Effects of Heat Treatment on the Mechanical Properties of Coarse-grained Cemented Carbide AITranslate

National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Research was made on the changes of mechanical properties of the binder phase and the whole alloy during heat treatment of the WC-8.4Co coarse-grained cemented carbide by nano indentation and high load HV test.The results show that heat treatment can improve hardness of the whole alloy by improving hardness of the binder phase,and meanwhile improve Palmqvist fracture toughness of the whole alloy.

KeyWords AITranslate

heat treatment coarse-grained cemented carbide binder phase nano indentation Palmqvist fracture toughness

1周定良;谢文;黄文亮.热处理对WC-10Co合金室温组织性能的影响[A]株洲:株洲硬质合金集团有限公司,2010193-197.

2马淳安,褚有群,黄辉,成旦红,周邦新.WC-Co硬质合金的相组成及其相变[J].浙江工业大学学报,2003,31(1):1-6. 被引量:31

1谭征.粗晶WC-Co类硬质合金的工艺研究进展[J].中国锰业,2013,31(3):47-49. 被引量:2

2吴冲浒,陈杉杉.热处理对超细晶硬质合金性能的影响[J].热处理技术与装备,2014,35(6):7-10. 被引量:4

3陈慧.硬质合金深冷处理的研究现状[J].铸造技术,2015,36(7):1703-1705. 被引量:2

4王洪福,王海鹏,何泠,王华君,王俊元.含有(Ti,Ta)C的梯度硬质合金的组织与性能分析[J].武汉理工大学学报,2015,37(3):28-33. 被引量:1

5戴俊.热处理工艺对硬质合金刀具复合材料组织与性能的影响[J].热加工工艺,2016,45(12):193-196.

6张佳,谭立群,谢晨辉,周华堂,郭建中.WC-25%Co硬质合金淬火热处理孔隙的微观特征及其形成机理[J].硬质合金,2018,35(3):171-179.

7蔡海燕.超粗晶硬质合金的研究现状与发展趋势[J].硬质合金,2018,35(4):297-303. 被引量:10

8顾金宝,时凯华,王可,曾伟,董凯林.热处理工艺对WC-10%Co粗晶硬质合金性能及微观结构的影响[J].硬质合金,2019,36(2):150-157. 被引量:4

1江丙武,蔡海燕,宋耀强,赵东,阳进,黄蕊,杜秋容.国内外路面铣刨刀具用硬质合金的现状与发展趋势[J].硬质合金,2014,31(3):194-200. 被引量:1

2丁鹏飞,刘宁,朱协彬,王刚,蔡聪聪.深冷处理对超音速火焰喷涂涂层显微组织和力学性能的影响[J].安徽工程大学学报,2016,31(4):52-57. 被引量:1

3莫敏,邹丹,易丹青.淬火与回火工艺对WC-20%Co硬质合金微观结构和性能的影响[J].硬质合金,2019,36(3):204-212. 被引量:2

4汤昌仁,梁瑜,郭永忠,陈玉柏,杨树忠.粉末粒度对超粗晶硬质合金性能影响的研究[J].中国钨业,2019,34(4):41-46. 被引量:4

5刘益兴,雍薇,彭晖,王晓灵.退火热处理对WC-6%Co超细晶硬质合金抗弯强度的影响[J].硬质合金,2020,37(2):127-132. 被引量:3

6邹爱忠,黄星,王永生,郭圣达.基于截齿用途的粗晶钨合金材料的再利用技术研究[J].中国钨业,2020,35(1):56-61.

7郭明忠.YG8硬质合金低温回火组织和性能研究[J].热加工工艺,2020,49(20):153-155.

8张宝林,石玉斌,韦玉青.浅析热处理对硬质合金结构及性能的影响[J].福建冶金,2021,50(1):24-28. 被引量:1

9卢翰林,陈乐平,方森鹏,周全.深冷处理对C17510铍铜合金组织及性能的影响[J].铸造技术,2021,42(4):304-307. 被引量:1

10徐伟,陈玉柏,汤昌仁,胡梦云,梁瑜.高性能非均匀结构硬质合金的制备及其形成机理研究[J].中国钨业,2021,36(1):48-54. 被引量:2

1张立,程鑫,陈述,马鋆,吴厚平,熊湘君.Cr、V、RE添加剂对特粗晶与超粗晶硬质合金微观组织与性能的影响[J].中国有色金属学报,2012,22(9):2620-2625. 被引量:9

2LaverniaEJ.Inconel纳米晶粉末的纳米压痕[J].粉末冶金技术,2003,21(1):56-56.

3Geva.,S,新观.杂质元素对维氏体和磁铁矿在CO/CO2和H2/H2O混合气体中还原为铁的影响[J].钒钛,1991(2):29-35.

4杨胜,顾金宝,廖军,陈洪霞.烧结压力对WC-12%Co粗晶硬质合金组织及性能的影响[J].稀有金属与硬质合金,2015,43(2):54-58.

5吴迪,熊志翔,白英龙,果世驹,杨霞,徐红霞.铸造碳化钨反应烧结制备粗晶硬质合金[J].粉末冶金材料科学与工程,2011,16(4):471-477. 被引量:3

6聂洪波.超粗晶WC-Co硬质合金的制备方法与机理及性能研究[J].中国钨业,2016,31(4):51-57. 被引量:10

7陈洪霞,薛林,顾金宝,杨胜,袁明健.烧结工艺对粗晶硬质合金微观组织及性能的影响[J].稀有金属与硬质合金,2015,43(5):64-67 71. 被引量:2

8郭圣达,羊建高,黄海平,许方,胡咏梅,郑彪华.粗晶硬质合金硬度和强度影响因素的分析研究[J].稀有金属与硬质合金,2012,40(4):56-58. 被引量:10

9李勇,谢淑华.WC粗晶硬质合金的研究进展[J].材料研究与应用,2009,3(2):77-80. 被引量:12

10陈芃,李海坤.硬质合金高温处理回收工艺研究[J].硬质合金,2001,18(4):201-203. 被引量:13

Basic Information:

DOI:

Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]

Citation Information:

Research was made on the changes of mechanical properties of the binder phase and the whole alloy during heat treatment of the WC-8.4Co coarse-grained cemented carbide by nano indentation and high load HV test.The results show that heat treatment can improve hardness of the whole alloy by improving hardness of the binder phase,and meanwhile improve Palmqvist fracture toughness of the whole alloy.

quote

GB/T 7714-2015 [1] CHENG Xin, ZHANG Li. Effects of Heat Treatment on the Mechanical Properties of Coarse-grained Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2012(2): 45-47.
MLA [1] CHENG Xin, and ZHANG Li. "Effects of Heat Treatment on the Mechanical Properties of Coarse-grained Cemented Carbide." Rare Metals and Cemented Carbides, no. 2, 2012, pp. 45-47.
APA [1] CHENG Xin, & ZHANG Li. (2012). Effects of Heat Treatment on the Mechanical Properties of Coarse-grained Cemented Carbide. Rare Metals and Cemented Carbides(2), 45-47.
IEEE [1] CHENG Xin and ZHANG Li, "Effects of Heat Treatment on the Mechanical Properties of Coarse-grained Cemented Carbide," Rare Metals and Cemented Carbides, no. 2, pp. 45-47, 2012. keywords: {heat treatment;coarse-grained cemented carbide;binder phase;nano indentation;Palmqvist fracture toughness}