Thermodynamic Behavior of Materials during Crushing and their Influence on Oxygen Content of the Na-reduced Ta Powder AITranslate
Abstract AITranslate
As a matter of record, using the thermodynamic theory ofmaterial crushing, the process of crushing of Ta lump is analysed. Itshoals the etistenc3 a-catty tiings of lit3tantaneous high temperature i'crushing process in open--type e4uipment, which resu its in format ionof Ta oxide and oxynitride .Oxygen enrichment of Ta powder from thisoperation is estimated and discussed. The conclusion is that crushingprocess of the Na--reduced Ta lump is a oxygen enriched one. so w.must give the matter thought.
KeyWords AITranslate
1李运姣,李洪桂,刘茂盛,孙培梅.浅谈机械活化在湿法冶金中的应用[J].稀有金属与硬质合金,1993,21(3):38-42. 被引量:18
1胡小锋,许茜,吴艳.钽粉制备工艺研究进展[J].材料导报,2005,19(10):97-99. 被引量:11
2杨国启,何季麟,郑爱国,罗文,周小军,李军义.电容器级高比容钽粉制备工艺研究进展[J].湖南有色金属,2014,30(1):48-52. 被引量:17
1蒋柏泉,黄庆荣,郑典模,全水清,曾庆芳.溶剂浸取法制备低氟高纯氧化钽研究[J].南昌大学学报:工科版,2008,30(2):120-122. 被引量:1
2梁栋,侯击波,殷涛,尚福军,史洪刚,黄伟,史文璐.感应等离子工艺参数对制备电容器级钽粉性能的影响[J].兵器材料科学与工程,2010,33(3):46-50. 被引量:5
3王东新,李军义,孙本双,任晓,何季麟.钽粉制备新工艺研究进展[J].湖南有色金属,2011,27(3):34-37. 被引量:19
4王东新,李军义,孙本双,任晓,何季麟.还原氧化钽制备钽粉工艺研究进展[J].中国材料进展,2011,30(10):54-58. 被引量:1
5杨国启,何季麟,郑爱国,罗文,周小军,李军义.电容器级高比容钽粉制备工艺研究进展[J].湖南有色金属,2014,30(1):48-52. 被引量:17
6李仲香,杨国启,程越伟,陈学清,李霞.表面活性剂在钽粉球磨工艺中的应用研究[J].湖南有色金属,2016,32(6):40-43. 被引量:1
7李慧,雒国清,程越伟,马跃忠,杨国启,柏林,马海燕.高比容钽粉的微观结构及电性能特性的研究[J].湖南有色金属,2017,33(1):48-52. 被引量:4
8杨国启,孙宇,李仲香,陈学清,林辅坤,程越伟,雒国清.高压高比容钽粉的制备及性能表征[J].湖南有色金属,2017,33(2):43-47. 被引量:3
9雒国清,李慧,赵春霞,马海燕.不同粒度高比容钽粉性能分析[J].湖南有色金属,2017,33(5):45-48. 被引量:2
10李丽君,杨国启,梁宏源,马应会.KCl/NaCl中pH的测定[J].湖南有色金属,2017,33(5):71-73.
1李晶,傅杰,王平,李铮,黄成钢,易继松.轴承钢生产过程中的增氧[J].特殊钢,1998,19(4):39-40. 被引量:8
2张旭辉,刘伟,刘小胡,时凯华,闵召宇.可还原氧含量对WC-0.5%TaC-10.5%Co性能及微观组织影响[J].四川冶金,2015,37(4):27-31.
3仉勇.钢包顶渣向钢液增氧解析[J].鞍钢技术,2013(4):18-23.
4李德刚,万雪峰,廖相巍,曹东,贾吉祥,赵刚.大罐顶渣向钢液增氧因素分析[J].钢铁,2009,44(3):28-31. 被引量:6
5张浩泽,刘晓红,代将,张启龙.高碳铁粉二次还原方法的研究[J].昆钢科技,2016,0(1):12-14.
6王务臣.TC-136氮氧仪脉冲炉故障分析及排除[J].宽厚板,2000,6(2):42-43.
7尚德礼,李德刚,吕春风,康磊.3次钛脱氧钢中非金属夹杂物及组织研究[J].炼钢,2014,30(1):13-16.
8竺维春,王冬青,秦岳义.焦化灰用于首钢京唐公司大型高炉喷吹的初步研究[J].首钢科技,2014(1):46-50.
9李会利,李楠,魏耀武.耐火材料对IF钢总氧含量及夹杂的影响[J].耐火材料,2003,37(1):22-24. 被引量:5
10赵海东,陈列,严清忠,李世健,杨亮,成国光.电渣重熔对GCr15轴承钢化学成分和夹杂物特性的影响[J].特殊钢,2016,37(4):44-48. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:TF123.24[冶金工程—粉末冶金]
Citation Information:
As a matter of record, using the thermodynamic theory ofmaterial crushing, the process of crushing of Ta lump is analysed. Itshoals the etistenc3 a-catty tiings of lit3tantaneous high temperature i'crushing process in open--type e4uipment, which resu its in format ionof Ta oxide and oxynitride .Oxygen enrichment of Ta powder from thisoperation is estimated and discussed. The conclusion is that crushingprocess of the Na--reduced Ta lump is a oxygen enriched one. so w.must give the matter thought.
quote
| GB/T 7714-2015 | [1] OU Yang-nan. Thermodynamic Behavior of Materials during Crushing and their Influence on Oxygen Content of the Na-reduced Ta Powder[J]. Rare Metals and Cemented Carbides, 1996(4): 1-6. |
| MLA | [1] OU Yang-nan. "Thermodynamic Behavior of Materials during Crushing and their Influence on Oxygen Content of the Na-reduced Ta Powder." Rare Metals and Cemented Carbides, no. 4, 1996, pp. 1-6. |
| APA | [1] OU Yang-nan. (1996). Thermodynamic Behavior of Materials during Crushing and their Influence on Oxygen Content of the Na-reduced Ta Powder. Rare Metals and Cemented Carbides(4), 1-6. |
| IEEE | [1] OU Yang-nan, "Thermodynamic Behavior of Materials during Crushing and their Influence on Oxygen Content of the Na-reduced Ta Powder," Rare Metals and Cemented Carbides, no. 4, pp. 1-6, 1996. keywords: {crushing of Ta lump;thermodynamics of crushiag process;oxygen enrichment} |