Study of Synthesis and Photocatalytic Property of Nano-Titania Powder by H_2/Air Flame Diffusion Combustion AITranslate

School of Chemistry and Chemical, Suzhou University;State Key Laboratory of Multiphase Reactions, Institute of Process Engineering, Chinese Academy of Sciences
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using titanium tetrachloride (TiCl4) as a precursor, titania nanoparticles were synthesized in the diffusion flame of air and hydrogen. TEM, XRD,DSC-TGA was used to characterize the properties of the synthesized particles. The photocatalytic property of titania nanoparticles was also studied in this paper. The experimental results indicated that the mean particle size of titania at optimal experimental conditions were about 10-20 nm,and were dispersed uniformly and were not aggregated. And results show that the synthesized titania nano-particles have good photocatalytic activities.

KeyWords AITranslate

gas-phase combustion gas-phase synthesis TiO2 nano-particle photocatalysis

1高敬.世界TiO_2市场动态[J].稀有金属与硬质合金,2001,29(4):53-56. 被引量:1

2洪若瑜,丁剑敏,李洪钟.纳米钛白合成过程的分析——从钛矿到纳米钛白(英文)[J].计算机与应用化学,2005,22(6):421-430. 被引量:2

3Lee C H,Choi H S,Lee C H,et al. Photocatalytic properties of nano-structured TiO2 plasma sprayed coating [J]. Surface & Coatings Technol, 2003,173 (2-3) : 192-200.

4邱电云,马荣骏.钛白粉工业的概况及其发展方向[J].稀有金属与硬质合金,1994,22(2):50-54. 被引量:2

5杨向萍,段学臣,周建.纳米TiO_2的制备方法及其进展[J].稀有金属与硬质合金,2001,29(1):33-35. 被引量:13

6赵小远.纳米TiO_2的制备及其应用[J].稀有金属与硬质合金,2003,31(1):25-27. 被引量:12

7Saini K K, Sharma S D, Kar M, et al. Structural and optical properties of TiO2 thin films derived by sol-gel dip coating process[J]. J Non-Crystalline Solids, 2007,353:2469-2473.

8段学臣,高桂兰,吴湘伟,杨向萍.纳米二氧化钛粉末的研制[J].稀有金属与硬质合金,2002,30(4):17-30. 被引量:26

9张敬畅,曹维良,于定新,石锦华,窦正仓.超临界流体干燥法制备纳米级TiO_2的研究[J].无机材料学报,1999,14(1):29-35. 被引量:108

10刘秀红,赵尹,姜海波,干路平,李春忠.扩散火焰法控制TiO_2纳米晶粒径和晶型的研究[J].非金属矿,2006,29(4):19-21. 被引量:7

1洪若瑜,任志强,李洪钟.扩散火焰燃烧法合成纳米二氧化钛[J].过程工程学报,2004(z1):502-508. 被引量:2

2周雄.气相燃烧合成纳米二氧化硅中试研究[J].上海氯碱化工,2004(2):6-10. 被引量:1

3方世杰,徐明霞,黄卫友,张玉珍.纳米TiO_2光催化降解甲基橙[J].硅酸盐学报,2001,29(5):439-442. 被引量:90

4吴祖燊,李齐春,戴品中.异丙醇铝气相燃烧法制备纳米氧化铝的实验研究[J].精细与专用化学品,2011,19(8):26-29. 被引量:4

5庄清平.电场控制气相燃烧法制备纳米无机氧化物的研究进展[J].无机盐技术,2005(3):27-31.

6严安,刘泽华,苗冉冉.不同粒径的二氧化钛对甲基红的光催化降解[J].杭州化工,2009,39(4):16-19. 被引量:4

7刘朝晖,杨怀霞,沈新元,董会超,温丽.纳米TiO_2的制备研究进展[J].河南化工,2002,21(8):3-5. 被引量:9

8庄清平.外加电场气相法制备纳米无机氧化物[J].中国工程科学,2007,9(2):74-78. 被引量:1

9镁合金表面直接纳米二氧化钛化学复合镀的方法[J].电镀与精饰,2009,31(4):16-16.

10张俊卿,冯德荣.溶胶-凝胶法制备纳米二氧化钛及其对苯酚的光催化性能研究[J].内蒙古石油化工,2006,32(7):1-3. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TQ038.7[化学工程]

Citation Information:

Using titanium tetrachloride (TiCl4) as a precursor, titania nanoparticles were synthesized in the diffusion flame of air and hydrogen. TEM, XRD,DSC-TGA was used to characterize the properties of the synthesized particles. The photocatalytic property of titania nanoparticles was also studied in this paper. The experimental results indicated that the mean particle size of titania at optimal experimental conditions were about 10-20 nm,and were dispersed uniformly and were not aggregated. And results show that the synthesized titania nano-particles have good photocatalytic activities.

quote

GB/T 7714-2015 [1] REN Zhi-qiang, HONG Ruo-yu. Study of Synthesis and Photocatalytic Property of Nano-Titania Powder by H_2/Air Flame Diffusion Combustion[J]. Rare Metals and Cemented Carbides, 2008(2): 23-28.
MLA [1] REN Zhi-qiang, and HONG Ruo-yu. "Study of Synthesis and Photocatalytic Property of Nano-Titania Powder by H_2/Air Flame Diffusion Combustion." Rare Metals and Cemented Carbides, no. 2, 2008, pp. 23-28.
APA [1] REN Zhi-qiang, & HONG Ruo-yu. (2008). Study of Synthesis and Photocatalytic Property of Nano-Titania Powder by H_2/Air Flame Diffusion Combustion. Rare Metals and Cemented Carbides(2), 23-28.
IEEE [1] REN Zhi-qiang and HONG Ruo-yu, "Study of Synthesis and Photocatalytic Property of Nano-Titania Powder by H_2/Air Flame Diffusion Combustion," Rare Metals and Cemented Carbides, no. 2, pp. 23-28, 2008. keywords: {gas-phase combustion;gas-phase synthesis;TiO2;nano-particle;photocatalysis}