Experimental Study on Rhenium Extraction from Waste Superalloy AITranslate
Abstract AITranslate
According to the characteristics of high density and insolubility of superalloy,fine particles with high activity were prepared from waste superalloy by vacuum atomization.Rhenium in waste superalloy powder was dissolved into solution in the form of ReO4^- after oxidation acid leaching.And Re leaching rate reaches 99.02%.Subsequently,the pH value of the acid leaching solution was adjusted to 1.5with saturated NaOH solution,and then rhenium was adsorbed onto D296 anion exchange resin.And Re adsorption rate reaches 98.76%.During the process of desorption,Mo loaded in the D296 resin was preferentially desorbed with the mixed solution of ammonia and ammonium chloride,with Re loss rate of 4.97%.Rheniumwas desorbed with ammonium thiocyanate solution,with Re desorption rate of 94.98%.The Re-containing products were prepared from the desorbed solution containing rhenium by adding KCl or NH4Cl and evaporation cooling crystallization.Re crystallization rate is higher than 90% by controlling the rhenium concentration over 22.38g/L in concentrated solution.The results of X-ray fluorescence analysis show that the purity of potassium rhenate and ammonium rhenate reaches 99.21% and 99.58%,respectively.
KeyWords AITranslate
1彭真,罗明标,花榕,廖桢葳.从矿石中回收铼的研究进展[J].湿法冶金,2012,31(2):76-80. 被引量:25
2孟晗琪,吴贤,陈昆昆,王靖坤.碱融—水浸法从高温合金废料中回收铼[J].有色金属工程,2014,4(4):44-46. 被引量:15
3杨志平,李庸华,唐宝彬.从废催化剂中回收铂铼的工艺研究[J].湿法冶金,1999,18(2):9-13. 被引量:16
4祁栋,王毅.钼精矿浸出液中铼与钼的分离试验研究[J].稀有金属与硬质合金,2013,41(1):20-23. 被引量:3
5陈德林,安悦,唱鹤鸣,徐慧.活性炭吸附铼性质的研究[J].中国有色金属学报,1994,4(2):41-44. 被引量:3
6胡家璜,关邑.膜法在提取铼工艺中的应用[J].中国钼业,1993(3):34-36. 被引量:2
7陈昆昆,马光,孟晗琪,王治钧,王靖坤,吴永谦.D296树脂从含钼酸性溶液中吸附钼的试验研究[J].中国钼业,2014,38(2):47-50. 被引量:8
8陈昆昆,吴贤,王治钧.D296树脂从含铼酸性溶液中吸附铼的研究[J].有色金属:冶炼部分,2015(7):43-46. 被引量:20
1陈昆昆,许万祥,郭瑞,操齐高.从高温合金电溶液中回收铼酸铵的工业试验[J].有色金属:冶炼部分,2018(7):31-34. 被引量:4
2陈昆昆,操齐高,张卜升,孟晗琪,赵盘巢.高温合金酸浸液回收高纯铼酸铵试验研究[J].有色金属:冶炼部分,2019,0(9):45-48. 被引量:6
3郭瑞,许万祥,王靖坤,李波,李进,周严.含钌含铼高温合金电化学溶解工艺研究[J].有色金属:冶炼部分,2019,0(8):57-60. 被引量:2
4郭瑞,许万祥,王靖坤,周严,李进.含钌含铼阳极泥处理工艺研究[J].有色金属:冶炼部分,2019,0(10):55-57. 被引量:1
5鲁兴武,李守荣,张恩玉,程亮,李俞良,牛永胜.铜冶炼污酸中铼富集工艺技术研究[J].有色金属:冶炼部分,2020,0(4):47-50. 被引量:9
6张春伟,孙元,唐俊杰,房大维.工业废料中铼元素的回收与再利用研究进展[J].材料导报,2020,34(15):15145-15152. 被引量:2
7卢晓锋,朱纪念,卢苏君,李亦婧,赵淑琴,郭勇.高温合金中铼金属回收制备高纯铼酸铵研究[J].稀有金属,2021,45(8):972-979. 被引量:3
8陈昆昆,李林波,操齐高,孟晗琪.从沉钨钼后液中制备高纯铼酸铵[J].稀有金属材料与工程,2022,51(8):3049-3056.
