Study on the Process and Equipment of Continuous Distillation and Concentration of High acid RE Strip Liquor AITranslate

Conghua Small Small Reining Factory;Hebi Chemical Reagent Equipment Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made on the process and equipment of continuous distillation and concentration of high acid RE strip liquor. The results show that the use of the patented porous micro circulation, double effect continuous evaporator (made of quartz and with electric tube internal heating function) allows not only for continuous distillation and concentration of RE strip liquor, but also HCl recovery. The said equipment features good technical coordination of the high acid RE strip liquor in RE grouping and separation,lower cost and higher recovery without environmental pollution.

KeyWords AITranslate

high acid RE strip liquor distillation and concentration HCl recovery porous micro circulation double effect evaporator

1化学工程手册编辑委员会.化学工程手册(第九篇蒸发与结晶)[M].北京:化学工业出版社,1985.18.

1唐建军,张伟,周康根,张启修.膜法回收稀土冶金过程中废酸的可行性研究[J].矿冶工程,2007,27(6):54-57. 被引量:3

2李小平,汪凯,张春恒,雒敏,马沁,王世民.钽及钽合金在废酸回收设备中的应用[J].材料开发与应用,2012,27(6):19-21. 被引量:5

3唐建军,周康根,赵方辉,李荣光,张启修.Hydrochloric Acid Recovery from Rare Earth Chloride Solutions by Vacuum Membrane Distillation (1) Study on the Possibility[J].稀土学报:英文版,2003,0(S1):78-82. 被引量:3

4TANG Jianjun,ZHOU Kanggen.Hydrochloric acid recovery from rare earth chloride solutions by vacuum membrane distillation[J].稀有金属:英文版,2006,25(3):287-292. 被引量:7

5韩建设,刘建华,叶祥,凌诚.南方稀土水冶含氨废水综合回收工艺探讨[J].稀土,2008,29(6):69-75. 被引量:27

6杨清宇,王琳丽,蔡锡元,韩建设.南方稀土湿法冶炼废水综合回收与治理研究(下)[J].有色冶金节能,2012,27(2):6-10. 被引量:4

7唐建军,周康根,张启修.用减压膜蒸馏法分离AlCl_3-HCl-H_2O体系中盐酸的研究[J].膜科学与技术,2002,22(3):11-14. 被引量:9

8唐建军,周康根,张启修.减压膜蒸馏从稀土氯化物溶液中回收盐酸[J].膜科学与技术,2002,22(4):38-42. 被引量:8

1徐世民,王军武,许松林.新型蒸馏技术及应用[J].化工机械,2004,31(3):183-187. 被引量:17

2范荣玉,郑细鸣.减压膜蒸馏技术及其在环保领域中的应用[J].化学工程师,2005,19(5):32-35. 被引量:4

3TANG Jianjun,ZHOU Kanggen.Hydrochloric acid recovery from rare earth chloride solutions by vacuum membrane distillation[J].稀有金属:英文版,2006,25(3):287-292. 被引量:7

4丁忠伟,李兆曼,刘丽英,杨祖荣.气扫式膜蒸馏用于脱除水中氨的分离性能[J].北京化工大学学报:自然科学版,2007,34(1):5-8. 被引量:5

5唐建军,张启修,张伟,邓爱华.减压膜蒸馏法浓缩氧化铝碳分母液的可行性[J].水处理技术,2007,33(12):23-25. 被引量:2

6曾理,高从堦.膜蒸馏在冶金工业中的应用前景[J].膜科学与技术,2008,28(6):87-92. 被引量:1

7王晓琴,马浴铭,王敏达,赵树英.膜蒸馏技术在水处理中的应用[J].工业水处理,2008,28(12):18-21. 被引量:6

8环国兰,杜启云,王薇.膜蒸馏技术研究现状[J].天津工业大学学报,2009,28(4):12-18. 被引量:33

9林振景,陈婧,郑辉,李志伟.真空膜蒸馏技术在水处理中的应用进展[J].广州化工,2011,39(4):34-35.

10刘捷,武春瑞,吕晓龙.减压膜蒸馏传热传质过程[J].化工学报,2011,62(4):908-915. 被引量:25

1黄祖诚,赵洪洋,刘祖波.“一体式”微脱碳铁水包的设计与应用[J].铁合金,2014,45(1):39-43.

2李亮,田阳,刘大春,周厚军,戴永年,杨斌.Pretreatment of lead anode slime with low silver by vacuum distillation for concentrating silver[J].中南大学学报:英文版,2013,20(3):615-621. 被引量:6

3乔素梅,葛晓陵,杨刚.湿式微轧法制备纳米片状锌粉[J].有色金属工程,2013,3(2):24-27. 被引量:4

4茅康林.海绵钛氯化过程中尾气吸收设计特点[J].有色金属设计,2014,41(1):25-27. 被引量:4

5王国荣.二期高镍锍分离生产及技术改造实践[J].金川科技,2000(2):29-31.

6周峰,戴方钦,祁霞.蓄热式卧式钢包烘烤器在韶钢的运用[J].冶金能源,2016,35(4):33-37. 被引量:4

7四川氟碳铈矿盐酸法分离生产稀土产品工艺调查分析[J].四川稀土,2007,0(3):24-27. 被引量:2

8肖永忠.某难选铁矿石煤基直接还原—磁选试验研究[J].涟钢科技与管理,2010(2):1-5.

9张丽霞.用Alamine 336,Aliquat 336,TBP和Cyanex 923分离和回收盐酸[J].湿法冶金,2006,25(4):197-197.

10陆仲权.稀土分离中萃取效率提升的工艺研究[J].有色金属文摘,2015,30(6):109-110. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF845.032[冶金工程—有色金属冶金]

Citation Information:

Study is made on the process and equipment of continuous distillation and concentration of high acid RE strip liquor. The results show that the use of the patented porous micro circulation, double effect continuous evaporator (made of quartz and with electric tube internal heating function) allows not only for continuous distillation and concentration of RE strip liquor, but also HCl recovery. The said equipment features good technical coordination of the high acid RE strip liquor in RE grouping and separation,lower cost and higher recovery without environmental pollution.

quote

GB/T 7714-2015 [1] HAN Jian-she, ZHANG Bai-hua. Study on the Process and Equipment of Continuous Distillation and Concentration of High acid RE Strip Liquor[J]. Rare Metals and Cemented Carbides, 2000(4): 1-6.
MLA [1] HAN Jian-she, and ZHANG Bai-hua. "Study on the Process and Equipment of Continuous Distillation and Concentration of High acid RE Strip Liquor." Rare Metals and Cemented Carbides, no. 4, 2000, pp. 1-6.
APA [1] HAN Jian-she, & ZHANG Bai-hua. (2000). Study on the Process and Equipment of Continuous Distillation and Concentration of High acid RE Strip Liquor. Rare Metals and Cemented Carbides(4), 1-6.
IEEE [1] HAN Jian-she and ZHANG Bai-hua, "Study on the Process and Equipment of Continuous Distillation and Concentration of High acid RE Strip Liquor," Rare Metals and Cemented Carbides, no. 4, pp. 1-6, 2000. keywords: {high acid RE strip liquor;distillation and concentration;HCl recovery;porous micro circulation double effect evaporator}