daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Cure-Dependent Morphology of Acrylic/Alkyd Hybrid Latex Films via Nanomechanical Mapping AITranslate

University of the Basque Country UPV/EHU; University of the Basque Country UPV/EHU; University of the Basque Country UPV/EHU; University of the Basque Country UPV/EHU
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Acrylic/alkyd hybrid latexes offer the potential to obtain hard films from waterborne polymer dispersions without using coalescing agents. However, despite being widely used commercially, the curing process of the alkyd resin used in such formulations, and its influence on the final film morphology, remain poorly understood. In this work, we explore the curing process and its influence on film morphology in alkyd/acrylic hybrid latexes by nanomechanical mapping of the film during curing. It is shown that, although acrylic domains aid oxygen diffusion and facilitate curing, the rate of curing was substantially lower in the interior. Nevertheless, homogeneous curing was achieved at long times. The role of primary and secondary catalysts in the process is also explored, finding that the variation of the rate of curing of the alkyd plays an influential role in the development of film structure due to phase migration of the two polymers as curing progresses. It is hoped this work goes some way to unraveling the mystery behind the curing process in acrylic/alkyd hybrid latex films.

KeyWords AITranslate

hybrid latex film structure curing nanomechanical mapping
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00507

Chinese Library Classification Number:

Citation Information:

Acrylic/alkyd hybrid latexes offer the potential to obtain hard films from waterborne polymer dispersions without using coalescing agents. However, despite being widely used commercially, the curing process of the alkyd resin used in such formulations, and its influence on the final film morphology, remain poorly understood. In this work, we explore the curing process and its influence on film morphology in alkyd/acrylic hybrid latexes by nanomechanical mapping of the film during curing. It is shown that, although acrylic domains aid oxygen diffusion and facilitate curing, the rate of curing was substantially lower in the interior. Nevertheless, homogeneous curing was achieved at long times. The role of primary and secondary catalysts in the process is also explored, finding that the variation of the rate of curing of the alkyd plays an influential role in the development of film structure due to phase migration of the two polymers as curing progresses. It is hoped this work goes some way to unraveling the mystery behind the curing process in acrylic/alkyd hybrid latex films.

quote

GB/T 7714-2015 [1] Elodie Limousin, Daniel E. MartinezTong, Nicholas Ballard, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00507.
MLA [1] Elodie Limousin, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00507.
APA [1] Elodie Limousin, Daniel E. MartinezTong, Nicholas Ballard, & José M. Asua. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00507
IEEE [1] Elodie Limousin, Daniel E. MartinezTong, Nicholas Ballard, and José M. Asua, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00507. keywords: {hybrid latex;film structure;curing;nanomechanical mapping}