Electrospun Polyurethane/Zeolitic Imidazolate Framework Nanofibrous Membrane with Superior Stability for Filtering Performance AITranslate
Abstract AITranslate
As a metal–organic framework material, the zeolite imidazole salt framework (ZIF) has a large specific surface area and excellent chemical sites. It not only has a high PM2.5 filtration efficiency but also exhibits excellent adsorption performance toward heavy metal ions. In this study, ZIF-modified soluble polyurethane (PU) nanofibrous membranes were prepared by the electrospinning method. Experimental results show that the PU@ZIF-15 membrane has high PM2.5 filtration efficiency and excellent mechanical properties as well as low pressure drop. Moreover, the composite membrane exhibits a high level of PM2.5 filtration performance even after 5 cycles of filtration, washing, and drying. The prepared PU@ZIF-15 membrane shows excellent comprehensive performance and broad application prospects in PM2.5 filtration. In addition, it has a certain adsorption capacity toward the heavy metal chromium ion.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01005
Chinese Library Classification Number:
Citation Information:
As a metal–organic framework material, the zeolite imidazole salt framework (ZIF) has a large specific surface area and excellent chemical sites. It not only has a high PM2.5 filtration efficiency but also exhibits excellent adsorption performance toward heavy metal ions. In this study, ZIF-modified soluble polyurethane (PU) nanofibrous membranes were prepared by the electrospinning method. Experimental results show that the PU@ZIF-15 membrane has high PM2.5 filtration efficiency and excellent mechanical properties as well as low pressure drop. Moreover, the composite membrane exhibits a high level of PM2.5 filtration performance even after 5 cycles of filtration, washing, and drying. The prepared PU@ZIF-15 membrane shows excellent comprehensive performance and broad application prospects in PM2.5 filtration. In addition, it has a certain adsorption capacity toward the heavy metal chromium ion.
quote
| GB/T 7714-2015 | [1] Haitao Wang, Huan Xu, Han Li, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01005. |
| MLA | [1] Haitao Wang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01005. |
| APA | [1] Haitao Wang, Huan Xu, Han Li, Xiang Liu, Zhaoqun Du, & Weidong Yu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01005 |
| IEEE | [1] Haitao Wang, Huan Xu, Han Li, Xiang Liu, Zhaoqun Du, and Weidong Yu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01005. keywords: {polyurethane;ZIF;excellent mechanical properties;air filtration;heavy metal adsorption} |