The Hump Phenomenon and Instability of Oxide TFT Were Eliminated by Interfacial Passivation and UV + Thermal Annealing Treatment AITranslate

South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this work, we propose a simple and efficient interfacial modification method for thin-film transistor (TFT)-1 with poor stability under bias stress. For conventional top-contact TFT-2, the sputtering passivation layer will cause the device to be in a short-circuit condition. We used inverted coplanar-structured TFT-3 to separate the high conductivity layer from the S/D electrodes to avoid the short-circuit failure of the device, but this will cause a hump effect. Ultraviolet treatment and air annealing were performed on TFT-3 simultaneously to obtain TFT-4 with high mobility (μsat = 45.5 cm2 V–1 s–1), steep subthreshold swing (SS = 86 mV/dec), and good bias stability (±20 V, 3600 s, NBS: −0.1 V, PBS: +0.9 V, PGDBS: +0.5 V). The forward and reverse tests of TFT-1 and TFT-4 after the PGDBS test show that TFT-4 has a good stability of the asymmetric electrical bias. Finally, XRR, XPS, AFM, and contact angle were tested to further investigate the material mechanisms. In this paper, we show that the interfacial passivation of TFT can effectively isolate the invasion of external water/oxygen and compensate for interfacial defects and dangling bonds. The decomposition and rearrangement of the oxide are induced by UV + thermal annealing, which optimizes the stacking pattern of the cells, effectively reducing the defect states and eliminating parasitic channels and the hump phenomenon. Finally, an amorphous oxide semiconductor (AOS)-TFT instrument with high mobility and good stability is prepared. The method in this paper addresses the problem that the passivation layer cannot be prepared by sputtering, which is a cost-effective process.

KeyWords AITranslate

thinfilm transistor hump phenomenon instability interfacial passivation coplanar
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00649

Chinese Library Classification Number:

Citation Information:

In this work, we propose a simple and efficient interfacial modification method for thin-film transistor (TFT)-1 with poor stability under bias stress. For conventional top-contact TFT-2, the sputtering passivation layer will cause the device to be in a short-circuit condition. We used inverted coplanar-structured TFT-3 to separate the high conductivity layer from the S/D electrodes to avoid the short-circuit failure of the device, but this will cause a hump effect. Ultraviolet treatment and air annealing were performed on TFT-3 simultaneously to obtain TFT-4 with high mobility (μsat = 45.5 cm2 V–1 s–1), steep subthreshold swing (SS = 86 mV/dec), and good bias stability (±20 V, 3600 s, NBS: −0.1 V, PBS: +0.9 V, PGDBS: +0.5 V). The forward and reverse tests of TFT-1 and TFT-4 after the PGDBS test show that TFT-4 has a good stability of the asymmetric electrical bias. Finally, XRR, XPS, AFM, and contact angle were tested to further investigate the material mechanisms. In this paper, we show that the interfacial passivation of TFT can effectively isolate the invasion of external water/oxygen and compensate for interfacial defects and dangling bonds. The decomposition and rearrangement of the oxide are induced by UV + thermal annealing, which optimizes the stacking pattern of the cells, effectively reducing the defect states and eliminating parasitic channels and the hump phenomenon. Finally, an amorphous oxide semiconductor (AOS)-TFT instrument with high mobility and good stability is prepared. The method in this paper addresses the problem that the passivation layer cannot be prepared by sputtering, which is a cost-effective process.

quote

GB/T 7714-2015 [1] Yilin Li, Rihui Yao, Jinyao Zhong, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00649.
MLA [1] Yilin Li, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00649.
APA [1] Yilin Li, Rihui Yao, Jinyao Zhong, Yuexin Yang, Zhihao Liang, Yubin Fu, Xuan Zeng, Guoping Su, Honglong Ning, & Junbiao Peng. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00649
IEEE [1] Yilin Li, Rihui Yao, Jinyao Zhong, Yuexin Yang, Zhihao Liang, Yubin Fu, Xuan Zeng, Guoping Su, Honglong Ning, and Junbiao Peng, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00649. keywords: {thinfilm transistor hump phenomenon instability interfacial passivation coplanar}