Thermal Annealing Driven Enhancement of Perpendicular Magnetic Anisotropy and the Interfacial Dzyaloshinskii–Moriya Interaction in Ultrathin Ru/Co/W/Ru Films Thermal Annealing Driven Enhancement of Perpendicular Magnetic Anisotropy and the Interfacial Dzyaloshinskii–Moriya Interaction in Ultrathin Ru/Co/W/Ru Films AITranslate
Abstract AITranslate
Spin-related effects discovered in ultrathin magnetic films generally have an interfacial nature. The quality of interfaces between a heavy metal and a ferromagnet is the main driver of surface anisotropy, antisymmetric exchange, chiral damping, spin Hall effect, and spin–orbit torques. To understand the physics and usage of these phenomena for future atomic-scale devices, one has to study systems with disordered interfaces and search there for novel practically desirable effects, which lie beyond the atomic order and surface flatness. Here, we report the interface-related effects in Ru/Co/W/Ru ultrathin films treated by thermal annealing in vacuum. The surface roughness and degree of atomic intermixing at Ru/Co and Co/W interfaces change with increasing annealing temperature up to 240 °C, promoting an enhancement of perpendicular magnetic anisotropy and the interfacial Dzyaloshinskii–Moriya interaction (i-DMI). Further annealing at higher temperatures brings the interface deterioration and, consequently, a drastic degradation of the magnetic properties. Our first-principles calculations qualitatively support the experimental findings, providing an understanding of the i-DMI enhancement nature.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00254
Chinese Library Classification Number:
Citation Information:
Spin-related effects discovered in ultrathin magnetic films generally have an interfacial nature. The quality of interfaces between a heavy metal and a ferromagnet is the main driver of surface anisotropy, antisymmetric exchange, chiral damping, spin Hall effect, and spin–orbit torques. To understand the physics and usage of these phenomena for future atomic-scale devices, one has to study systems with disordered interfaces and search there for novel practically desirable effects, which lie beyond the atomic order and surface flatness. Here, we report the interface-related effects in Ru/Co/W/Ru ultrathin films treated by thermal annealing in vacuum. The surface roughness and degree of atomic intermixing at Ru/Co and Co/W interfaces change with increasing annealing temperature up to 240 °C, promoting an enhancement of perpendicular magnetic anisotropy and the interfacial Dzyaloshinskii–Moriya interaction (i-DMI). Further annealing at higher temperatures brings the interface deterioration and, consequently, a drastic degradation of the magnetic properties. Our first-principles calculations qualitatively support the experimental findings, providing an understanding of the i-DMI enhancement nature.
quote
| GB/T 7714-2015 | [1] Aleksei Yu. Samardak, Alexander Kolesnikov, Maksim E. Stebliy, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00254. |
| MLA | [1] Aleksei Yu. Samardak, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00254. |
| APA | [1] Aleksei Yu. Samardak, Alexander Kolesnikov, Maksim E. Stebliy, Andrey V. Gerasimenko, Alexandr V. Sadovnikov, Sergei A. Nikitov, Anastasiia A. Pervishko, Dmitry Yudin, Alexey V. Ognev, Oleg A. Tretiakov, Caihua Wan, XiuFeng Han, & Alexander S. Samardak. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00254 |
| IEEE | [1] Aleksei Yu. Samardak, Alexander Kolesnikov, Maksim E. Stebliy, Andrey V. Gerasimenko, Alexandr V. Sadovnikov, Sergei A. Nikitov, Anastasiia A. Pervishko, Dmitry Yudin, Alexey V. Ognev, Oleg A. Tretiakov, Caihua Wan, XiuFeng Han, and Alexander S. Samardak, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00254. keywords: {ultrathin film perpendicular magnetic anisotropy interfacial Dzyaloshinskii−Moriya interaction thermal annealing atom intermixing} |