Mixed Ionic-Electronic Transport for PEDOT:PSS-Based Zero-Gated Organic Electrochemical Transistors Using Impedance Spectroscopy and Micro-Raman Imaging AITranslate
Abstract AITranslate
Recent studies are being focused on establishing a link between structural and mixed ionic-electronic transport properties based on the characterization of organic mixed ionic-electronic conductors (OMIECs) under operation conditions in organic electrochemical transistor (OECT) devices. Here, we report the simultaneous access to microstructural, chemical, and physical information using impedance spectroscopy and micro-Raman imaging techniques to address the mixed ionic-electronic transport mechanisms in PEDOT:PSS-based OMIECs working as OECT channel materials. We focused on the out-of-plane and in-plane mixed ionic-electronic transport mechanisms and complement our experimental studies with computational simulations using molecular dynamics (MD) and density functional theory (DFT) methodologies. Our studies revealed that the out-of-plane transport is based on ionic injection and diffusion mainly associated with the formation of nanopore channels in PEDOT:PSS exhibiting sulfonic groups toward the aqueous media. Thus, we also evidenced that the dedoping is not only due to the direct interaction of positive ions with PEDOT:PSS bulk region but also indirectly by the rearrangements of sulfonic groups from PSS toward the aqueous media. The in-plane transport in the OECT channel was properly described as a mixed ionic-electronic transport, with not only ionic transport of sodium (Na+) but also hydronium (H3O+) species mainly through nanopores and PEDOT:PSS bulk regions and with electronic transport mainly through the PEDOT:PSS bulk region. Although it is shown that the electronic transport monotonically declines with increasing ionic concentration, the Na+ diluted regime (1 mM) exhibits weak selectivity compared to H3O+ species, and the Na+ concentrated regime (100 mM) induces extreme porosity in PEDOT:PSS yielding to the destruction of the device. These results introduce some particular features for PEDOT:PSS-based OECT channel materials that need to be considered not only for ionic concentration and selectivity but also other related stability issues.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00655
Chinese Library Classification Number:
Citation Information:
Recent studies are being focused on establishing a link between structural and mixed ionic-electronic transport properties based on the characterization of organic mixed ionic-electronic conductors (OMIECs) under operation conditions in organic electrochemical transistor (OECT) devices. Here, we report the simultaneous access to microstructural, chemical, and physical information using impedance spectroscopy and micro-Raman imaging techniques to address the mixed ionic-electronic transport mechanisms in PEDOT:PSS-based OMIECs working as OECT channel materials. We focused on the out-of-plane and in-plane mixed ionic-electronic transport mechanisms and complement our experimental studies with computational simulations using molecular dynamics (MD) and density functional theory (DFT) methodologies. Our studies revealed that the out-of-plane transport is based on ionic injection and diffusion mainly associated with the formation of nanopore channels in PEDOT:PSS exhibiting sulfonic groups toward the aqueous media. Thus, we also evidenced that the dedoping is not only due to the direct interaction of positive ions with PEDOT:PSS bulk region but also indirectly by the rearrangements of sulfonic groups from PSS toward the aqueous media. The in-plane transport in the OECT channel was properly described as a mixed ionic-electronic transport, with not only ionic transport of sodium (Na+) but also hydronium (H3O+) species mainly through nanopores and PEDOT:PSS bulk regions and with electronic transport mainly through the PEDOT:PSS bulk region. Although it is shown that the electronic transport monotonically declines with increasing ionic concentration, the Na+ diluted regime (1 mM) exhibits weak selectivity compared to H3O+ species, and the Na+ concentrated regime (100 mM) induces extreme porosity in PEDOT:PSS yielding to the destruction of the device. These results introduce some particular features for PEDOT:PSS-based OECT channel materials that need to be considered not only for ionic concentration and selectivity but also other related stability issues.
quote
| GB/T 7714-2015 | [1] Mariano Romero, Dominique Mombrú, Fernando Pignanelli, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00655. |
| MLA | [1] Mariano Romero, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00655. |
| APA | [1] Mariano Romero, Dominique Mombrú, Fernando Pignanelli, Ricardo Faccio, & Álvaro W. Mombrú. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00655 |
| IEEE | [1] Mariano Romero, Dominique Mombrú, Fernando Pignanelli, Ricardo Faccio, and Álvaro W. Mombrú, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00655. keywords: {mixed ionicelectronic organic electrochemical transistors impedance spectroscopy microRaman imaging modeling} |