The Study on Fluorine Residue of Zr-4 Alloy Pipe after Pickling Based on Finite Element Method(FEM) AITranslate
Abstract AITranslate
With conventional pickling process parameters of zirconium alloy pipe,study was made on the law of influence of inner diameter,sampling location,water temperature and flaw depth of the alloy pipe during pickling on its fluorine residue.And the experimental results were analyzed in theory by using finite element method(FEM).The results show that with the increase of Zr-4alloy pipe inner diameter,fluorine residue on pipe inner surface gradually increases.Fluorine residues in the head,middle and tail of Zr-4alloy pipe are nearly identical.With the increase of water temperature,fluorine residue on Zr-4alloy pipe inner surface is reduced.Fluorine residue has no obvious corresponding relation with flaw depth of Zr-4alloy pipe.
KeyWords AITranslate
1于军辉,吕亮亮,张谭,王晨阳.酸洗工艺对Zr-4合金管材氟残留影响[J].金属世界,2018(6):46-49. 被引量:3
2张伟,王旭峰,杨锋,张海芹,雷江,王盈辉.内喷砂工艺对Zr-4合金管材表面质量及尺寸的影响[J].金属功能材料,2021,28(4):85-90. 被引量:1
1张永刚,杨晓康,乔军伟,王海.含铌锆合金酸洗研究[J].中国金属通报,2021(1):120-121.
2刘邯涛,杨鹏,吕江,武晓斌,孔立群.一种新型酸洗装置的智能化设计及应用[J].机械研究与应用,2023,36(1):78-81.
3王云普,袁小虎,李定骏,唐春梅,袁卫锋,赖建平,余家欣.喷砂工艺对CB2铁素体耐热钢表面粗糙度和夹砂率的影响[J].热喷涂技术,2022,14(4):35-41.
4王燕.核级锆材质量控制——基于故障树法的Zr-4棒材氢元素检测超标原因排查分析[J].金属世界,2023(4):49-51.
1高世奇,李小宁,薛艳丽,王鑫佳.加工工艺对锆合金微观结构及力学性能的影响[J].热加工工艺,2013,42(16):64-66. 被引量:4
2孙阳平,许妍,冯辉,薛艳丽.锆管缺陷的无损检测及处置措施[J].无损检测,2014,36(11):54-58. 被引量:1
3王洪波,程健伟,李金梁.锆合金管材高精度矫直机的研究[J].科技经济导刊,2015(18):95-96.
4曾庆芦,叶力平,李铂涛,刘昊,帅美荣.钢-铜包覆管连续减径轧制变形过程研究[J].热加工工艺,2016,45(3):171-174.
5王德华,袁改焕,李恒羽.核用锆合金管材爆破试验工艺的改进[J].稀有金属快报,2006,25(10):36-38. 被引量:4
6孙阳平,王高飞,张广辉.退火方式对锆合金管材性能的影响[J].热加工工艺,2015,44(4):211-212.
7李少华,杨世杰.稀有金属管材内表面流动酸洗设备的研制[J].稀有金属快报,2005,24(3):35-37.
8夏坚平,于润康,李增儒.高精度管材内表面处理设备的研制[J].稀有金属材料与工程,1991,20(5):72-75. 被引量:1
9支颖,刘相华,喻海良,于明,杨贵敏.板带钢加速冷却过程中下冲水的流动特性[J].钢铁研究学报,2009,21(2):13-17.
10孙旭东,郝勇,刘燕德.表面增强拉曼光谱法检测农药残留的研究进展[J].食品安全质量检测学报,2012,3(5):421-426. 被引量:15
Basic Information:
DOI:
Chinese Library Classification Number:TG146.414[金属学及工艺—金属材料]
Citation Information:
With conventional pickling process parameters of zirconium alloy pipe,study was made on the law of influence of inner diameter,sampling location,water temperature and flaw depth of the alloy pipe during pickling on its fluorine residue.And the experimental results were analyzed in theory by using finite element method(FEM).The results show that with the increase of Zr-4alloy pipe inner diameter,fluorine residue on pipe inner surface gradually increases.Fluorine residues in the head,middle and tail of Zr-4alloy pipe are nearly identical.With the increase of water temperature,fluorine residue on Zr-4alloy pipe inner surface is reduced.Fluorine residue has no obvious corresponding relation with flaw depth of Zr-4alloy pipe.
quote
| GB/T 7714-2015 | [1] YU Jun-hui, YUAN Gai-huan, WANG Zeng-min, et al. The Study on Fluorine Residue of Zr-4 Alloy Pipe after Pickling Based on Finite Element Method(FEM)[J]. Rare Metals and Cemented Carbides, 2015(2): 64-68. |
| MLA | [1] YU Jun-hui, et al., "The Study on Fluorine Residue of Zr-4 Alloy Pipe after Pickling Based on Finite Element Method(FEM)." Rare Metals and Cemented Carbides, no. 2, 2015, pp. 64-68. |
| APA | [1] YU Jun-hui, YUAN Gai-huan, WANG Zeng-min, LI Xiao-ning, LIU Lei, YU Hai-ping, & LI Qi-ming. (2015). The Study on Fluorine Residue of Zr-4 Alloy Pipe after Pickling Based on Finite Element Method(FEM). Rare Metals and Cemented Carbides(2), 64-68. |
| IEEE | [1] YU Jun-hui, YUAN Gai-huan, WANG Zeng-min, LI Xiao-ning, LIU Lei, YU Hai-ping, and LI Qi-ming, "The Study on Fluorine Residue of Zr-4 Alloy Pipe after Pickling Based on Finite Element Method(FEM)," Rare Metals and Cemented Carbides, no. 2, pp. 64-68, 2015. keywords: {Zr-4alloy pipe;pickling;fluorine residue;finite element method(FEM)} |