Research Progress on Impurity Behavior and Purification Technology of Waste Liquid during Silver Electrolyzation AITranslate
Abstract AITranslate
The behavior of various impurities in silver electrolyzation process is analyzed,purification methods of silver electrolytic waste liquid at present are introduced,and the advantages and disadvantages of these methods are compared.The development direction of comprehensive recovery and treatment technology of silver electrolytic waste liquid is pointed out.
KeyWords AITranslate
1王光忠,刘超,陈海军.银电解液净化系统的安全改造[J].湖南有色金属,2010,26(6):47-51. 被引量:4
2容智梅.银电解过程中杂质的行为及其控制[J].湖南有色金属,2003,19(3):16-18. 被引量:12
3黄绍勇.银电解液中杂质的行为及净化方法[J].湿法冶金,2004,23(1):53-56. 被引量:26
4王青,蒲保春,魏东.银电解精炼中铋的行为分析[J].黄金,2002,23(11):35-38. 被引量:9
5王少龙,丁旭,余秋雁.银电解废液综合回收利用新工艺[J].世界有色金属,2013(11):34-35. 被引量:5
6徐淳,资云从.硫酸净化电解液中杂质铅的工艺实验[J].化学工程与装备,2009(6):47-48. 被引量:5
7刘庆杰,胡世勋,赵国成.银电解废液净化方法浅析[J].中国有色冶金,2011,40(1):22-26. 被引量:17
1于凯,艾峥嵘,宁志强,胡伟,谢宏伟.离子交换法净化硝酸银溶液吸附过程研究[J].稀有金属,2021,45(11):1352-1358. 被引量:3
2张济祥,冯俊花,朱勇,阳岸恒,邓志明,吴庆伟.半导体行业镀膜用高纯银的制备方法及展望[J].云南冶金,2018,47(5):55-58. 被引量:6
3孔德颂,王鹏程,叶钟林,段建锋.银电解液中钯的定向分离试验研究[J].矿冶工程,2019,39(2):85-88. 被引量:4
4周方,钟茂礼,吴卫煌.高纯银工业制备[J].黄金,2020,41(6):4-6.
5郑学军,王涵睿,史智锋,董蔚,孟志军,贺慧,蔡兴顺.利用铜片置换法回收含银废液中银的工艺实践[J].中国材料进展,2020,39(10):787-789. 被引量:1
6谭代娣,罗正波,张剑锋,张圣南,李家元.从银电解废液中回收银试验研究[J].湿法冶金,2022,41(2):113-116.
7张腾,张善辉,赵祝鹏,孙尚,吴昌南.用二乙酰二肟从银电解液中选择性沉淀钯试验研究[J].湿法冶金,2022,41(4):308-311. 被引量:1
1于凯,艾峥嵘,宁志强,胡伟,谢宏伟.离子交换法净化硝酸银溶液吸附过程研究[J].稀有金属,2021,45(11):1352-1358. 被引量:3
2陈永红,苏广东,洪博,孟宪伟,芦新根.2017—2018年中国银分析测定的进展[J].黄金,2020,41(2):81-86. 被引量:2
3周方,钟茂礼,吴卫煌.高纯银工业制备[J].黄金,2020,41(6):4-6.
4郝海英,张巧霞,熊晓东,罗俊锋,付丰年,于文军,户赫龙,董亭义.新型贵金属材料在5G时代的研究现状及应用展望[J].贵金属,2020,41(S01):68-72. 被引量:4
5肖忠良,曾超,刘佩,吴道新,宋刘斌,曹忠.稀有金属材料钯湿法回收的研究进展[J].功能材料,2020,51(11):11008-11016.
6李伟,杨晓艳,张亚东,柴明强,艾琳,黎楷.高纯蒸镀材料的发展及现状[J].中国金属通报,2021(4):5-6.
7赵梅莉,刘明,马一丹,李江祺,严继康,冷崇燕.Mn^(2+)作为控制剂对银纳米线的合成的影响[J].云南冶金,2021,50(5):70-73.
