Electronic structure and optical gain of InAsSbN/InAs quantum dots AITranslate

Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The electronic structure and optical gain of InAsSbN/InAs QDs are investigated in the framework of effective-mass envelope function theory. The strain distribution is calculated using the valence force field (VFF) method. When the composition of Sb increases, both the conduction and valence bands offset and the compressive strain increase, and the transition energy decreases and the strained band alignment may change from type I to type II. The added nitrogen can reduce the compressive strain in QD, and it reduces the C1-HH1 transition energy due to the strong repulsion between nitrogen resonant band and conduction band. When the Sb composition increases, the overlapping of wave-functions of electrons and holes are less efficient, the optical transition matrix element decreases. For the optical gain, we should consider the factors including the transition matrix element, the matrix element of Kane’s theory, the refractive index and Fermi-Dirac distributions for electrons fc in the conduction bands and holes fv in the valence bands. So depending on the specific application requirements, we should select the appropriate compositions of Sb and N accordingly.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.01.038

Chinese Library Classification Number:

Citation Information:

The electronic structure and optical gain of InAsSbN/InAs QDs are investigated in the framework of effective-mass envelope function theory. The strain distribution is calculated using the valence force field (VFF) method. When the composition of Sb increases, both the conduction and valence bands offset and the compressive strain increase, and the transition energy decreases and the strained band alignment may change from type I to type II. The added nitrogen can reduce the compressive strain in QD, and it reduces the C1-HH1 transition energy due to the strong repulsion between nitrogen resonant band and conduction band. When the Sb composition increases, the overlapping of wave-functions of electrons and holes are less efficient, the optical transition matrix element decreases. For the optical gain, we should consider the factors including the transition matrix element, the matrix element of Kane’s theory, the refractive index and Fermi-Dirac distributions for electrons fc in the conduction bands and holes fv in the valence bands. So depending on the specific application requirements, we should select the appropriate compositions of Sb and N accordingly.

quote

GB/T 7714-2015 [1] J. Chen, W.J. Fan, Q. Xu, et al. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.01.038.
MLA [1] J. Chen, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.01.038.
APA [1] J. Chen, W.J. Fan, Q. Xu, & X.W. Zhang. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.01.038
IEEE [1] J. Chen, W.J. Fan, Q. Xu, and X.W. Zhang, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.01.038.