Coprecipitation Preparation and Characterization of Mixed Rare Earth Oxide Fine Powders AITranslate
Abstract AITranslate
Using rare earth oxide(RE 95%)as raw material. mixed rareearth oxide fine powders were prepared by coprecipitation method inwhich urea--aqua ammonia adhere tised to adjtlst the system PH in heatedsolution. The in f luences of preparation condition for products werediscussed init laily. The f me poal-ders were character lied by thermogravimetric, differential thermal analysis, sweep electron microscope,infrared spectrum. The result sho-tvs that mixed rare earth oxide finepowders can be obtained. and under the selected conditions its gra in sizeis about 1  ̄1. 5μm.
KeyWords AITranslate
1洪广言,李红云.热分解法制备希土氧化物超微粉末[J].无机化学学报,1991,7(2):241-243. 被引量:20
2景晓燕,洪广言,李有谟.醇盐法制备稀土化合物超微粉末[J].应用化学,1990,7(2):92-94. 被引量:32
1孙健哲,陆晖.电解锰生产过程中调氨的作用[J].中国锰业,1991,9(6):33-36. 被引量:6
2杨幼平,黄可龙.混合稀土氧化物微粉的制备与表征[J].稀土,1996,17(4):20-23. 被引量:4
3彭及,彭兵.高镍粗铜火法精炼过程中“调铜保镍”的技术措施[J].有色金属:冶炼部分,1998(4):7-8.
4朱瑞.钼酸铵动态焙解还原过程中有关影响因素的探讨[J].钨钼材料,1994(2):20-24. 被引量:1
5陆德君.转炉除尘系统中调径文氏管的液压电液伺服控制系统[J].上海冶金设计,1993,7(3):27-29.
6林锋,段学臣,任先京.Preparation and characterization of conductive antimony-doped tin oxide (ATO) nanoparticles[J].广东有色金属学报,2005,15(2):258-261.
7李晓波.精炼镁渣制光卤石和硫酸镁工艺研究[J].世界有色金属,2002(10):29-31. 被引量:1
8张利民,乔峥.65Mn钢控碳工艺调整[J].河北冶金,2014(10):43-44.
9何平.高温管式电阻炉在喷气冶金反应研究中的应用[J].电炉,1989(3):3-4.
10何平,张菜平,梅洪生.10吨底吹电弧炉工业实验研究[J].钢铁,1994,29(3):35-39. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF123.25[冶金工程—粉末冶金]
Citation Information:
Using rare earth oxide(RE 95%)as raw material. mixed rareearth oxide fine powders were prepared by coprecipitation method inwhich urea--aqua ammonia adhere tised to adjtlst the system PH in heatedsolution. The in f luences of preparation condition for products werediscussed init laily. The f me poal-ders were character lied by thermogravimetric, differential thermal analysis, sweep electron microscope,infrared spectrum. The result sho-tvs that mixed rare earth oxide finepowders can be obtained. and under the selected conditions its gra in sizeis about 1  ̄1. 5μm.
quote
| GB/T 7714-2015 | [1] YANG You-ping, HUANG Ke-long, LIU Zhi-guo. Coprecipitation Preparation and Characterization of Mixed Rare Earth Oxide Fine Powders[J]. Rare Metals and Cemented Carbides, 1996(4): 8-12. |
| MLA | [1] YANG You-ping, et al., "Coprecipitation Preparation and Characterization of Mixed Rare Earth Oxide Fine Powders." Rare Metals and Cemented Carbides, no. 4, 1996, pp. 8-12. |
| APA | [1] YANG You-ping, HUANG Ke-long, & LIU Zhi-guo. (1996). Coprecipitation Preparation and Characterization of Mixed Rare Earth Oxide Fine Powders. Rare Metals and Cemented Carbides(4), 8-12. |
| IEEE | [1] YANG You-ping, HUANG Ke-long, and LIU Zhi-guo, "Coprecipitation Preparation and Characterization of Mixed Rare Earth Oxide Fine Powders," Rare Metals and Cemented Carbides, no. 4, pp. 8-12, 1996. keywords: {mixed rare earth oxide;fine powder;coprecipitation method} |