daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Discussion of the Relationship between Temperature/Pressure Gradients and Sm Recovery in the Course of La Thermal Reduction of Sm_2O_3 AITranslate

School of Civil Engineering, Hunan University of Science and Technology;School of Mechanical and Electrical Engineering, Hunan University of Science and Technology;Baotou Iron and Steel Group Corporation Ironmaking Plant
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Chemical analysis and thermogravimetric analysis is made of La slag from La thermal reduction of Sm2O3 to obtain Sm recovery from the materials in the different parts of the pot. The relationship between temperature/pressure gradients and Sm recovery is discussed based on the test results.

KeyWords AITranslate

La thermal reduction Sm2O3 temperature gradient pressure gradient Sm recovery

1郝占忠,姜银举,秦凤启,蔡安洪.用富镧合金做还原剂制取金属钐[J].稀土,1992,13(1):47-49. 被引量:11

2吕恩保,刘兴山.镧热和铈热还原法制取金属钐影响因素的研究[J].江西有色金属,1990,4(4):9-13. 被引量:11

3杨惠,康金华,黄文莉.金属钐真空还原蒸馏试验[J].赣南师范学院学报,2001,22(6):56-57. 被引量:6

4姜银举,储爱民.镧热还原氧化钐过程冶金动力学分析[J].稀土,2006,27(2):49-52. 被引量:9

5储爱民,姜银举,赵玉萍.镧热还原氧化钐过程动力学控速环节的探索[J].江西有色金属,2005,19(2):26-27. 被引量:4

6姜银举,储爱民.镧热还原氧化钐烧结堆料对金属钐收率的影响研究[J].稀有金属与硬质合金,2005,33(4):19-22. 被引量:4

1郝占忠,许林成.钐钆富集物直接还原蒸馏制备金属钐[J].有色金属:冶炼部分,2018(3):69-73.

2张先恒,赵二雄,苗旭晨,董岳阳.镧热还原法制备金属钐的研究[J].金属功能材料,2022,29(3):85-89.

1储爱民,姜银举,赵玉萍.镧热还原氧化钐过程动力学控速环节的探索[J].江西有色金属,2005,19(2):26-27. 被引量:4

2姜银举,储爱民.镧热还原氧化钐烧结堆料对金属钐收率的影响研究[J].稀有金属与硬质合金,2005,33(4):19-22. 被引量:4

3储爱民,姜银举.镧热还原氧化钐过程镧的表面富集现象探索[J].湖南有色金属,2005,21(5):22-23.

4储爱民,高春贵,蒋学智.镧热还原氧化钐过程镧的非平衡扩散的研究[J].有色金属:冶炼部分,2008(5):32-34. 被引量:2

5吕恩保,刘兴山.镧热和铈热还原法制取金属钐影响因素的研究[J].江西有色金属,1990,4(4):9-13. 被引量:11

6姜银举,储爱民.镧热还原氧化钐过程冶金动力学分析[J].稀土,2006,27(2):49-52. 被引量:9

7储爱民,姜银举.镧热还原氧化钐过程镧在镧渣表面的富集研究[J].稀有金属快报,2005,24(8):22-24. 被引量:2

8吴炳乾,张耀文.镧热还原铥镜镥富集物时杂质行为的讨论[J].江西有色金属,1997,11(2):34-37. 被引量:1

9黄美松,成维,杨露辉,贾帅广.高纯金属镱的制备工艺研究[J].矿冶工程,2013,33(6):94-96. 被引量:7

10张宝业.氧化铝超浓相输送系统供料状态不稳定原因分析及对策[J].甘肃冶金,2005,27(2):38-39.

Basic Information:

DOI:

Chinese Library Classification Number:TF845.6[冶金工程—有色金属冶金]

Citation Information:

Chemical analysis and thermogravimetric analysis is made of La slag from La thermal reduction of Sm2O3 to obtain Sm recovery from the materials in the different parts of the pot. The relationship between temperature/pressure gradients and Sm recovery is discussed based on the test results.

quote

GB/T 7714-2015 [1] ZHAO Yu-ping, CHU Ai-min, GAO Chun-gui. Discussion of the Relationship between Temperature/Pressure Gradients and Sm Recovery in the Course of La Thermal Reduction of Sm_2O_3[J]. Rare Metals and Cemented Carbides, 2008(2): 19-22.
MLA [1] ZHAO Yu-ping, et al., "Discussion of the Relationship between Temperature/Pressure Gradients and Sm Recovery in the Course of La Thermal Reduction of Sm_2O_3." Rare Metals and Cemented Carbides, no. 2, 2008, pp. 19-22.
APA [1] ZHAO Yu-ping, CHU Ai-min, & GAO Chun-gui. (2008). Discussion of the Relationship between Temperature/Pressure Gradients and Sm Recovery in the Course of La Thermal Reduction of Sm_2O_3. Rare Metals and Cemented Carbides(2), 19-22.
IEEE [1] ZHAO Yu-ping, CHU Ai-min, and GAO Chun-gui, "Discussion of the Relationship between Temperature/Pressure Gradients and Sm Recovery in the Course of La Thermal Reduction of Sm_2O_3," Rare Metals and Cemented Carbides, no. 2, pp. 19-22, 2008. keywords: {La thermal reduction;Sm2O3;temperature gradient;pressure gradient;Sm recovery}