Effects of Sintering Pressure on Microstructure and Properties of WC-12%Co Coarse Grained Cemented Carbide AITranslate
Abstract AITranslate
Study was made on the effects of different sintering pressure on metallographic microstructure and physical and mechanical properties of WC-12%Co coarse grained cemented carbide.The results show that the cemented carbide can be highly densified at relatively low sintering pressure.With the increase of sintering pressure,three properties of the cemented carbide have no obvious change.When sintering pressure is about 2 MPa,both flexural strength and impact toughness of the cemented carbide are highest with good comprehensive performance.
KeyWords AITranslate
1罗桂甫,吴建国.粗晶硬质合金的研究进展[J].硬质合金,2013,30(1):46-52. 被引量:13
2郭圣达,羊建高,黄海平,许方,胡咏梅,郑彪华.粗晶硬质合金硬度和强度影响因素的分析研究[J].稀有金属与硬质合金,2012,40(4):56-58. 被引量:10
3张正富,黄莉玲,彭金辉,谭竹峰,袁明健,张华明,李芳.WC-Co硬质合金硬度和冲击韧度影响因素的变量搜索试验[J].金属热处理,2011,36(5):83-89. 被引量:8
4湘子.硬质合金晶粒度分级标准[J].硬质合金,2006,23(2):68-68. 被引量:18
5易勇,熊继,李懿,沈保罗.硬质合金抗弯强度及其分散性的研究[J].工具技术,2002,36(10):16-19. 被引量:32
6莫盛秋,程继贵,王华林.真空烧结低钴粗晶硬质合金及其性能的研究[J].合肥工业大学学报:自然科学版,2000,23(2):294-297. 被引量:7
7莫盛秋.低钴粗晶Wc—Co合金的烧结[J].常州工业技术学院学报,1998,11(4):40-46. 被引量:2
8Sandvik Hard Materials.Understanding cemented carbide. . 2004
1陈洪霞,薛林,顾金宝,杨胜,袁明健.烧结工艺对粗晶硬质合金微观组织及性能的影响[J].稀有金属与硬质合金,2015,43(5):64-67 71. 被引量:2
2吴迪,熊志翔,白英龙,果世驹,杨霞,徐红霞.铸造碳化钨反应烧结制备粗晶硬质合金[J].粉末冶金材料科学与工程,2011,16(4):471-477. 被引量:3
3聂洪波.超粗晶WC-Co硬质合金的制备方法与机理及性能研究[J].中国钨业,2016,31(4):51-57. 被引量:10
4郭圣达,羊建高,黄海平,许方,胡咏梅,郑彪华.粗晶硬质合金硬度和强度影响因素的分析研究[J].稀有金属与硬质合金,2012,40(4):56-58. 被引量:10
5李勇,谢淑华.WC粗晶硬质合金的研究进展[J].材料研究与应用,2009,3(2):77-80. 被引量:12
6程鑫,张立.热处理对粗晶WC-Co硬质合金力学性能的影响[J].稀有金属与硬质合金,2012,40(2):45-47. 被引量:8
7陈芃,李海坤.硬质合金高温处理回收工艺研究[J].硬质合金,2001,18(4):201-203. 被引量:13
8马鋆,张立,南晴,解明伟,冯于平,雷霆.Cr、V、Ta添加剂对超粗晶和特粗晶硬质合金电化学腐蚀行为的影响[J].粉末冶金材料科学与工程,2012,17(6):825-832. 被引量:16
9张立,程鑫,陈述,马鋆,吴厚平,熊湘君.Cr、V、RE添加剂对特粗晶与超粗晶硬质合金微观组织与性能的影响[J].中国有色金属学报,2012,22(9):2620-2625. 被引量:9
10张立,王元杰,余贤旺,王振波.WC粉末粒度与形貌对硬质合金中WC晶粒度、晶粒形貌与合金性能的影响[J].中国钨业,2008,23(4):23-26. 被引量:28
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]
Citation Information:
Study was made on the effects of different sintering pressure on metallographic microstructure and physical and mechanical properties of WC-12%Co coarse grained cemented carbide.The results show that the cemented carbide can be highly densified at relatively low sintering pressure.With the increase of sintering pressure,three properties of the cemented carbide have no obvious change.When sintering pressure is about 2 MPa,both flexural strength and impact toughness of the cemented carbide are highest with good comprehensive performance.
quote
| GB/T 7714-2015 | [1] YANG Sheng, GU Jin-bao, LIAO Jun, et al. Effects of Sintering Pressure on Microstructure and Properties of WC-12%Co Coarse Grained Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2015(2): 54-58. |
| MLA | [1] YANG Sheng, et al., "Effects of Sintering Pressure on Microstructure and Properties of WC-12%Co Coarse Grained Cemented Carbide." Rare Metals and Cemented Carbides, no. 2, 2015, pp. 54-58. |
| APA | [1] YANG Sheng, GU Jin-bao, LIAO Jun, & CHEN Hong-xia. (2015). Effects of Sintering Pressure on Microstructure and Properties of WC-12%Co Coarse Grained Cemented Carbide. Rare Metals and Cemented Carbides(2), 54-58. |
| IEEE | [1] YANG Sheng, GU Jin-bao, LIAO Jun, and CHEN Hong-xia, "Effects of Sintering Pressure on Microstructure and Properties of WC-12%Co Coarse Grained Cemented Carbide," Rare Metals and Cemented Carbides, no. 2, pp. 54-58, 2015. keywords: {sintering pressure;WC-12%Co coarse grained cemented carbide;microstructure;property} |