Fabricating Flexible Strain Sensor with Direct Writing Graphene/Carbon Nanotube Aerogel Fabricating Flexible Strain Sensor with Direct Writing Graphene/Carbon Nanotube Aerogel AITranslate
Abstract AITranslate
Flexible strain sensor has wide applications in wearable devices and human–computer interaction. These sensors exhibit a flexible performance, which makes the structure of the device adapt to a wide range of application scenarios. This work proposes a low-cost and accurate direct writing method to fabricate a three-dimensional graphene/carbon nanotube strain sensor by using prepared printing ink with good dispersion, extruding ordered lamellae, and controlling porous aerogel structure. The morphology of the prepared three-dimensional porous aerogel was controlled with the ice template method. The strain sensor could be obtained by encapsulating the PDMS precursor, which shows high stretchability with a sensitivity of 18.55 at a 20% tensile strain. It offers good stability after 900 times of repeated stretching under 20% strain. This study of fabricating flexible strain sensors could provide a facile and effective way to apply intelligent packaging and wearable electronic devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01338
Chinese Library Classification Number:
Citation Information:
Flexible strain sensor has wide applications in wearable devices and human–computer interaction. These sensors exhibit a flexible performance, which makes the structure of the device adapt to a wide range of application scenarios. This work proposes a low-cost and accurate direct writing method to fabricate a three-dimensional graphene/carbon nanotube strain sensor by using prepared printing ink with good dispersion, extruding ordered lamellae, and controlling porous aerogel structure. The morphology of the prepared three-dimensional porous aerogel was controlled with the ice template method. The strain sensor could be obtained by encapsulating the PDMS precursor, which shows high stretchability with a sensitivity of 18.55 at a 20% tensile strain. It offers good stability after 900 times of repeated stretching under 20% strain. This study of fabricating flexible strain sensors could provide a facile and effective way to apply intelligent packaging and wearable electronic devices.
quote
| GB/T 7714-2015 | [1] Chen Chen, Fuqiang Chu, Yang Zhang, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01338. |
| MLA | [1] Chen Chen, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01338. |
| APA | [1] Chen Chen, Fuqiang Chu, Yang Zhang, Mengdi Ma, Rui Sun, Peng Jia, & Jiazhen Sun. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01338 |
| IEEE | [1] Chen Chen, Fuqiang Chu, Yang Zhang, Mengdi Ma, Rui Sun, Peng Jia, and Jiazhen Sun, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01338. keywords: {graphene/carbon nanotube aerogel direct printing flexible structure strain sensor} |