daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preliminary Study of the Process for the Production of Mn-Zn Ferrite Head Particle AITranslate

AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Brief description is made of the process and equipment for the production of Mn-Zn ferrite head particle with focus on the well-established coprecipitation operation and technology. The production methods are reviewd.

KeyWords AITranslate

Mn-Zn ferrire magnetic head material coprecipitation for powder preparation production process

1锰—锌铁氧体及制造方法[J].佛山陶瓷,2002(9):45-45.

2陈国钧,吕键,陈殿金,王旭军.HDD用磁头材料的发展现状[J].信息记录材料,2002,3(1):25-30. 被引量:2

3王建中,魏春华.高频铁氧体磁头材料测试样环尺寸同初始磁导率的关系[J].电子材料与电子技术,1992,19(3):44-46. 被引量:1

4张瑜,张野,李劲松,赵修彬,佘世杰,陈星.空气净化器电机用永磁铁氧体多极磁环研制[J].磁性材料及器件,2016,47(5):51-53. 被引量:1

5DONG Li-min HAN Zhi-dong WU Ze ZHANG Xian-you.Effect of Sintering Conditions on Structure of Manganese Zinc Ferrite Powders[J].中国航空学报:英文版,2006,19(B12):179-182.

6林河成.我国稀土永磁材料的发展现状及前景[J].金属材料研究,2006,32(4):19-27.

7董安智,吴隆鹏.磁头材料阻抗磁导率的测量[J].大连特殊钢,1994(1):57-61.

8任平,张俊喜,李雪,杜欣欣,刘国平,邓惠勇,戴宁.钴掺杂量对Mn-Zn铁氧体结构和磁性质的影响(英文)[J].硅酸盐学报,2011,39(11):1882-1886. 被引量:1

9黄凤群,王治,成宁宁.少量钴掺杂对Mn-Zn铁氧体结构和磁性质的影响(英文)[J].材料开发与应用,2012,27(4):50-54.

10钟太彬,林均品,陈国良.Fe_3Si基合金的制备及应用研究进展[J].功能材料,1999,30(4):337-339. 被引量:31

Basic Information:

DOI:

Chinese Library Classification Number:TM277.051[一般工业技术—材料科学与工程]

Citation Information:

Brief description is made of the process and equipment for the production of Mn-Zn ferrite head particle with focus on the well-established coprecipitation operation and technology. The production methods are reviewd.

quote

GB/T 7714-2015 [1] LIU Rui-hua. Preliminary Study of the Process for the Production of Mn-Zn Ferrite Head Particle[J]. Rare Metals and Cemented Carbides, 1998(1): 58-60.
MLA [1] LIU Rui-hua. "Preliminary Study of the Process for the Production of Mn-Zn Ferrite Head Particle." Rare Metals and Cemented Carbides, no. 1, 1998, pp. 58-60.
APA [1] LIU Rui-hua. (1998). Preliminary Study of the Process for the Production of Mn-Zn Ferrite Head Particle. Rare Metals and Cemented Carbides(1), 58-60.
IEEE [1] LIU Rui-hua, "Preliminary Study of the Process for the Production of Mn-Zn Ferrite Head Particle," Rare Metals and Cemented Carbides, no. 1, pp. 58-60, 1998. keywords: {Mn-Zn ferrire;magnetic head material;coprecipitation for powder preparation;production process}