daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Vapor Phase Infiltration Doping of the Semiconducting Polymer Poly(aniline) with TiCl4 + H2O: Mechanisms, Reaction Kinetics, and Electrical and Optical Properties AITranslate

Georgia Institute of Technology; Georgia Institute of Technology; Georgia Institute of Technology; Georgia Institute of Technology; Georgia Institute of Technology; Georgia Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This study reports on the optical and electronic properties of organic–inorganic hybrid semiconductors synthesized via vapor phase infiltration (VPI) of poly(aniline) (PAni) with TiCl4 and H2O. This process results in (1) oxidative doping of PAni with the TiCl4 precursor, (2) acid doping of PAni with the HCl byproduct to form polaronic charge carriers, and (3) infiltration and deposition of a UV absorbing material (TiOx) within the final hybrid film. The electrical conductivity initially increases with increasing TiCl4 exposure time up to 0.2 S/cm, but eventually (above ca. 400 min of TiCl4 exposure), the electrical conductivity decreases due to increased TiOx deposition. Increasing the TiCl4 exposure time also decreases visible absorption while increasing UV and IR absorptions to a saturation point. This narrow window for visible light transmission is uncommon in these materials. The changes in optical absorption as a function of precursor exposure time are also fit to a diffusion kinetics model to ascertain effective diffusion constants of ca. 1 × 10–15 cm2/s for the TiCl4 + H2O VPI process in PAni at 80 °C. In summary, this work demonstrates that VPI precursors, products, and byproducts can be used to synthesize hybrid organic–inorganic semiconductors with distinctive optical and electronic properties.

KeyWords AITranslate

vapor phase infiltration doping semiconducting polymers atomic layer deposition poly(aniline) titania TiO2
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01014

Chinese Library Classification Number:

Citation Information:

This study reports on the optical and electronic properties of organic–inorganic hybrid semiconductors synthesized via vapor phase infiltration (VPI) of poly(aniline) (PAni) with TiCl4 and H2O. This process results in (1) oxidative doping of PAni with the TiCl4 precursor, (2) acid doping of PAni with the HCl byproduct to form polaronic charge carriers, and (3) infiltration and deposition of a UV absorbing material (TiOx) within the final hybrid film. The electrical conductivity initially increases with increasing TiCl4 exposure time up to 0.2 S/cm, but eventually (above ca. 400 min of TiCl4 exposure), the electrical conductivity decreases due to increased TiOx deposition. Increasing the TiCl4 exposure time also decreases visible absorption while increasing UV and IR absorptions to a saturation point. This narrow window for visible light transmission is uncommon in these materials. The changes in optical absorption as a function of precursor exposure time are also fit to a diffusion kinetics model to ascertain effective diffusion constants of ca. 1 × 10–15 cm2/s for the TiCl4 + H2O VPI process in PAni at 80 °C. In summary, this work demonstrates that VPI precursors, products, and byproducts can be used to synthesize hybrid organic–inorganic semiconductors with distinctive optical and electronic properties.

quote

GB/T 7714-2015 [1] Shawn A. Gregory, Yi Li, Timothy D. Monroe, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01014.
MLA [1] Shawn A. Gregory, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01014.
APA [1] Shawn A. Gregory, Yi Li, Timothy D. Monroe, Junjian Li, Shannon K. Yee, & Mark D. Losego. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01014