1陈昆昆,操齐高,张卜升,孟晗琪,赵盘巢.高温合金酸浸液回收高纯铼酸铵试验研究[J].有色金属:冶炼部分,2019,0(9):45-48. 被引量:6
2郭瑞,许万祥,王靖坤,周严,李进.含钌含铼阳极泥处理工艺研究[J].有色金属:冶炼部分,2019,0(10):55-57. 被引量:1
3李文静,黄龙,唐和清,董学林,吕基平,朱丽华.铼元素分离富集研究进展[J].中国有色金属学报,2020,30(1):214-226. 被引量:9
4鲁兴武,李守荣,张恩玉,程亮,李俞良,牛永胜.铜冶炼污酸中铼富集工艺技术研究[J].有色金属:冶炼部分,2020,0(4):47-50. 被引量:9
5李来平,刘燕,曹亮,蒋丽娟,李延超.铼技术研究进展[J].中国钼业,2020,44(4):1-6. 被引量:3
6陈昆昆,操齐高,张卜升,孟晗琪,戎万,赵盘巢.钨铼合金废料电化学溶解研究[J].有色金属:冶炼部分,2020(9):54-58. 被引量:1
7张家润,刘智勇,刘志宏,李启厚.高纯铼及其化合物的制备与应用研究进展[J].粉末冶金材料科学与工程,2020,25(4):273-279. 被引量:6
8方健,吴丹丹,文书明,张松,林启镪.稀散金属铼资源综合回收利用研究进展[J].矿产保护与利用,2020,40(5):62-69. 被引量:3
9郑朝振,林江顺,王海北,秦树辰,吴涛,张登凯,冯爱玲.铅锌冶炼污酸处理及汞的脱除技术研究[J].中国资源综合利用,2021,39(6):1-5. 被引量:1
10刘碧媛.赤泥-石灰土路基材料制备与性能研究[J].城市道桥与防洪,2021(7):246-248. 被引量:1
1秦玉楠.提取钼酸铵和铼酸铵的新工艺[J].企业技术开发,1991(12):12-16.
2钱勇.溶剂萃取法制取铼酸铵[J].铜业工程,2004(3):26-28. 被引量:13
3陈昆昆,吴贤,王治钧.D296树脂从含铼酸性溶液中吸附铼的研究[J].有色金属:冶炼部分,2015(7):43-46. 被引量:20
4“铜冶炼还原终液中回收铼酸铵研究”通过鉴定[J].有色设备,2004(4):12-12.
5陈昆昆,马光,孟晗琪,王治钧,王靖坤,吴永谦.D296树脂从含钼酸性溶液中吸附钼的试验研究[J].中国钼业,2014,38(2):47-50. 被引量:8
6常云龙,刘洋,邓丽,宋增意,刘丹.NH_4SCN解吸剂对负载Re的D296树脂的解吸影响[J].沈阳工业大学学报,2016,38(3):263-267. 被引量:1
7刘小龙,任萌,李佳,黎志万,刘锦洪.D296树脂吸附分离锆铪试验研究[J].湿法冶金,2015,34(6):474-477. 被引量:2
8刘沙.粉末冶金法制取低铼钼合金的研究[J].稀有金属与硬质合金,1997,25(4):26-29.
9孙世杰.低成本生产钛粉及钛粉末冶金制品途径的探索[J].粉末冶金工业,2005,15(4):28-28. 被引量:2
10秦玉楠.离子交换法提取铼酸铵新工艺[J].中国钼业,1998,22(5):39-41. 被引量:10
Basic Information:
DOI:
Chinese Library Classification Number:TF841.8[冶金工程—有色金属冶金]
Citation Information:
According to the characteristics of high density and insolubility of superalloy,fine particles with high activity were prepared from waste superalloy by vacuum atomization.Rhenium in waste superalloy powder was dissolved into solution in the form of ReO4^- after oxidation acid leaching.And Re leaching rate reaches 99.02%.Subsequently,the pH value of the acid leaching solution was adjusted to 1.5with saturated NaOH solution,and then rhenium was adsorbed onto D296 anion exchange resin.And Re adsorption rate reaches 98.76%.During the process of desorption,Mo loaded in the D296 resin was preferentially desorbed with the mixed solution of ammonia and ammonium chloride,with Re loss rate of 4.97%.Rheniumwas desorbed with ammonium thiocyanate solution,with Re desorption rate of 94.98%.The Re-containing products were prepared from the desorbed solution containing rhenium by adding KCl or NH4Cl and evaporation cooling crystallization.Re crystallization rate is higher than 90% by controlling the rhenium concentration over 22.38g/L in concentrated solution.The results of X-ray fluorescence analysis show that the purity of potassium rhenate and ammonium rhenate reaches 99.21% and 99.58%,respectively.
quote
| GB/T 7714-2015 | [1] CHEN Kun-kun, MENG Han-qi, WU Yong-qian, et al. Experimental Study on Rhenium Extraction from Waste Superalloy[J]. Rare Metals and Cemented Carbides, 2016(6): 26-30. |
| MLA | [1] CHEN Kun-kun, et al., "Experimental Study on Rhenium Extraction from Waste Superalloy." Rare Metals and Cemented Carbides, no. 6, 2016, pp. 26-30. |
| APA | [1] CHEN Kun-kun, MENG Han-qi, WU Yong-qian, & WU Xian. (2016). Experimental Study on Rhenium Extraction from Waste Superalloy. Rare Metals and Cemented Carbides(6), 26-30. |
| IEEE | [1] CHEN Kun-kun, MENG Han-qi, WU Yong-qian, and WU Xian, "Experimental Study on Rhenium Extraction from Waste Superalloy," Rare Metals and Cemented Carbides, no. 6, pp. 26-30, 2016. keywords: {rhenium;superalloy;vacuum atomization;oxidation acid leaching;D296 resin;ammonium rhenate;potassium rhenate} |