Patterning Bacterial Cellulose Films with Iron Oxide Nanoparticles and Magnetic Resonance Imaging Monitoring AITranslate

Institute of Materials Science of Barcelona;Institute of Materials Science of Barcelona;Institute of Materials Science of Barcelona;Institute of Materials Science of Barcelona;Institute of Materials Science of Barcelona
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Biomaterials derived from nature can offer sustainable, biomimetic, and biointeractive solutions. Bacterial cellulose (BC) is a natural biopolymer gaining popularity in the medical field due to its biocompatibility, excellent mechanical properties, and animal-free origin. Those attributes, together with its optimal conformability to different surfaces and high water holding capacity, have endorsed the use of BC films in wound healing, tissue engineering, implants, or wearable sensors. The functionalization of the BC films with nanoparticles (NPs) and the spatial control of their disposition in a BC substrate could further boost BC opportunities in those sectors. Here we report on an original method to deposit superparamagnetic iron oxide NPs (SPIONs) in selected areas of a flat BC film (thickness 6 ± 1 μm, roughness 26 ± 3 nm) using a screen-printing process to create ad hoc NPs patterns on the film surface. The ink used for screen-printing consisted of a dense solution of blended BC fibers (BCf, length 14 ± 9 μm) previously coated with SPIONs using a microwave-assisted synthetic route. In addition, we have tested the easy identification of a BC/SPIONs implant inserted in a simulated tissue by magnetic resonance imaging (MRI) as provided by an ex vivo test. The SPIONs in the BC presented an excellent performance as a transverse relaxation (T2) contrast agent. Those functionalized BC films could enlarge their application as bioimplants and be noninvasively monitored for the detection of deformations and adhesions.

KeyWords AITranslate

bacterial cellulose superparamagnetic nanoparticles patterning implant magnetic resonance imaging
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00723

Chinese Library Classification Number:

Citation Information:

Biomaterials derived from nature can offer sustainable, biomimetic, and biointeractive solutions. Bacterial cellulose (BC) is a natural biopolymer gaining popularity in the medical field due to its biocompatibility, excellent mechanical properties, and animal-free origin. Those attributes, together with its optimal conformability to different surfaces and high water holding capacity, have endorsed the use of BC films in wound healing, tissue engineering, implants, or wearable sensors. The functionalization of the BC films with nanoparticles (NPs) and the spatial control of their disposition in a BC substrate could further boost BC opportunities in those sectors. Here we report on an original method to deposit superparamagnetic iron oxide NPs (SPIONs) in selected areas of a flat BC film (thickness 6 ± 1 μm, roughness 26 ± 3 nm) using a screen-printing process to create ad hoc NPs patterns on the film surface. The ink used for screen-printing consisted of a dense solution of blended BC fibers (BCf, length 14 ± 9 μm) previously coated with SPIONs using a microwave-assisted synthetic route. In addition, we have tested the easy identification of a BC/SPIONs implant inserted in a simulated tissue by magnetic resonance imaging (MRI) as provided by an ex vivo test. The SPIONs in the BC presented an excellent performance as a transverse relaxation (T2) contrast agent. Those functionalized BC films could enlarge their application as bioimplants and be noninvasively monitored for the detection of deformations and adhesions.

quote

GB/T 7714-2015 [1] Cristina MiraCuenca, Thomas Meslier, Soledad RoigSanchez, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00723.
MLA [1] Cristina MiraCuenca, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00723.
APA [1] Cristina MiraCuenca, Thomas Meslier, Soledad RoigSanchez, Anna Laromaine, & Anna Roig. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00723
IEEE [1] Cristina MiraCuenca, Thomas Meslier, Soledad RoigSanchez, Anna Laromaine, and Anna Roig, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00723. keywords: {bacterial cellulose;superparamagnetic nanoparticles;patterning implant;magnetic resonance imaging}