Study on Thermal Decomposition-Reduction Process for Preparing W-Ni-Cu Tungsten Alloys AITranslate

Zhongnan University of Technology;Zhongnan University of Technology;Zhongnan University of Technology;Zhongnan University of Technology;Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

W-Ni-Cu Tungsten alloys can be produced by the thermal decomposition-reduction of the W powder mixture with Ni(NO3)2, CuCl2solutions or with Ni(CH3COO)2, Cu(CH3COO)2 solutions. Both manufactured alloys are available for use. The characteristics and problems of the processes using two different mixtures were studied in details. It was clearly shown that the use of the first mixture during reduction results in a lot of toxic gases, which are harm to the environment, and the second mixture is favourable for environment protect and product quality during reduction.

KeyWords AITranslate

thermal decomposition-reduction tungsten alloys

1沈宏芳,陈文革,谷臣清.纳米W-Ni-Fe高比重合金的研究[J].稀有金属,2005,29(2):133-137. 被引量:6

2沈宏芳,陈文革,谷臣清.纳米W-Ni-Fe复合粉末的制备及其对组织性能的影响[J].新技术新工艺,2005(5):59-61. 被引量:1

3李移贵,熊湘君,王伏生.W-Ni-Cu合金的断口缺陷与工艺因素分析[J].稀有金属与硬质合金,1995,23(4):17-21. 被引量:2

1刘桂荣,王德文,陈伟.93W-5Ni-2Cu烧结工艺的研究[J].粉末冶金工业,2004,14(4):10-13. 被引量:1

2王雅慧,李云凯,李玉秋,尹静静.钨合金强化机制的电子结构表征[J].稀有金属,2007,31(4):430-433. 被引量:2

3邹惠兰.钨基重合金的研究与应用现状[J].湖南冶金,1997(2):60-64. 被引量:11

4彭石高,范景莲,刘涛,祁美贵,丁飞,田家敏.稀土含量和还原温度对制备超细(W,Ni,Fe)复合粉末的影响[J].粉末冶金技术,2009,27(1):36-39. 被引量:6

5李小强,辛红伟,胡可,陈维平,李元元.高密度W-Ni-Fe合金的研究进展[J].材料导报,2009,23(15):66-69. 被引量:9

6刘桂荣,蒲治军,王玲,裴燕斌.细晶钨合金密度均匀性研究[J].粉末冶金工业,2010(4):24-27. 被引量:2

7刘桂荣,王玲,裴燕斌.细晶钨合金内部组织均匀性研究[J].中国钨业,2010,25(5):32-34.

8张陈增,张雪辉,周亮亮,王成,章标,李晓闲,陈颢.稀土CeO_2对W-Ni-Fe高比重合金摩擦磨损性能的影响[J].中国钨业,2016,31(6):18-24.

9张雪辉,周亮亮,李晓闲,张陈增,王成,章标,陈颢,梁彤祥.Y_2O_3对W-4.9Ni-2.1Fe合金摩擦磨损行为的影响[J].材料工程,2017,45(11):115-121. 被引量:4

1马小强,朱晓云,龙晋明,李伟力,曹梅.铜盐种类及表面活性剂对制备超细铜粉的影响[J].热加工工艺,2016,45(20):34-38. 被引量:3

2王艳芝,李秋荣,陈闽子.铸造铝合金电解着色工艺研究[J].电镀与精饰,2001,23(2):33-36.

3向铁根,刘海湘.还原工艺对钼粉粒度和氧含量的影响[J].中国钼业,2004,28(2):42-45. 被引量:8

4黄晓玲,张菊平,王引婷.二钼酸铵性能及还原工艺对钼粉粒度的影响[J].中国钼业,2008,32(3):47-49. 被引量:5

5肖冰.镀镍棕刚玉磨料制备与性能研究[J].河南科学,2010,28(10):1254-1256.

6肖江涛.Mo-La掺杂粉生产工艺研究[J].铸造技术,2015,36(6):1536-1540.

7孙永辉.电解氯化铜时金属铜在阴极不同部位析出的原因[J].化学教学,2007(8):6-6.

8陈开权.氧化铜无机胶粘接加长钻头的工艺介绍[J].重发科技,2000(1):25-26.

9张春丽,任广军.磷化助剂对铝合金磷化膜耐蚀性能的影响[J].有色矿冶,2013,29(4):40-41. 被引量:1

10赵思萌,郝建军,崔珊.钢铁件序间防锈剂的研究[J].电镀与精饰,2016,38(11):40-42.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]

Citation Information:

W-Ni-Cu Tungsten alloys can be produced by the thermal decomposition-reduction of the W powder mixture with Ni(NO3)2, CuCl2solutions or with Ni(CH3COO)2, Cu(CH3COO)2 solutions. Both manufactured alloys are available for use. The characteristics and problems of the processes using two different mixtures were studied in details. It was clearly shown that the use of the first mixture during reduction results in a lot of toxic gases, which are harm to the environment, and the second mixture is favourable for environment protect and product quality during reduction.

quote

GB/T 7714-2015 [1] LIANG Rong-hai, WANG Fu-sheng, ZHOU Zai-ming, et al. Study on Thermal Decomposition-Reduction Process for Preparing W-Ni-Cu Tungsten Alloys[J]. Rare Metals and Cemented Carbides, 1994(3): 28-32.
MLA [1] LIANG Rong-hai, et al., "Study on Thermal Decomposition-Reduction Process for Preparing W-Ni-Cu Tungsten Alloys." Rare Metals and Cemented Carbides, no. 3, 1994, pp. 28-32.
APA [1] LIANG Rong-hai, WANG Fu-sheng, ZHOU Zai-ming, YI Fu-de, & GAO Hong-wei. (1994). Study on Thermal Decomposition-Reduction Process for Preparing W-Ni-Cu Tungsten Alloys. Rare Metals and Cemented Carbides(3), 28-32.
IEEE [1] LIANG Rong-hai, WANG Fu-sheng, ZHOU Zai-ming, YI Fu-de, and GAO Hong-wei, "Study on Thermal Decomposition-Reduction Process for Preparing W-Ni-Cu Tungsten Alloys," Rare Metals and Cemented Carbides, no. 3, pp. 28-32, 1994. keywords: {thermal decomposition-reduction, tungsten alloys}