Carbon Removal during Production of K_2 TaF_7from Ti-Sn Slag AITranslate
Abstract AITranslate
The carbon content in K2TaF7 produced from Ti--Sn slagal ways too high. Study was made on filtration of the Ta filtrate priorto cryst allization in a new material--made filter for carbon removal,and satisfaction result was obtained.The carbon content in filtered Taliquid can meet the requirements
KeyWords AITranslate
1李济华.氟钽酸钾中控制碳量原因及剔除方法[J].稀有金属与硬质合金,1995,23(1):40-41. 被引量:4
1林翠华,姜恒,宫红,苏婷婷.热分解法低温合成氟钽酸钾粉体[J].稀有金属,2011,35(6):934-938.
2邱衍嵩.氟钽酸钾结晶工艺研究[J].广东化工,2014,41(13):76-77. 被引量:1
1洪根德.树脂除油法在制取低碳氟钽酸钾中的实验研究[J].中国金属通报,2020(12):183-184.
1周丽.提高氟钽酸钾产品直收率的研究[J].稀有金属与硬质合金,2006,34(1):49-51. 被引量:3
2韩建设,赵明智,周勇.氟钽酸钾生产工艺及装备的进展[J].稀有金属与硬质合金,2004,32(3):44-48. 被引量:10
3黎俊宏.利用硅锰渣和锡渣烧制硅酸盐水泥熟料[J].水泥,2000(9):15-16. 被引量:6
4张荣良,丘克强.从含锡渣中提取锡制取锡酸钠的研究[J].矿冶,2008,17(1):34-37. 被引量:15
5过滤槽[J].酿酒,2003,30(1):89-89.
6陈世民,林兴铭.锡渣直接生产锡酸钠的试验研究[J].有色冶炼,2000,29(4):34-36. 被引量:9
7宋允嘉.离子交换分离—DSPCF吸光光度法测定氟钽酸钾中痕量铌[J].有色金属分析通讯,1994(2):27-28.
8分离锡渣的方法[J].无机盐工业,2011,43(7):28-28.
9王应民,李丰,曹华兴.氟钽酸钾中微量碳的测定[J].理化检验:化学分册,1999,35(3):108-110. 被引量:5
10苏延任.用铜锌尾矿和锡渣配料生产525R普通硅酸盐水泥[J].水泥,1998(10):1-3. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TQ131.13[化学工程—无机化工]
Citation Information:
The carbon content in K2TaF7 produced from Ti--Sn slagal ways too high. Study was made on filtration of the Ta filtrate priorto cryst allization in a new material--made filter for carbon removal,and satisfaction result was obtained.The carbon content in filtered Taliquid can meet the requirements
quote
| GB/T 7714-2015 | [1] LI Ji-hua. Carbon Removal during Production of K_2 TaF_7from Ti-Sn Slag[J]. Rare Metals and Cemented Carbides, 1996(4): 6-8. |
| MLA | [1] LI Ji-hua. "Carbon Removal during Production of K_2 TaF_7from Ti-Sn Slag." Rare Metals and Cemented Carbides, no. 4, 1996, pp. 6-8. |
| APA | [1] LI Ji-hua. (1996). Carbon Removal during Production of K_2 TaF_7from Ti-Sn Slag. Rare Metals and Cemented Carbides(4), 6-8. |
| IEEE | [1] LI Ji-hua, "Carbon Removal during Production of K_2 TaF_7from Ti-Sn Slag," Rare Metals and Cemented Carbides, no. 4, pp. 6-8, 1996. keywords: {Ta-Sn slag;K2TaF7;carbon removal} |