8王宇,林霄,黄培颖,陈晓,陈日耀,刘键熙.硫脲-壳聚糖(TU-CS)选择性吸附膜的制备及其对废水中Ag^(+)的吸附[J].福建师范大学学报:自然科学版,2022,38(2):42-49.
9张建文,王海东,梁汉,张胜广,刘浪,马崇振.退役晶硅光伏组件回收技术研究进展[J].矿冶工程,2022,42(3):147-152. 被引量:2
10张腾,张善辉,赵祝鹏,孙尚,吴昌南.用二乙酰二肟从银电解液中选择性沉淀钯试验研究[J].湿法冶金,2022,41(4):308-311. 被引量:1
1黄善富.浅析砷锑在铜电解过程中的行为[J].有色冶炼,2002,31(3):20-23. 被引量:14
2孟庆应,常国威,王建中,毛彩珠.紫杂铜中杂质行为的研究[J].辽宁工学院学报,1998,18(1):59-61. 被引量:5
3C.A.Pickles,阎惠君.高碳铬铁生产过程中杂质行为的研究[J].铁合金,1990(3):45-55.
4王建英,周银东.从金电解废液中提取铂钯[J].江苏冶金,1999,27(4):11-12.
5容智梅.从金银冶炼系统中回收铂、钯[J].有色冶炼,2003,32(6):27-29. 被引量:10
6袁明亮,梅贤功,庄剑鸣,陈荩,蒋汉瀛.菱锰矿酸浸过程杂质行为[J].中南工业大学学报,1996,27(1):40-43. 被引量:3
7隋智通,卢琛.纯钒熔盐电解精炼过程研究[J].钒钛,1991(1):4-9.
8魏昶,何蔼平,任国民.锌电积过程中杂质行为及其相互反应[J].昆明理工大学学报:理工版,1996,21(6):71-74. 被引量:7
9肖方春,杨惠.金属镝冶炼过程中杂质行为及其控制方法[J].有色金属,2002,54(4):56-58. 被引量:2
10赵海涛.碲电解废液中锡的分离[J].铜业工程,2013(5):22-24.
Basic Information:
DOI:
Chinese Library Classification Number:TF832[冶金工程—有色金属冶金]
Citation Information:
The behavior of various impurities in silver electrolyzation process is analyzed,purification methods of silver electrolytic waste liquid at present are introduced,and the advantages and disadvantages of these methods are compared.The development direction of comprehensive recovery and treatment technology of silver electrolytic waste liquid is pointed out.
quote
| GB/T 7714-2015 | [1] ZHANG Ji-xiang, YANG An-heng, ZHU Yong, et al. Research Progress on Impurity Behavior and Purification Technology of Waste Liquid during Silver Electrolyzation[J]. Rare Metals and Cemented Carbides, 2016(6): 31-34. |
| MLA | [1] ZHANG Ji-xiang, et al., "Research Progress on Impurity Behavior and Purification Technology of Waste Liquid during Silver Electrolyzation." Rare Metals and Cemented Carbides, no. 6, 2016, pp. 31-34. |
| APA | [1] ZHANG Ji-xiang, YANG An-heng, ZHU Yong, DENG Zhi-ming, KONG Jian-wen, & XIE Hong-chao. (2016). Research Progress on Impurity Behavior and Purification Technology of Waste Liquid during Silver Electrolyzation. Rare Metals and Cemented Carbides(6), 31-34. |
| IEEE | [1] ZHANG Ji-xiang, YANG An-heng, ZHU Yong, DENG Zhi-ming, KONG Jian-wen, and XIE Hong-chao, "Research Progress on Impurity Behavior and Purification Technology of Waste Liquid during Silver Electrolyzation," Rare Metals and Cemented Carbides, no. 6, pp. 31-34, 2016. keywords: {silver;electrolytic waste liquid;impurity behavior;purification technology;research progress;development direction} |