daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Analysis of Influencing Factors on Electrochemical Corrosion Behavior of Cemented Carbides AITranslate

School of Mechanical Engineering, Jincheng College, Sichuan University;School of Mechanical Engineering, Jincheng College, Sichuan University;School of Mechanical Engineering, Jincheng College, Sichuan University;School of Mechanical Engineering, Jincheng College, Sichuan University;School of Mechanical Engineering, Jincheng College, Sichuan University;School of Mechanical Engineering, Jincheng College, Sichuan University;School of Mechanical Engineering, Jincheng College, Sichuan University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Research progress is reviewed on the electrochemical corrosion behavior of cemented carbide. The effects of the internal factors are emphatically analyzed such as grain size,bonding phase composition (Ni, Co and so on),sintering process and added alloying elements (Cr,Ti,V,A1) on the electrochemical corrosion behavior of cemented carbides. The effects of the external factors are discussed such as working tem- perature, corrosive medium and surface treatment on the corrosion of cemented carbides. It is found that the effect of grain size is inconsistent in different corrosive media. The bonding phase Ni is more resistant to corrosion than Co,and reasonable sintering technology and appropriate addition of alloying elements can improve the corrosion resistance of cemented carbides. Compared with working temperature, the corrosive medium has more influence on the corrosion of cemented carbides, and different corrosive media lead to dif- ferent corrosion behavior and corrosion rate. The surface treatment of the cemented carbide can improve its corrosion resistance.

KeyWords AITranslate

cemented carbide electrochemical corrosion corrosive medium bonding phase

1马丽丽.WC-Co硬质合金在水中的腐蚀行为[J].粉末冶金材料科学与工程,2010,15(6):635-639. 被引量:9

2张好强,王莉娜,张桓,贾晓鸣.超细晶硬质合金线切割加工过程的腐蚀机理研究[J].稀有金属与硬质合金,2013,41(5):47-50. 被引量:8

3朱斌,柏振海,高阳,罗兵辉.WC粒度对WC-15Fe-5Ni硬质合金组织与性能的影响[J].中国有色金属学报,2016,26(5):1065-1074. 被引量:11

4易丹青,陈丽勇,刘会群,王斌,聂灿.硬质合金电化学腐蚀行为的研究进展[J].硬质合金,2012,29(4):238-253. 被引量:26

5林春芳,杜玉国,孙丹,陈蓓瑾,刘莹华.WC-(7-9)Ni-(1-2)Cr硬质合金耐蚀性能的研究[J].硬质合金,2010,27(4):224-229. 被引量:12

6林春芳,杜玉国,孙丹,陈蓓瑾,刘莹华.Ni、Cr对碳化钨基硬质合金耐腐蚀性能的影响[J].腐蚀与防护,2010,31(9):678-681. 被引量:11

7王兴庆,李晓东,郭海亮,何宝山.Al含量对WC-Co硬质合金耐腐蚀性能的影响[J].粉末冶金材料科学与工程,2006,11(4):219-224. 被引量:20

8佘俊杰,李昆.硬质合金刀片清洗及表面腐蚀的研究[J].硬质合金,2011,28(4):228-232. 被引量:3

9马鋆,张立,南晴,解明伟,冯于平,雷霆.Cr、V、Ta添加剂对超粗晶和特粗晶硬质合金电化学腐蚀行为的影响[J].粉末冶金材料科学与工程,2012,17(6):825-832. 被引量:16

10万庆磊,张立,王喆,徐涛,张忠健,刘向中,柯荣现.WC-Co合金在不同介质中的电化学腐蚀行为与腐蚀机理研究[J].硬质合金,2014,31(4):201-208. 被引量:6

1施远,金洙吉,姜冠楠,刘作涛,周忠正,王泽北.YG15硬质合金电化学腐蚀机理研究[J].中国腐蚀与防护学报,2019,39(3):253-259. 被引量:2

2金鹏,马赛,孟湘君,涂俊平,彭文,魏修宇,孔德方.原料总碳含量对WC-15%Co-1.1%Cr3C2硬质合金性能的影响[J].硬质合金,2020,37(4):266-272. 被引量:5

3杜伟,刘宾,刘勋,刘诗彪.硬质合金机械加工常见缺陷与工艺优化[J].硬质合金,2021,38(2):123-132. 被引量:6

4蔡浩钦,邓汝荣.一种硬质合金铝型材挤压模[J].铝加工,2021(5):55-58. 被引量:1

5韩彬,董威威,骆祎岚,朱世根.金属元素对WC-Al_(2)O_(3)复合材料在NaCl溶液中腐蚀行为的影响研究[J].稀有金属与硬质合金,2022,50(6):33-40.

6韩彬,朱世根.WC-Al_(2)O_(3)复合材料在不同浓度NaCl溶液中的腐蚀行为[J].稀有金属与硬质合金,2023,51(2):30-38.

1朱新生.镁合金的电化学腐蚀行为与反应机理研究[J].中国金属通报,2020(12):111-112.

2冯志,程登峰,黎明华,刘娜娜,朱福明.碳化配碳量对粗颗粒WC粉末形貌及WC-8%Co合金性能的影响[J].硬质合金,2021,38(3):171-178.

