Enhanced Low Frequency Sound Absorption of Bilayer Nanocomposite Acoustic Absorber Laminated with Microperforated Nanofiber Felt AITranslate

Myongji University; Myongji University; Myongji University; Myongji University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A laminar nanocomposite sound absorber was fabricated by laminating a microperforated nanofiber felt (MPNF) on a reinforced nanofibrous cryogel. The spatial morphology of both dense and porous nanofiber layers combined with the microperforations employed on the dense layer delivered a sound absorption average (SAA) rating of 0.61. A lower frequency average sound absorption coefficient of 0.56 was achieved when a denser nanofiber felt layer with the incorporation of 1.78% microperforation rate was employed. A highly porous cryogel layer permits excellent mid- and high-frequency absorption coefficients of 0.74 and 0.51, respectively. The nanocomposite sound absorber has a remarkable areal density of 771 g m–2, making it lightweight and less bulky ideal for acoustic building material. The perforated nanofiber felt, however, has a minimal effect on the sound transmission coefficient (STC) of the nanocomposite sound absorber with an STC of 6.75 dB. By tuning the perforation diameter, perforation rate, and thickness of the nanofiber felt, the overall acoustic absorption performance of the nanocomposite sound absorber can be improved.

KeyWords AITranslate

Sound absorption Nanocomposite Microperforated Wideband Low frequency
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01249

Chinese Library Classification Number:

Citation Information:

A laminar nanocomposite sound absorber was fabricated by laminating a microperforated nanofiber felt (MPNF) on a reinforced nanofibrous cryogel. The spatial morphology of both dense and porous nanofiber layers combined with the microperforations employed on the dense layer delivered a sound absorption average (SAA) rating of 0.61. A lower frequency average sound absorption coefficient of 0.56 was achieved when a denser nanofiber felt layer with the incorporation of 1.78% microperforation rate was employed. A highly porous cryogel layer permits excellent mid- and high-frequency absorption coefficients of 0.74 and 0.51, respectively. The nanocomposite sound absorber has a remarkable areal density of 771 g m–2, making it lightweight and less bulky ideal for acoustic building material. The perforated nanofiber felt, however, has a minimal effect on the sound transmission coefficient (STC) of the nanocomposite sound absorber with an STC of 6.75 dB. By tuning the perforation diameter, perforation rate, and thickness of the nanofiber felt, the overall acoustic absorption performance of the nanocomposite sound absorber can be improved.

quote

GB/T 7714-2015 [1] John Marc C. Puguan, David Brylle A. Agbayani, Ariel Jan V. Sadural, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01249.
MLA [1] John Marc C. Puguan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01249.
APA [1] John Marc C. Puguan, David Brylle A. Agbayani, Ariel Jan V. Sadural, & Hern Kim. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01249
IEEE [1] John Marc C. Puguan, David Brylle A. Agbayani, Ariel Jan V. Sadural, and Hern Kim, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01249. keywords: {Sound absorption;Nanocomposite;Microperforated;Wideband;Low frequency}