daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Bismuth Vanadate Inorganic Pigments──Study of Rare Metal Refined Chemicals(I) AITranslate

Beijing Normal University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper briefly describes the recent research and development of bimuth vanadate inorganic pigments──bismuth vanadate yellow. bismuth vanadate molybdate,yellow and bismuth vanadate thermochemic pigments.

KeyWords AITranslate

bismuth vanadate yellow bismuth vanadate molybdate yellow bismuth vanadate thermochemic pigments inorganic pigment.

1宋文学.氧化铋钒的制取方法及其热色特性[J].涂料工业,1995,25(6):9-10. 被引量:2

1唐安平,殷钢城,杨惠乐.包核法制备钒酸铋颜料的研究[J].涂料工业,2004,34(10):8-10. 被引量:8

2刘进,吴绍华,兰尧中.新型材料铋黄的研究进展[J].涂料技术与文摘,2004,25(6):6-8. 被引量:12

1董伟霞,包启富,顾幸勇,吴燕春.仿金锂云母基珠光颜料的制备及性能表征[J].陶瓷学报,2009,30(3):357-361. 被引量:2

2李伟洲,李月巧,梁天权,赖武铨,胡治流.铋钒氧系颜料的研究进展[J].材料导报,2006,20(6):49-51.

3张萍,次立杰,张星辰,段书德,许保恩,赵建路.钒酸铋黄色颜料的制备及其影响因素[J].石家庄学院学报,2006,8(6):9-11. 被引量:8

4李静平,朱振峰.铋基黄色颜料的研究现状[J].佛山陶瓷,2007,17(1):32-34. 被引量:3

5张萍,张星辰,次立杰,段书德,许保恩,赵建路.耐高温钒酸铋黄色颜料的制备[J].精细化工,2007,24(7):706-709. 被引量:12

6高善民,乔青安,赵培培,陶芙蓉,张江,戴瑛,黄柏标.沉淀法制备不同形貌和结构的纳米BiVO_4[J].无机化学学报,2007,23(7):1153-1158. 被引量:22

7陶芙蓉,高善民,许璞,乔青安,林芳芳,赵培培,黄百勇.纳米BiVO4黄色颜料的制备研究[J].功能材料,2007,38(A07):2526-2529.

8邢占军,郝乐,仇洁楠,次立杰,任蕾,张萍.包覆型超细黄色颜料BiVO_4的制备研究[J].石家庄学院学报,2008,10(3):14-17. 被引量:2

9张萍,王焕英,许保恩,次立杰,刘树彬,张星辰.化学沉淀法制备BiVO4及其表征[J].人工晶体学报,2008,37(3):716-720. 被引量:20

10傅梦笔,唐培松,曹枫,余丹凤,黄重金.新型窄带隙半导体BiVO_4的制备与性能表征[J].湖州师范学院学报,2009,31(1):57-60. 被引量:1

1秦毅红,王云燕.共沉淀法制备铋黄颜料[J].涂料工业,2000,30(9):18-21. 被引量:4

2刘进,吴绍华,兰尧中.新型材料铋黄的研究进展[J].涂料技术与文摘,2004,25(6):6-8. 被引量:12

3可逆示温颜料和涂料[J].科技开发动态,1995(3):42-42.

4唐安平,周如梅.钒酸铋颜料[J].涂料工业,2002,32(6):27-28. 被引量:4

5张文朴.稀有金属精细化学品研究与开发进展(Ⅰ)──催化剂与颜料[J].稀有金属与硬质合金,1995,23(1):28-34. 被引量:2

6王志坚,窦传龙,涂文,陈燕彬.高效绿色颜料铋黄的制备研究[J].矿冶,2009,18(3):52-55. 被引量:3

7王云燕,秦毅红.新型无机黄色颜料——铋黄[J].湖南化工,1999,29(1):13-15.

8王云燕,秦毅红.新型黄色无机颜料——铋黄[J].涂料工业,1999,29(3):38-40. 被引量:12

9王云燕,秦毅红.新型无机黄色颜料铋黄[J].世界有色金属,1999(2):32-34. 被引量:1

10陈山南,蒋孟华.国外重防腐蚀涂料的发展情况[J].中国涂料,1993(4):31-39.

Basic Information:

DOI:

Chinese Library Classification Number:TQ62[化学工程—精细化工]

Citation Information:

This paper briefly describes the recent research and development of bimuth vanadate inorganic pigments──bismuth vanadate yellow. bismuth vanadate molybdate,yellow and bismuth vanadate thermochemic pigments.

quote

GB/T 7714-2015 [1] ZHANG Wen-pu. Bismuth Vanadate Inorganic Pigments──Study of Rare Metal Refined Chemicals(I)[J]. Rare Metals and Cemented Carbides, 1998(1): 51-57.
MLA [1] ZHANG Wen-pu. "Bismuth Vanadate Inorganic Pigments──Study of Rare Metal Refined Chemicals(I)." Rare Metals and Cemented Carbides, no. 1, 1998, pp. 51-57.
APA [1] ZHANG Wen-pu. (1998). Bismuth Vanadate Inorganic Pigments──Study of Rare Metal Refined Chemicals(I). Rare Metals and Cemented Carbides(1), 51-57.
IEEE [1] ZHANG Wen-pu, "Bismuth Vanadate Inorganic Pigments──Study of Rare Metal Refined Chemicals(I)," Rare Metals and Cemented Carbides, no. 1, pp. 51-57, 1998. keywords: {bismuth vanadate yellow;bismuth vanadate molybdate yellow;bismuth vanadate thermochemic pigments;inorganic pigment.}