Gloria Oporto, Matthew Barre, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01387. |
| MLA | [1] Kavin Sivaneri Varadharajan Idhaiam, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01387. |
| APA | [1] Kavin Sivaneri Varadharajan Idhaiam, Gloria Oporto, Matthew Barre, Masako Terada, Jonathan Boyd, William Goldsmith, Timothy Nurkiewicz, Rakesh K. Gupta, & Edward M. Sabolsky. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01387 |
| IEEE | [1] Kavin Sivaneri Varadharajan Idhaiam, Gloria Oporto, Matthew Barre, Masako Terada, Jonathan Boyd, William Goldsmith, Timothy Nurkiewicz, Rakesh K. Gupta, and Edward M. Sabolsky, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01387. keywords: {nanostructured biopolymer;sustainable manufacturing;textured PLA fibers;SARSCoV2;Xray microtomography (XRM)} |