Research on Deternination of Boron in LaB_6 by Acid-Base Titration AITranslate

Hunan Rare Earth Metal Material Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The LaB6 sample was dissolved with dilute nitric acid,and then its boron content was determined by acid-base titration with EDTA as the masking agent and mannitol as the complexing agent of boronic acid.Sample dissolution methods,reagent dosage,judgment methods of titration end-point,interfering elements,recovery ratio and precision were investigated.Operation with the method is simple and fast,and the method has good accuracy and precision with boron recovery of 99.45% ~100.48% and RSD less than0.50%。

KeyWords AITranslate

LaB6 B determination acid-base titration

1谭朝晖,郑灵芝.二硼化钛粉末总硼量测定方法修订实验研究[J].有色冶金设计与研究,2020,41(5):16-18.

1澳大利亚发明阻挡热量的玻璃[J].中国建筑金属结构,2003(8):43-43.

2澳大利亚科学家发明新型玻璃[J].新材料产业,2003(7):42-43.

3澳大利亚科学家发明新型玻璃称透明度极高[J].科技成果纵横,2003(4):37-37.

4郭海军,刘荣丽.等离子发射光谱法测定六硼化镧中铁、钙、镁、铬、锰、铜[J].湖南有色金属,2009,25(4):56-59.

5张学钢,许涛.高频红外吸收法测定六硼化镧中碳含量[J].稀土,2003,24(6):86-87. 被引量:2

6申泮文,龚毅生,周永洽,林东风.熔盐电解合成希土六硼化物的研究——REBO_3、LiBO_2和LiF体系熔盐电解合成RER_6[J].无机化学学报,1991,7(3):306-310. 被引量:7

7姜岩,王颖.硼热还原法制备六硼化镧粉末[J].辽宁化工,2010,39(9):904-905. 被引量:1

8石志霞,余章龙,孙静,彭程,段华英,张碧田,王星明,储茂友.两段焙烧法制备六硼化镧工艺研究[J].材料导报,2015,29(6):88-92. 被引量:1

9吴冬梅.ICP-AES法同时测定石油焦中的铁、硅、钛[J].现代科学仪器,2002,19(5):56-57. 被引量:7

10李友君.分析化学实验中测Bi^(3+)、Pb^(2+)废液的回收与再生[J].化学世界,1997,38(1):49-51. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:O655.22[理学—分析化学];TQ133.3[化学工程—无机化工]

Citation Information:

The LaB6 sample was dissolved with dilute nitric acid,and then its boron content was determined by acid-base titration with EDTA as the masking agent and mannitol as the complexing agent of boronic acid.Sample dissolution methods,reagent dosage,judgment methods of titration end-point,interfering elements,recovery ratio and precision were investigated.Operation with the method is simple and fast,and the method has good accuracy and precision with boron recovery of 99.45% ~100.48% and RSD less than0.50%。

quote

GB/T 7714-2015 [1] LIU Rong-li. Research on Deternination of Boron in LaB_6 by Acid-Base Titration[J]. Rare Metals and Cemented Carbides, 2015(2): 59-63.
MLA [1] LIU Rong-li. "Research on Deternination of Boron in LaB_6 by Acid-Base Titration." Rare Metals and Cemented Carbides, no. 2, 2015, pp. 59-63.
APA [1] LIU Rong-li. (2015). Research on Deternination of Boron in LaB_6 by Acid-Base Titration. Rare Metals and Cemented Carbides(2), 59-63.
IEEE [1] LIU Rong-li, "Research on Deternination of Boron in LaB_6 by Acid-Base Titration," Rare Metals and Cemented Carbides, no. 2, pp. 59-63, 2015. keywords: {LaB6;B determination;acid-base titration}