Study on Ore Properties and Beneficiation Technology of the Southwest Rare Earth Ore in China AITranslate

Tsinghua University Nuclear Energy Technology Design Research Institute;Tsinghua University Nuclear Energy Technology Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The ore properties of rare earth (RE) ore of Southwest Territory, China, and its beneficiation technology have been studied. The ore is strongly weathered to produce 20% black slime. RE available for commercial use in ore is occurred in two phases: mineral and colloidal. The main (>96%) RE mineral of mineral phase is bastnaesite. The bastnaesite concentrates (30%、 50% and 60% REO) can be obtained by gravity separation or gravity-flotation combined process at 65% recovery of RE. RE minerals of colloidal phase is absorbed in non-crystal minerals of Fe-Mn oxide. It can be recovered by hot HC1 leaching-purification with liquid ammonia-oxalic acid precipitation route at 74.3% of RE, and lead can be obtained as byproduct. The ore and the black weathered minerals are rich in cerium family RE (∑CeO2>90%, CeO2>La2O3>Nd2O3).

KeyWords AITranslate

bastnaesite beneficiation weathering action colloid phase rare earth

1张金山,郝文刚,屈奇奇.我国稀土选矿联合工艺的发展现状[J].中国矿业,2018,27(1):127-131. 被引量:10

2迈倩琳,王丽明,曹钊.矿物型稀土矿的选矿工艺研究进展[J].现代矿业,2021,37(4):1-4. 被引量:4

1胡洋,何东升,刘爽,谢志豪,陈飞.含稀土磷矿稀土元素赋存特性[J].矿物学报,2020,0(1):101-105. 被引量:5

2王瑞祥,郭跃东,方壮,陈芳会,余攀,徐志峰.离子型稀土矿硫酸镁柱浸过程中水、稀土和硫酸镁的平衡研究[J].有色金属:冶炼部分,2018(10):36-40. 被引量:3

3李文博,武锋,杨峰,卢位.国内矿物型稀土选别工艺及浮选捕收剂机理研究新进展[J].现代矿业,2019,35(6):1-5. 被引量:6

4王秀丽,张哲源,李恒凯.离子型稀土矿开采的环境影响及治理措施[J].国土与自然资源研究,2020,0(2):20-22. 被引量:8

5丁祥,王建军,况侨,王辉涛,张德康,肖金花.离子型稀土矿冶炼分离过程中的环境影响分析[J].矿冶,2020,29(2):98-104. 被引量:1

6徐岳清,陈旗.基于自适应极限学习机的磨机负荷智能控制研究[J].中国矿业,2020,29(9):82-86. 被引量:1

7郭春雷,王维维,金海龙.山东某稀土矿浮选过程及工艺优化[J].中国稀土学报,2020,38(6):823-831. 被引量:3

8洪秋阳,梁冬云,李波,张莉莉,饶金山.某复杂铌稀土矿石工艺矿物性质及可选性分析[J].矿产综合利用,2021(1):171-178. 被引量:8

9李梦闪,黄伟欣,张臻悦,张文才,唐鸿鹄,曹学锋,孙伟.煤及其副产物中稀土元素的赋存特征与选矿富集研究进展[J].有色金属:选矿部分,2021(6):61-81. 被引量:5

10邓善芝,熊文良,邓杰,陈达,张丽军.某富铁型稀土矿中稀土分离富集研究[J].有色金属:选矿部分,2021(6):97-101.

1池汝安,王淀佐.浮选氟碳鈰矿捕收剂[J].有色矿冶,1992(6):16-20. 被引量:5

2李芳积,廖维凯.耗牛坪氟碳铈矿选矿工艺研究[J].四川稀土,2002(2):7-12.

3汪中,车丽萍.我国氟碳铈矿浮选研究的新进展[J].稀土,1991,12(4):42-46. 被引量:4

4冯婕,张燕云.微山稀土矿地表矿选矿试验研究[J].山东冶金,1992,14(2):27-32. 被引量:2

5池汝安,王淀佐.稀土矿的分类和选别及冶炼[J].国外金属矿选矿,1991,28(12):13-20. 被引量:3

6宋常青.影响稀土矿浮选指标几个主要因素的研究[J].稀土,1992,13(1):24-27. 被引量:3

7王景伟.氟碳铈矿及伴生矿物浮选行为的研究[J].稀土,1991,12(2):33-37. 被引量:9

8池汝定,王淀佐.我国稀土矿选矿实践[J].有色冶金设计与研究,1990,11(2):29-35.

9向井滋,吴继宝.稀土矿物的选矿[J].江西有色金属,1990,4(3):59-63.

10刘蓉生.稀土基本知识(四)[J].四川稀土,2002(1):32-32.

Basic Information:

DOI:

Chinese Library Classification Number:TD955[矿业工程—选矿]

Citation Information:

The ore properties of rare earth (RE) ore of Southwest Territory, China, and its beneficiation technology have been studied. The ore is strongly weathered to produce 20% black slime. RE available for commercial use in ore is occurred in two phases: mineral and colloidal. The main (>96%) RE mineral of mineral phase is bastnaesite. The bastnaesite concentrates (30%、 50% and 60% REO) can be obtained by gravity separation or gravity-flotation combined process at 65% recovery of RE. RE minerals of colloidal phase is absorbed in non-crystal minerals of Fe-Mn oxide. It can be recovered by hot HC1 leaching-purification with liquid ammonia-oxalic acid precipitation route at 74.3% of RE, and lead can be obtained as byproduct. The ore and the black weathered minerals are rich in cerium family RE (∑CeO2>90%, CeO2>La2O3>Nd2O3).

quote

GB/T 7714-2015 [1] CHI Ru-an, SHI Ze-min. Study on Ore Properties and Beneficiation Technology of the Southwest Rare Earth Ore in China[J]. Rare Metals and Cemented Carbides, 1994(3): 33-39.
MLA [1] CHI Ru-an, and SHI Ze-min. "Study on Ore Properties and Beneficiation Technology of the Southwest Rare Earth Ore in China." Rare Metals and Cemented Carbides, no. 3, 1994, pp. 33-39.
APA [1] CHI Ru-an, & SHI Ze-min. (1994). Study on Ore Properties and Beneficiation Technology of the Southwest Rare Earth Ore in China. Rare Metals and Cemented Carbides(3), 33-39.
IEEE [1] CHI Ru-an and SHI Ze-min, "Study on Ore Properties and Beneficiation Technology of the Southwest Rare Earth Ore in China," Rare Metals and Cemented Carbides, no. 3, pp. 33-39, 1994. keywords: {bastnaesite, beneficiation, weathering action, colloid phase,rare earth}