Abstract AITranslate

Melanin is a natural biopolymer with a conjugated backbone that supposedly provides conductive pathways. However, few studies have synthesized electrically conductive melanin-like polymers (eMLPs) so far. In this study, highly electrically conductive melanin-like polymers (eMLPs) were electrochemically synthesized with tunable morphologies. After a bare gold electrode was coated with eMLP, the electrochemical performances were dramatically improved by a 2-order of magnitude decrease in impedance and up to a 60-fold increase in charge storage capacity. The morphology of the eMLP could be modulated by the ratios of carboxylic acid-bearing poly(l-3,4-dihydroxyphenylalanine) nanoparticles (PLDA NPs) to dopamine without compromising the electrochemical properties. Unlike conventionally insulating polydopamine, eMLP was demonstrated in glucose detection to be a nonenzymatic biosensor with high sensitivity (752.5 μA mM–1 cm–2), a low limit of detection (23 μM), a wide linear range up to 70 mM, and physiological selectivity. This eMLP composite with superior electrochemical performances can be utilized in a wide range of bioelectronics applications from in situ biosensors to implantable bionic interfaces.

KeyWords AITranslate

melaninlike polymers conductive polydopamine electrochemical deposition nonenzymatic glucose sensor bioelectronics
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01818

Chinese Library Classification Number:

Citation Information:

Melanin is a natural biopolymer with a conjugated backbone that supposedly provides conductive pathways. However, few studies have synthesized electrically conductive melanin-like polymers (eMLPs) so far. In this study, highly electrically conductive melanin-like polymers (eMLPs) were electrochemically synthesized with tunable morphologies. After a bare gold electrode was coated with eMLP, the electrochemical performances were dramatically improved by a 2-order of magnitude decrease in impedance and up to a 60-fold increase in charge storage capacity. The morphology of the eMLP could be modulated by the ratios of carboxylic acid-bearing poly(l-3,4-dihydroxyphenylalanine) nanoparticles (PLDA NPs) to dopamine without compromising the electrochemical properties. Unlike conventionally insulating polydopamine, eMLP was demonstrated in glucose detection to be a nonenzymatic biosensor with high sensitivity (752.5 μA mM–1 cm–2), a low limit of detection (23 μM), a wide linear range up to 70 mM, and physiological selectivity. This eMLP composite with superior electrochemical performances can be utilized in a wide range of bioelectronics applications from in situ biosensors to implantable bionic interfaces.

quote

GB/T 7714-2015 [1] Busra Ozlu, Bong Sup Shim. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01818.
MLA [1] Busra Ozlu, and Bong Sup Shim. ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01818.
APA [1] Busra Ozlu, & Bong Sup Shim. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01818
IEEE [1] Busra Ozlu and Bong Sup Shim, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01818. keywords: {melaninlike polymers;conductive polydopamine;electrochemical deposition;nonenzymatic glucose sensor;bioelectronics}