Abstract AITranslate
The coronavirus (SARS-CoV-2) has prompted a global need and shortage of face masks and respirators. Electrospinning of polystyrene and cellulose nanocrystals (CNCs) is used to fabricate filter materials exceeding N95 standards set by the National Institute for Occupational Health and Safety. The desired filtration efficiency and pressure drop are achieved from filters with varying amounts of input material. The water contact angle, fiber morphology, and surface potential are reported to explain the enhancements in filtration performance after the addition of CNCs or application of intense pulsed light (IPL). The improved durability in the form of increased mechanical properties and lower pressure drop after testing are also examined. The samples exhibited filtration efficiencies greater than 99% and an initial pressure drop as low as 231 Pa. The combination of CNCs and IPL shows the potential to use thinner membranes with less material to achieve comparable filtration performance, which may result in lower manufacturing costs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00722
Chinese Library Classification Number:
Citation Information:
The coronavirus (SARS-CoV-2) has prompted a global need and shortage of face masks and respirators. Electrospinning of polystyrene and cellulose nanocrystals (CNCs) is used to fabricate filter materials exceeding N95 standards set by the National Institute for Occupational Health and Safety. The desired filtration efficiency and pressure drop are achieved from filters with varying amounts of input material. The water contact angle, fiber morphology, and surface potential are reported to explain the enhancements in filtration performance after the addition of CNCs or application of intense pulsed light (IPL). The improved durability in the form of increased mechanical properties and lower pressure drop after testing are also examined. The samples exhibited filtration efficiencies greater than 99% and an initial pressure drop as low as 231 Pa. The combination of CNCs and IPL shows the potential to use thinner membranes with less material to achieve comparable filtration performance, which may result in lower manufacturing costs.
quote
| GB/T 7714-2015 | [1] Danny Wong, Sean Hartery, Erin Keltie, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00722. |
| MLA | [1] Danny Wong, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00722. |
| APA | [1] Danny Wong, Sean Hartery, Erin Keltie, Rachel Chang, Jong Sung Kim, & Simon S. Park. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00722 |
| IEEE | [1] Danny Wong, Sean Hartery, Erin Keltie, Rachel Chang, Jong Sung Kim, and Simon S. Park, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00722. keywords: {electrospinning;intense pulsed light;N95;filtration;surface potential;tensile testing} |