3赵声志,毛善文,崔焱茗,谢浩.TiC添加对粗晶WC-10%Co硬质合金组织和性能的影响[J].硬质合金,2021,38(3):179-184. 被引量:4

4赵玉玲,张颢,邹德良,魏修宇,金鹏,崔焱茗.钴镍比对WC-14%(Co,Ni)硬质合金力学性能和在中性NaCl溶液中耐腐蚀性能的影响[J].硬质合金,2021,38(4):236-243. 被引量:2

5卢继,张勇,王晓琴,覃俊.YG8硬质合金高效精密磨削实验研究[J].现代制造技术与装备,2021,57(12):61-63.

6华涛,郭智兴,杨露,荆凯峰,鲜广.粗晶粒硬质合金材料的制备与表征[J].实验室研究与探索,2022,41(1):33-36. 被引量:1

7张彬.硬质合金烧结尾气处理方案分析[J].广州化工,2022,50(9):159-161.

8邝宏有,戴炳蔚,吴育藩.WC-11%(Ti,W)(Ta,Nb)C-11%Co合金制取过程中碳量和球磨时间的优化[J].硬质合金,2022,39(2):111-117.

9黄开靓,邓静,张鑫泉.硬质合金加工用无线超声刀柄开发[J].组合机床与自动化加工技术,2022(7):134-138.

10刘海军,伍文辉,汪巍,金鹏,孔德方,龙坚战,谭立群.不同粘结剂成分WC-30%(Co-Ni-Cr)粗晶硬质合金高温氧化行为的研究[J].硬质合金,2022,39(3):182-188. 被引量:2

1刘丹.高考英语改革对高中英语教学的反拨效应[J].英语教师,2017,17(19):99-103. 被引量:3

2周元洪.大学生就业困难的原因分析及指导对策[J].长春理工大学学报:高教版,2010(1):88-89. 被引量:9

3张礼,张保国,罗超,刘宜霖,韩丽楠,缪玉欣.紫外光照射下GaN的电化学性质及CMP应用[J].微纳电子技术,2017,54(12):858-863. 被引量:3

4孙颖.群文阅读在农村小学语文中的探究与应用[J].学周刊,2017(36):134-135. 被引量:8

5赵仲茜,王金辉.Sn含量对Mg-Sn-Al-Zn镁合金组织与性能的影响[J].热加工工艺,2017,46(21):21-24. 被引量:2

6安文强,邓鹏.轧后快冷工艺对叉车门架型钢20MnSiV组织性能的影响[J].轧钢,2017,34(4):36-38. 被引量:2

7廖帮全,徐亮,周圣丰,杨光,尚纯,雷剑波.激光熔化沉积TC4-Cu双相涂层的结构与性能[J].中国激光,2017,44(11):89-96. 被引量:1

8刘金礼.研究建筑工程质量标准化监督管理[J].建材与装饰,2017,13(46):131-132. 被引量:4

9孟维艳,赵爽,王鹤龄,蔡青,李保胜,周延民.不同钛表面形貌对人牙龈成纤维细胞附着及胶原沉积的影响[J].实用口腔医学杂志,2017,33(6):772-777. 被引量:4

10叶兵兵,李小丹.母猪产后缺乳的原因及对策[J].湖北畜牧兽医,2017,38(11):26-29.

Basic Information:

DOI:

Chinese Library Classification Number:TG172[金属学及工艺—金属表面处理]

Citation Information:

Research progress is reviewed on the electrochemical corrosion behavior of cemented carbide. The effects of the internal factors are emphatically analyzed such as grain size,bonding phase composition (Ni, Co and so on),sintering process and added alloying elements (Cr,Ti,V,A1) on the electrochemical corrosion behavior of cemented carbides. The effects of the external factors are discussed such as working tem- perature, corrosive medium and surface treatment on the corrosion of cemented carbides. It is found that the effect of grain size is inconsistent in different corrosive media. The bonding phase Ni is more resistant to corrosion than Co,and reasonable sintering technology and appropriate addition of alloying elements can improve the corrosion resistance of cemented carbides. Compared with working temperature, the corrosive medium has more influence on the corrosion of cemented carbides, and different corrosive media lead to dif- ferent corrosion behavior and corrosion rate. The surface treatment of the cemented carbide can improve its corrosion resistance.

quote

GB/T 7714-2015 [1] QIN Qin, FANG Yun-long, LI Jing-xiao, et al. Analysis of Influencing Factors on Electrochemical Corrosion Behavior of Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2017(5): 74-78.
MLA [1] QIN Qin, et al., "Analysis of Influencing Factors on Electrochemical Corrosion Behavior of Cemented Carbides." Rare Metals and Cemented Carbides, no. 5, 2017, pp. 74-78.
APA [1] QIN Qin, FANG Yun-long, LI Jing-xiao, SUN Wen-wen, BAO Shuai, LUAN Dao-cheng, & WANG Zheng-yun. (2017). Analysis of Influencing Factors on Electrochemical Corrosion Behavior of Cemented Carbides. Rare Metals and Cemented Carbides(5), 74-78.
IEEE [1] QIN Qin, FANG Yun-long, LI Jing-xiao, SUN Wen-wen, BAO Shuai, LUAN Dao-cheng, and WANG Zheng-yun, "Analysis of Influencing Factors on Electrochemical Corrosion Behavior of Cemented Carbides," Rare Metals and Cemented Carbides, no. 5, pp. 74-78, 2017. keywords: {cemented carbide;electrochemical corrosion;corrosive medium;bonding phase}