daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

THz Generation from the Topological Nodal Line Semimetal Co2MnGa THz Generation from the Topological Nodal Line Semimetal Co2MnGa AITranslate

Sapienza University;INFN section of Rome, P.Le Aldo Moro; Sapienza University;Max Planck Institute for Chemical Physics of Solids;Max Planck Institute for Chemical Physics of Solids;Max Planck Institute for Chemical Physics of Solids; Sapienza University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nonlinear optical spectroscopy is a fundamental probe for the investigation of topological effects in quantum materials. In this paper, we report on the terahertz (THz) emission from thin films at various thicknesses of the magnetic topological nodal semimetal Co2MnGa (CMG) when excited by femtosecond optical pulses. Experimental results suggest the presence of multiple THz generation mechanisms, originating from both bulk and surface states of CMG. The former is explained in terms of a photon-drag effect as induced by radiation pressure. The latter emission mechanism instead appears to be related to the photovoltaic effect coming from the topological surface states. This interplay between generation mechanisms indicates that Co2MnGa topological nodal semimetals are a valuable platform for THz emitter devices.

KeyWords AITranslate

THz emission spectroscopy topology magnetism photogalvanic effect
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01376

Chinese Library Classification Number:

Citation Information:

Nonlinear optical spectroscopy is a fundamental probe for the investigation of topological effects in quantum materials. In this paper, we report on the terahertz (THz) emission from thin films at various thicknesses of the magnetic topological nodal semimetal Co2MnGa (CMG) when excited by femtosecond optical pulses. Experimental results suggest the presence of multiple THz generation mechanisms, originating from both bulk and surface states of CMG. The former is explained in terms of a photon-drag effect as induced by radiation pressure. The latter emission mechanism instead appears to be related to the photovoltaic effect coming from the topological surface states. This interplay between generation mechanisms indicates that Co2MnGa topological nodal semimetals are a valuable platform for THz emitter devices.

quote

GB/T 7714-2015 [1] Luca Tomarchio, Sen Mou, Lorenzo Mosesso, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01376.
MLA [1] Luca Tomarchio, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01376.
APA [1] Luca Tomarchio, Sen Mou, Lorenzo Mosesso, Anastasios Markou, Edouard Lesne, Claudia Felser, & Stefano Lupi. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01376
IEEE [1] Luca Tomarchio, Sen Mou, Lorenzo Mosesso, Anastasios Markou, Edouard Lesne, Claudia Felser, and Stefano Lupi, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01376. keywords: {THz emission spectroscopy topology magnetism photogalvanic effect}