Recyclable and Self-Healing Natural Rubber Vitrimers from Anhydride-Epoxy Exchangeable Covalent Bonds AITranslate

University of Waterloo; McMaster University; University of Waterloo; University of Waterloo; University of Waterloo
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Dynamic covalent networks (DCNs) contain exchangeable covalent bonds that can undergo dynamic structural changes under external stimuli. Employment of DCNs in elastomers instead of static cross-links provides a pathway for designing reprocessable and recyclable rubbers. Vitrimers are examples of DCNs that utilize associative covalent bond-exchanging chemistry to keep the total number of cross-links constant, making them recyclable, reprocessable, and self-healing. This study primarily investigated the design of a natural rubber (NR) vitrimer via anhydride-epoxy dynamic cross-linking using a scalable process and benign reagents, such as maleic anhydride (MA) or bisphenol A diglycidyl ether (DGEBA), which can be reprocessed and self-heal with heat stimuli. Reactive melt mixing was employed to synthesize the vitrimers, and the reaction success was confirmed by using various chemical analysis approaches. The rubber vitrimer possesses a high activation energy (139.7 kJ/mol) and low freezing topology temperature (65 °C), demonstrating a robust exchange network. The NR vitrimers could undergo multiple rounds of reprocessing, unlike peroxide- or sulfur-cured NR, due to their robust dynamical cross-linking networks generated by the adaptable covalent bonds. Moreover, the NR vitrimers exhibited unprecedented self-healing capabilities to maintain their original mechanical characteristics. The recyclability of NR is a significant achievement in reducing post-consumer rubber waste and virgin material utilization. The self-healing functionality is also appealing in applications that require on-site assembly or repair as well as to help increase the lifespan of the elastomers.

KeyWords AITranslate

natural rubber vitrimers dynamic crosslinking rubber recyclable selfhealing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01258

Chinese Library Classification Number:

Citation Information:

Dynamic covalent networks (DCNs) contain exchangeable covalent bonds that can undergo dynamic structural changes under external stimuli. Employment of DCNs in elastomers instead of static cross-links provides a pathway for designing reprocessable and recyclable rubbers. Vitrimers are examples of DCNs that utilize associative covalent bond-exchanging chemistry to keep the total number of cross-links constant, making them recyclable, reprocessable, and self-healing. This study primarily investigated the design of a natural rubber (NR) vitrimer via anhydride-epoxy dynamic cross-linking using a scalable process and benign reagents, such as maleic anhydride (MA) or bisphenol A diglycidyl ether (DGEBA), which can be reprocessed and self-heal with heat stimuli. Reactive melt mixing was employed to synthesize the vitrimers, and the reaction success was confirmed by using various chemical analysis approaches. The rubber vitrimer possesses a high activation energy (139.7 kJ/mol) and low freezing topology temperature (65 °C), demonstrating a robust exchange network. The NR vitrimers could undergo multiple rounds of reprocessing, unlike peroxide- or sulfur-cured NR, due to their robust dynamical cross-linking networks generated by the adaptable covalent bonds. Moreover, the NR vitrimers exhibited unprecedented self-healing capabilities to maintain their original mechanical characteristics. The recyclability of NR is a significant achievement in reducing post-consumer rubber waste and virgin material utilization. The self-healing functionality is also appealing in applications that require on-site assembly or repair as well as to help increase the lifespan of the elastomers.

quote

GB/T 7714-2015 [1] Binh Trinh, Patricia Owen, Anna vanderHeide, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01258.
MLA [1] Binh Trinh, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01258.
APA [1] Binh Trinh, Patricia Owen, Anna vanderHeide, Arvind Gupta, & Tizazu H. Mekonnen. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01258