daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Monte Carlo study of the spin transport in magnetic materials AITranslate

Université de Cergy-Pontoise; Okayama University; Université de Cergy-Pontoise; Okayama University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The resistivity in magnetic materials has been theoretically shown to depend on the spin–spin correlation function which in turn depends on the magnetic field, the density of conduction electron, the magnetic ordering stability, etc. However, these theories involved a lot of approximations, so their validity remained to be confirmed. The purpose of this work is to show by newly improved extensive Monte Carlo (MC) simulation the resistivity of the spin resistivity from low-T ordered phase to high-T paramagnetic phase in ferromagnetic and antiferromagnetic films. We take into account the interaction between the itinerant spins and the localized lattice spins as well as the interaction between itinerant spins themselves. We show that in ferromagnets the resistivity shows a sharp peak at the magnetic phase transition in agreement with previous theories in spite of their numerous approximations. Resistivity in antiferromagnets on the other hand shows no peak for the SC, BCC and diamond lattices. Discussion on the origin of these resistivity behaviors is given.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.02.011

Chinese Library Classification Number:

Citation Information:

The resistivity in magnetic materials has been theoretically shown to depend on the spin–spin correlation function which in turn depends on the magnetic field, the density of conduction electron, the magnetic ordering stability, etc. However, these theories involved a lot of approximations, so their validity remained to be confirmed. The purpose of this work is to show by newly improved extensive Monte Carlo (MC) simulation the resistivity of the spin resistivity from low-T ordered phase to high-T paramagnetic phase in ferromagnetic and antiferromagnetic films. We take into account the interaction between the itinerant spins and the localized lattice spins as well as the interaction between itinerant spins themselves. We show that in ferromagnets the resistivity shows a sharp peak at the magnetic phase transition in agreement with previous theories in spite of their numerous approximations. Resistivity in antiferromagnets on the other hand shows no peak for the SC, BCC and diamond lattices. Discussion on the origin of these resistivity behaviors is given.

quote

GB/T 7714-2015 [1] Y. Magnin, K. Akabli, H.T. Diep, et al. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.02.011.
MLA [1] Y. Magnin, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.02.011.
APA [1] Y. Magnin, K. Akabli, H.T. Diep, & I. Harada. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.02.011
IEEE [1] Y. Magnin, K. Akabli, H.T. Diep, and I. Harada, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.02.011.