Interfacial adhesion influences mechanical strength, structural integrity, and overall performance for adhesively bonded structures and composite materials. In this work, we investigate the effect of resin formulation chemistry on wetting behavior and interfacial adhesion with a glass substrate. Thermosetting elastomer resin and cured network properties, including viscosity, surface tension, glass transition temperature, and molecular weight between cross-links, were also characterized, and the relative importance of these properties on adhesive strength was evaluated. Resin wettability was found to be the factor most predictive of adhesive strength between thermosetting elastomers and glass surfaces, with increasing wettability (decreasing resin contact angle) correlated with increasing interfacial fracture energy. This finding provides a convenient and fast method to screen polymer networks and enables informed tailoring of interfacial fracture energy.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00217
Chinese Library Classification Number:
Citation Information:
Interfacial adhesion influences mechanical strength, structural integrity, and overall performance for adhesively bonded structures and composite materials. In this work, we investigate the effect of resin formulation chemistry on wetting behavior and interfacial adhesion with a glass substrate. Thermosetting elastomer resin and cured network properties, including viscosity, surface tension, glass transition temperature, and molecular weight between cross-links, were also characterized, and the relative importance of these properties on adhesive strength was evaluated. Resin wettability was found to be the factor most predictive of adhesive strength between thermosetting elastomers and glass surfaces, with increasing wettability (decreasing resin contact angle) correlated with increasing interfacial fracture energy. This finding provides a convenient and fast method to screen polymer networks and enables informed tailoring of interfacial fracture energy.
quote
| GB/T 7714-2015 | [1] Ye Wang, Christopher J. Hansen, Ian M. McAninch, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00217. |
| MLA | [1] Ye Wang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00217. |
| APA | [1] Ye Wang, Christopher J. Hansen, Ian M. McAninch, E. Jason Robinette, & Amy M. Peterson. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00217 |
| IEEE | [1] Ye Wang, Christopher J. Hansen, Ian M. McAninch, E. Jason Robinette, and Amy M. Peterson, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00217. keywords: {thermosetting elastomers;resin wettability;viscosity;glass transition temperature;viscoelastic behavior;interfacial adhesion} |