Thermally Activated Delayed Fluorescence Polymer Emitters with Tunable Emission from Yellow to Warm White Regulated by Triphenylamine Derivatives AITranslate

Beijing University of Chemical Technology; Wuhan University; Beijing University of Chemical Technology; Qingdao University of Science & Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

By virtue of electron-rich structure, relatively low electronic band gap, and strong blue fluorescence emission, triphenylamine derivatives (TPAs) can serve as effective host units for the π-conjugated thermally activated delayed fluorescence (TADF) polymer. In this work, we designed and synthesized two kinds of dual-emission TADF polymers, PTDP-5 and PTDP-10, in which the TPAs act as the host unit and blue light emitter simultaneously, and the alkylated TADF small molecule, 2-(10H-phenothiazin-10-yl) dibenzothiophene-S,S-dioxide, serves as an orange-yellow light emitter. It is proved that the TADF characteristics can be inherited by polymers effectively from TADF small molecules. By regulation of the content of TPA moieties, the emission colors of polymers can also be conveniently tuned from yellow to warm white light. The fabricated polymer light-emitting diodes (PLEDs) show an EQEmax of 7.1% with Commission Internationale de l’Eclairage(CIE) coordinates of (0.42, 0.33) for PTDP-5 and an EQEmax of 4.8% with CIE coordinates of (0.46, 0.41) for PTDP-10.

KeyWords AITranslate

TADF solutionprocessed fabrication dual emission conjugated TADF polymer warm white emission
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00461

Chinese Library Classification Number:

Citation Information:

By virtue of electron-rich structure, relatively low electronic band gap, and strong blue fluorescence emission, triphenylamine derivatives (TPAs) can serve as effective host units for the π-conjugated thermally activated delayed fluorescence (TADF) polymer. In this work, we designed and synthesized two kinds of dual-emission TADF polymers, PTDP-5 and PTDP-10, in which the TPAs act as the host unit and blue light emitter simultaneously, and the alkylated TADF small molecule, 2-(10H-phenothiazin-10-yl) dibenzothiophene-S,S-dioxide, serves as an orange-yellow light emitter. It is proved that the TADF characteristics can be inherited by polymers effectively from TADF small molecules. By regulation of the content of TPA moieties, the emission colors of polymers can also be conveniently tuned from yellow to warm white light. The fabricated polymer light-emitting diodes (PLEDs) show an EQEmax of 7.1% with Commission Internationale de l’Eclairage(CIE) coordinates of (0.42, 0.33) for PTDP-5 and an EQEmax of 4.8% with CIE coordinates of (0.46, 0.41) for PTDP-10.

quote

GB/T 7714-2015 [1] Yuchao Liu, Guohua Xie, Zhongjie Ren, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00461.
MLA [1] Yuchao Liu, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00461.
APA [1] Yuchao Liu, Guohua Xie, Zhongjie Ren, & Shouke Yan. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00461
IEEE [1] Yuchao Liu, Guohua Xie, Zhongjie Ren, and Shouke Yan, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00461. keywords: {TADF;solutionprocessed fabrication;dual emission;conjugated TADF polymer;warm white emission}