Conducting-polymer-based electrical percolation networks are promising materials for use in high-sensitivity chemiresistive devices. An ongoing challenge is to create percolation networks that have consistent properties, so that devices based on these materials do not have to be individually calibrated. Here, an in situ conductance technique is used during the electrochemical growth of polypyrrole (PPy) percolation networks. The drain current (id) across the interdigitated electrodes (IDEs) is a measure of the conductance of the PPy network during electrochemical polymerization. The id curve is used to determine the percolation region. To improve the reproducibility of PPy percolation networks, an in situ conductance monitoring method based on the value of id is used. A set of optimal ammonia gas percolation sensors was created using this method with an average sensitivity of ΔR/R0 × 100% ppm–1 = 11.3 ± 1.2% ppm–1 and an average limit of detection of 15.0 ± 3.6 ppb.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01819
Chinese Library Classification Number:
Citation Information:
Conducting-polymer-based electrical percolation networks are promising materials for use in high-sensitivity chemiresistive devices. An ongoing challenge is to create percolation networks that have consistent properties, so that devices based on these materials do not have to be individually calibrated. Here, an in situ conductance technique is used during the electrochemical growth of polypyrrole (PPy) percolation networks. The drain current (id) across the interdigitated electrodes (IDEs) is a measure of the conductance of the PPy network during electrochemical polymerization. The id curve is used to determine the percolation region. To improve the reproducibility of PPy percolation networks, an in situ conductance monitoring method based on the value of id is used. A set of optimal ammonia gas percolation sensors was created using this method with an average sensitivity of ΔR/R0 × 100% ppm–1 = 11.3 ± 1.2% ppm–1 and an average limit of detection of 15.0 ± 3.6 ppb.
quote
| GB/T 7714-2015 | [1] Weishuo Li, Merel J. Lefferts, Ben I. Armitage, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01819. |
| MLA | [1] Weishuo Li, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01819. |
| APA | [1] Weishuo Li, Merel J. Lefferts, Ben I. Armitage, Krishnan Murugappan, & Martin R. Castell. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01819 |
| IEEE | [1] Weishuo Li, Merel J. Lefferts, Ben I. Armitage, Krishnan Murugappan, and Martin R. Castell, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01819. keywords: {conducting polymer;gas sensor;percolation network;in situ electrochemical conductance;electrochemical polymerization;Show More} |